Effect of dew point during annealing on phosphatability of ultra-high-strength steel
Source abstract
Abstract
This study aims to investigate the impact of controlled surface oxides on the phosphatability of ultra-high-strength steel, particularly for automotive applications. Surface oxides were controlled by adjusting the dew point to −30 and + 10 °C during the annealing process, and the consequent alterations in phosphatability were examined. XPS and TEM were utilized to analyze the surface characteristics of the samples. At dew points of −30 °C, minimal phosphating reaction was observed, whereas a significant enhancement in phosphating performance was noted with an increase in dew point to 10 °C. This improvement was attributed to structural modification influenced by the chemical composition of surface oxides, particularly the reduction in Si content and relatively higher Mn content and the enhanced internal oxidation at a dew point of 10 °C. The present results provide a heat treatment approach as a viable method to enhance phosphatability in ultra-high-strength steel.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Surface Treatment and Residual Stress
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Lightweight materials equal lightweight greenhouse gas emissions?: a historical analysis of greenhouse gases of vehicle material substitution10.1016/j.jclepro.2019.119805 ↗
2. Advanced lightweight materials for Automobiles: a review10.1016/j.matdes.2022.110994 ↗
3. Thermodynamic analysis of selective oxidation behavior of Si and Mn-added steel during recrystallization annealing10.2355/isijinternational.49.564 ↗
4. Selective oxidation and sub‐surface phase transformation of TWIP steel during continuous annealing10.1002/srin.201100122 ↗
5. Effect of Si content on wettability of dual phase high strength steels by liquid Zn-0.23 wt.% Al10.1007/s12540-011-0812-x ↗
6. The influence of Mn Content on the wettability of dual-phase high-strength steels by liquid Zn—0.23% Al10.1007/s10853-012-6737-z ↗
7. Effect of surface microstructure on oxidation of a CMnSi advanced high strength steel10.2355/isijinternational.ISIJINT-2017-016 ↗
8. Selective oxidation of ternary Fe-Mn-Si alloys during annealing process10.1016/j.corsci.2020.108859 ↗
9. Yoshihara · 1983 · 984
10. Surface pretreatment by phosphate conversion coatings-A review
11. Phosphatability of cold rolled steel sheet for automotive bodies10.2355/tetsutohagane1955.68.7_720 ↗
12. Effects of Ti and Mn addition on the surface state and phosphatability of cold rolled steel sheets10.2355/tetsutohagane1955.77.3_398 ↗
13. Effect of Cu and Sn on phosphatability of cold-rolled steel sheets10.2355/tetsutohagane1955.90.7_494 ↗
14. Effects of surface oxides on the phosphatability of the high strength cold rolled steels10.2355/tetsutohagane1955.92.6_378 ↗
15. Nanolayered oxide on a steel surface reduces surface reactivity: evaluation by glow discharge optical emission spectroscopy (GDOES)10.1016/j.scriptamat.2006.12.032 ↗
16. Effects of the surface state on phosphatability for high-strength cold-rolled steel sheets10.4139/sfj.66.372 ↗
17. The influence of silicon on the formation of phosphate coatings for low-carbon IF steels10.1016/j.surfcoat.2022.128599 ↗
18. Enhanced phosphatability by decorating ferrite layer on the surface of a multi-phase steel10.1016/j.matchar.2022.112373 ↗
19. Influence of surface segregation of tin on the phosphatability of cold‐rolled steel sheets10.1002/srin.202300592 ↗
20. Investigation into the surface selective oxidation of dual‐phase steels by XPS, SAM and SIMS10.1002/sia.1639 ↗
21. Numerical simulation of internal oxidation of steels during annealing treatments10.1007/s11085-005-5718-x ↗
22. Influence of Si content on selective oxidation and oxide scale phase transition during hot-rolled coiling10.1016/j.jmrt.2023.06.163 ↗
23. Internal oxidation during intercritical annealing of CMnSi TRIP steel10.2355/isijinternational.49.557 ↗
24. Calculations of internal oxidation rate equations and boundary conditions between internal and external oxidation in silicon containing steels10.2320/matertrans.M2009256 ↗
25. The influence of the dew point on the wettability of twinning-induced-plasticity steels by liquid Zn–0.23-wt% Al10.1016/j.corsci.2014.04.034 ↗
26. Effect of dew point on the formation of surface oxides of twinning-induced plasticity steel10.1016/j.matchar.2014.01.012 ↗
27. Changing oxide layer structures with respect to the dew point prior to hot-dip galvanizing of δ-TRIP steel10.1016/j.surfcoat.2017.12.046 ↗
28. Selective oxidation of a medium-Mn third generation advanced high strength steel during austenitizing and intercritical annealing10.1149/1945-7111/ac790a ↗
29. On the interaction between Mn, Sb and O during the annealing and selective oxidation of Fe-Mn-Sb alloys10.1016/j.scriptamat.2022.115096 ↗
30. Development of the surface structure of TRIP steels prior to hot-dip galvanizing10.1016/j.msea.2006.09.117 ↗
31. Improvement of the wettability of SiMn IF-HSS by liquid zinc by controlling the dew point of the annealing gas atmosphere10.1007/s10853-009-4131-2 ↗
32. Nucleation and formation of zinc phosphate conversion coating on cold-rolled steel10.1016/0010-938X(91)90112-3 ↗
33. Effect of annealing temperature on the surface and subsurface microstructure of Al-added TWIP steel10.1016/j.surfcoat.2020.125479 ↗
34. Effect of water pressure and soaking time on the selective oxidation of DP980 advanced high strength steel10.1016/j.apsusc.2018.05.034 ↗
35. Thermodynamic and kinetic aspects on the selective surface oxidation of binary, ternary and quaternary model alloys10.1016/j.apsusc.2006.10.031 ↗
36. Moulder · 1992
37. XPS and EELS characterization of Mn2SiO4, MnSiO3 and MnAl2O410.1016/j.apsusc.2016.03.235 ↗