Enhancement of pitting corrosion resistance for AA1050 processed by continuous closed die forging
Source abstract
Abstract
The pitting corrosion of an aluminum alloy AA1050 after being processed by continuous closed die forging (CCDF) was evaluated by cyclic potentiodynamic polarization (CPP). Microstructure evolution, mechanical and corrosion behaviors were studied as a function of the total strain imposed. The CCDF process was carried out at 0, 16 and 24 passes with loading times of 10 and 15 s. The electron backscatter diffraction (EBSD) analysis revealed a grain refinement of 0.78 µm after 24 passes, which promoted an increment in the yield strength (YS), ultimate tensile strength (UTS) and vickers hardness (HV) by a factor of 9, 3 and 2 respectively; but the uniform strain and strain to rupture decreased by 93% and 72% respectively. Resistance to corrosion after 16 and 24 passes was compared with the reference material (0 passes), using CPP in a Na2S04 0.1 mol/l +100 mg/l of NaCl electrolyte. Results showed that the specimens with 24 passes decreased its corrosion rate one order of magnitude. In addition, specimens with very fine grain sizes have shown nobler pitting potential and lower pitting volume fraction than coarse grain specimens.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Novel method of severe plastic deformation–continuous closed die forging: CP aluminium case study10.4028/www.scientific.net/DDF.385.302 ↗
2. Microestructure and physical-mechanical properties evolution of pure tantalum processed with hard cyclic viscoplastic deformation10.1016/j.ijrmhm.2019.104983 ↗
3. Hardness inhomogeneity and local strengthening mechanisms of an Al1050 aluminium alloy after one pass of equal channel angular pressing
4. Experimental and numerical investigation on pure aluminium by ECAP10.1016/S1003-6326(08)60442-2 ↗
5. Microestructural evolution in an aluminium solid solution alloy processed by ECAP10.1016/j.msea.2011.04.017 ↗
6. Corrosion behaviour of ultra-fine grained industrial pure Al fabricated by ECAP10.1016/S1003-6326(08)60407-0 ↗
7. Twenty-five years of ultrafine-grained materials: achieving exceptional properties through grain refinement10.1016/j.actamat.2013.08.018 ↗
8. Nanostructured aluminium alloys produced by severe plastic deformation. New horizons in development10.1016/j.msea.2012.09.020 ↗
9. A review on processing of aluminium and its alloys through Equal Channel Angular Pressing die
10. Corrosion behaviour of 1050 severely deformed by rotary swaging10.1016/j.matdes.2014.01.005 ↗
11. A study on the corrosion behavior of aluminum alloys in seawater10.1016/j.matdes.2007.01.021 ↗
12. Corrosion of ultrafine grained materials by severe plastic deformation
13. Effect of the number of ECAP pass time on the electrochemical properties of 1050 Al alloys10.1016/j.msea.2003.08.056 ↗
14. Corrosion resistance of model ultrafine-grained Al-Li alloys produced by severe plastic deformation10.1007/s10853-011-6133-0 ↗
15. Effects of high-pressure torsion on the pitting corrosion resistance of aluminum-iron alloys10.2320/matertrans.MH201301 ↗
16. Impact of ultrafine-grained microstructure on the corrosion of aluminium alloy AA202410.1016/j.corsci.2011.12.016 ↗
17. Effects of grain size on the corrosion resistance of wrought magnesium alloys containing neodymium10.1016/j.corsci.2012.01.021 ↗
18. In vitro study on equal channel angular pressing AZ31 magnesium alloy with and without back pressure10.1016/j.mseb.2011.04.003 ↗
19. Corrosion behavior of commercial aluminum alloy processed by equal channel angular pressing
20. Pitting corrosion resistance of anodized aluminium alloy processed by severe plastic deformation10.2320/matertrans.48.21 ↗
21. Corrosion behavior of equal-channel-angular-pressed pure magnesium in NaCl aqueous solution10.1016/j.corsci.2009.10.004 ↗
22. Effect of grain size on corrosion: a review10.5006/1.3462912 ↗
23. Microestructural evolution of Fe-rich particles in an Al-Zn-Mg-Cu alloy during equal-channel angular pressing10.1016/j.msea.2010.04.041 ↗
24. The effect of pre-annealing on defects, microstructure and recrystallization of ultra-fine grained Al produced by high-pressure torsion10.1016/j.msea.2017.09.126 ↗
25. The effect of pre-annealing on the evolution of the microstructure and mechanical behavior of aluminum processed by a novel SPD method10.3390/ma13102361 ↗
26. Influence of ECAP as grain refinement technique on microstructure evolution mechanical properties and corrosion behavior of pure aluminium10.1016/S1003-6326(15)64034-1 ↗
27. Effects of pH and chloride concentration on pitting corrosion of AA6061 aluminum alloy10.1016/j.corsci.2008.03.006 ↗
28. Electrochemical behavior of Al, Al–Sn, Al–Zn and Al–Zn–Sn alloys in chloride solutions containing indium ions10.1023/A:1003425306696 ↗
29. Thompson · 1988
30. Trethewey · 1995
31. Silverman · 1998 · 1
32. Corrosion behaviour of Al 1050 severely deformed by rotatory swaging10.1016/j.matdes.2014.01.005 ↗
33. Influence of dynamic recrystallization and shear banding on localized corrosion of severely deformed Al-Mg-Si alloy10.1016/j.mtla.2018.11.005 ↗