Microstructure and mechanical properties of the Mg98.5Zn0.5RE1 (RE=Gd and/or Y) alloys processed by equal channel angular pressing
Source abstract
Abstract
In this work, Mg98.5Zn0.5RE1 (RE=Gd and/or Y) and Mg97Zn1Y2 (at%) alloys were subjected to homogenization and equal channel angular pressing (ECAP) to systematically compare the microstructure evolution and mechanical properties. The results indicate that, instead of the lamellar LPSO phases in the as-cast Mg-Zn-Y series alloys, the β-Mg5(Gd, Zn) phases appear in the as-cast Mg98.5Zn0.5Gd1 alloy which tend to be dissolved during homogenization. The furnace cooling after homogenization promotes the precipitation of numerous lamellar LPSO phases in all the studied alloys which inhibit the DRX behavior but facilitate the operation of kinking deformation during ECAP for the Mg98.5Zn0.5RE1 alloys, especially the Mg98.5Zn0.5Gd1 one. After the 5p-ECAP process at 350 °C, the larger density of kink bands, more LAGBs (low-angle grain boundaries) and lower SFB (Schmid factor for basal slip) combine to endow the Mg98.5Zn0.5Gd1 alloy with the higher strength-ductility synergy, exhibiting the tensile yield strength (TYS) of 214 MPa and elongation of 9.6%. The Mg97Zn1Y2 alloy with the larger volume fraction of interdendritic LPSO phases and dynamically recrystallized (DRXed) regions exhibits the superior ultimate tensile strength (UTS) of 277 MPa and moderate elongation of 7.2%.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Hydrogen Storage and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (57)
Show source-provided references
1. Rapidly solidified powder metallurgy Mg97Zn1Y2 alloys with excellent tensile yield strength above 600 MPa10.2320/matertrans.42.1172 ↗
2. Formation and mechanical properties of Mg97Zn1RE2 alloys with long-period stacking ordered structure10.2320/matertrans.MER2007142 ↗
3. Recent developments in high-strength Mg-RE-based alloys: focusing on Mg-Gd and Mg-Y systems10.1016/j.jma.2018.08.001 ↗
4. Recent research and developments on wrought magnesium alloys10.1016/j.jma.2017.09.001 ↗
5. Effects of pre-annealing on microstructure and mechanical properties of as-extruded Mg-Gd-Y-Zn-Zr alloy10.1016/j.jallcom.2017.09.214 ↗
6. Achieving ultra-high hardness of nanostructured Mg-8.2Gd-3.2Y-1.0Zn-0.4Zr alloy produced by a combination of high pressure torsion and ageing treatment10.1016/j.scriptamat.2018.06.009 ↗
7. A high-performance Mg-4.9Gd-3.2Y-1.1Zn-0.5Zr alloy via multidirectional forging after analyzing its compression behavior10.1016/j.jmst.2020.08.054 ↗
8. Bulk nanocrystalline high-strength magnesium alloys prepared via rotary swaging10.1016/j.actamat.2020.09.024 ↗
9. Fabrication of a high strength Mg–11Gd–4.5Y–1Nd–1.5Zn–0.5Zr (wt%) alloy by thermomechanical treatments10.1016/j.msea.2014.10.077 ↗
10. Effects of heat treatment on mechanical properties of an extruded Mg-4.3Gd-3.2Y-1.2Zn-0.5Zr alloy and establishment of its Hall–Petch relation10.1016/j.jma.2020.09.023 ↗
11. Microstructure and mechanical properties of extruded Mg-Gd-Y-Zn-Zr alloys filled with intragranular LPSO phases10.1016/j.matchar.2017.11.027 ↗
12. Hall-Petch relationship in Mg alloys: a review10.1016/j.jmst.2017.07.022 ↗
13. Achieving ultra-fine grains and high strength of Mg–9Li alloy via room-temperature ECAP and post rolling10.1016/j.msea.2021.142371 ↗
14. Effect of Y content and equal channel angular pressing on the microstructure, texture and mechanical property of extruded Mg-Y alloys10.1016/j.jma.2020.08.021 ↗
15. Effect of intersection annealing on the microstructure and compressive properties of pure Mg processed by four-pass ambient ECAP10.1016/j.jmrt.2022.01.165 ↗
16. Exceptional grain refinement in a Mg alloy during high pressure torsion due to rare earth containing nanosized precipitates10.1016/j.msea.2018.05.021 ↗
17. Altered ageing behaviour of a nanostructured Mg-8.2Gd-3.8Y-1.0Zn-0.4Zr alloy processed by high pressure torsion10.1016/j.actamat.2018.04.003 ↗
18. Evolution of long-period stacking ordered structure and hardness of Mg-8.2Gd-3.8Y-1.0Zn-0.4Zr alloy during processing by high pressure torsion10.1016/j.msea.2018.09.063 ↗
19. Inhomogeneous microstructure and mechanical anisotropy of multi-directional forged Mg-Gd-Y-Zn-Ag-Zr alloy10.1016/j.msea.2021.140853 ↗
20. Fabrication of high-strength AZ80 alloys via multidirectional forging in air with no need of ageing treatment10.1016/j.jallcom.2019.02.133 ↗
21. Microstructure, texture evolution and mechanical properties of a large-scale multidirectionally forged Mg-Gd-Y-Zn-Zr-Ag alloy10.1016/j.jmrt.2023.04.076 ↗
22. Microstructure and mechanical property of a high-strength Mg–10Gd–6Y–1.5Zn–0.5Zr alloy prepared by multi-pass equal channel angular pressing10.1016/j.jma.2017.05.002 ↗
23. Microstructure and mechanical properties of ultrafine grained Mg97Y2Zn1 alloy processed by equal channel angular pressing10.1016/j.jallcom.2006.09.005 ↗
24. Formation of profuse long period stacking ordered microcells in Mg–Gd–Zn–Zr alloy during multipass ECAP process10.1016/j.jallcom.2014.02.175 ↗
25. Synergistic effect of LPSO and eutectic phase on mechanical properties of Mg-Gd-Nd-Zn-Zr alloy during equal channel angular pressing10.1016/j.jmrt.2021.09.058 ↗
26. Dynamically recrystallized structure and mechanical properties of Mg96Zn2Y2 alloys deformed by ECAP10.2320/matertrans.L-M2021840 ↗
27. Increase in the mechanical strength of Mg-8Gd-3Y-1Zn alloy containing long-period stacking ordered phases using equal channel angular pressing processing10.3390/met9020221 ↗
28. Hydrogen storage properties and mechanisms of as-cast, homogenized and ECAP processed Mg98.5Y1Zn0.5 alloys containing LPSO phase10.1016/j.energy.2020.119315 ↗
29. Improving corrosion resistance of RE-containing magnesium alloy ZE41A through ECAP10.1016/S1002-0721(08)60348-8 ↗
30. Improving microstructure and corrosion resistance of LPSO-containing Mg–Y–Zn–Mn alloy through ECAP integrated with prior solution treatment10.1016/j.jmrt.2022.05.161 ↗
31. The 18R and 14H long-period stacking ordered structures in Mg–Y–Zn alloys10.1016/j.actamat.2010.01.022 ↗
32. Microstructure and mechanical properties of Mg97Zn1Y2 alloy reinforced with LPSO structure produced by semisolid squeeze casting10.1016/j.msea.2018.07.025 ↗
33. The role of metastable LPSO building block clusters in phase transformations of an Mg-Y-Zn alloy10.1016/j.actamat.2016.04.016 ↗
34. Effect of multi-pass equal channel angular pressing on microstructure and mechanical properties of Mg97.1Zn1Gd1.8Zr0.1 alloy10.1016/j.msea.2013.11.081 ↗
35. Mechanical properties of warm-extruded Mg–Zn–Gd alloy with coherent 14H long periodic stacking ordered structure precipitate10.1016/j.scriptamat.2005.06.006 ↗
36. Formation of 14H long period stacking ordered structure and profuse stacking faults in Mg–Zn–Gd alloys during isothermal aging at high temperature10.1016/j.actamat.2007.08.033 ↗
37. Formation of a lamellar 14H-type long period stacking ordered structure in an as-cast Mg–Gd–Zn–Zr alloy10.1007/s10853-008-3213-x ↗
38. Evolution of LPSO phases and their effect on dynamic recrystallization in a Mg-Gd-Y-Zn-Zr alloy10.1007/s11661-017-4081-2 ↗
39. Mechanical properties of the Mg-Gd-Y-Zn-Zr alloys with different morphologies of long-period stacking ordered phases10.1007/s11665-018-3713-z ↗
40. Growth and transformation mechanisms of 18R and 14H in Mg–Y–Zn alloys10.1016/j.actamat.2012.08.022 ↗
41. Effect of long-period stacking ordered phase on mechanical properties of Mg97Zn1Y2 extruded alloy10.1016/j.actamat.2010.07.050 ↗
42. Tensile behavior at various temperatures of the Mg-Gd-Y-Zn-Zr alloys with different initial morphologies of LPSO phases prior to extrusion10.1016/j.msea.2022.143634 ↗
43. Improved workability for Mg-Y-Zn alloys via increased volume fraction of block LPSO phases10.1016/j.msea.2020.139934 ↗
44. Processing and properties of Mg–6Gd–1Zn–0.6Zr: Part 1 – recrystallisation and texture development10.1016/j.msea.2010.12.100 ↗
45. Kink formation process in long-period stacking ordered Mg-Zn-Y alloy10.1016/j.actamat.2020.04.051 ↗
46. Kink-band formation in directionally solidified Mg/Mg2Yb and Mg/Mg2Ca eutectic alloys with Mg/Laves-phase lamellar microstructure10.1016/j.jma.2021.02.006 ↗
47. Improved workability and ductility of the Mg-Gd-Y-Zn-Zr alloy via enhanced kinking and dynamic recrystallization10.1016/j.jallcom.2018.03.359 ↗
48. A two-step dynamic recrystallization induced by LPSO phases and its impact on mechanical property of severe plastic deformation processed Mg97Y2Zn1 alloy10.1016/j.jallcom.2017.02.107 ↗
49. Hot compression behavior of the Mg-Gd-Y-Zn-Zr alloy filled with intragranular long-period stacking ordered phases10.1016/j.jallcom.2017.07.088 ↗
50. Particle effects on recrystallization in magnesium–manganese alloys: particle-stimulated nucleation10.1016/j.actamat.2009.02.032 ↗
51. Combined effects of LPSO orientation and α-Mg texture on tensile anisotropy of an extruded Mg-Gd-Y-Zn-Zr alloy10.1016/j.msea.2020.140596 ↗
52. Optimization of strength by microstructural refinement of MgY2Zn1 alloy during extrusion and ECAP processing10.1016/j.msea.2014.07.012 ↗
53. Strengthening and toughening mechanisms in Mg–Zn–Y alloy with a long period stacking ordered structure10.1016/j.actamat.2010.05.012 ↗
54. Tailoring microstructural evolution and fracture damage behavior of a Mg–Y–Zn alloy during hot tensile deformation
55. The evolution of internal strain in Mg–Y–Zn alloys with a long period stacking ordered structure10.1016/j.scriptamat.2011.07.017 ↗
56. Effect of the morphology of long-period stacking ordered phase on mechanical properties and corrosion behavior of cast Mg-Zn-Y-Ti alloy10.1016/j.jallcom.2018.06.056 ↗
57. Microstructures and mechanical properties of Mg–13Gd–5Er–1Zn–0.3Zr alloy10.1016/j.matdes.2014.01.058 ↗