Effect of defects on environment-assisted fracture (EAF) behavior of Ti–6Al–4V alloy fabricated by direct energy deposition (DED)
Source abstract
Abstract
Environment-assisted fracture (EAF) behavior of direct energy deposition (DED) Ti–6Al–4V (Ti64) specimen was investigated using a slow strain rate test (SSRT) method in air and 3.5% NaCl solution under controlled potentials, where the susceptibility to EAF was described by the reduction in tensile elongation (RTE) with exposure to aggressive environment. It was found that RTE value of DED Ti64 specimen was approximately 4 times greater than that of conventional manufacturing (CM) counterpart. The fractographic analysis on DED Ti64 specimen tested in 3.5% NaCl solution suggested that crack-like discontinuity was instantly formed from corrosion damages by merging into band-like lack of fusion (LOF) near the surface. Since LOFs were developed perpendicular to build direction (BD), the RTE value of DED Ti64 specimen with tensile direction (TD) perpendicular to BD was approximately 4 times lower than those with TD parallel to BD. Excellent correlation between the area fraction of LOF and the RTE was observed, indicating that LOFs were responsible for high susceptibility to EAF of DED Ti64 specimen in Cl− bearing environment.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Nuclear Materials and Properties · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Costs, benefits, and adoption of additive manufacturing: a supply chain perspective10.1007/s00170-015-7973-6 ↗
2. 3D printing of Aluminium alloys: additive manufacturing of Aluminium alloys using selective laser melting10.1016/j.pmatsci.2019.100578 ↗
3. Additive manufacturing in the spare parts supply chain10.1016/j.compind.2013.07.008 ↗
4. Additive manufacturing of Ti-6Al-4V parts through laser metal deposition (LMD): process, microstructure, and mechanical properties10.1016/j.jallcom.2019.04.255 ↗
5. High-performance eco-friendly trimming die manufacturing using heterogeneous material additive manufacturing technologies
6. Toward developing Ti alloys with high fatigue crack growth resistance by additive manufacturing10.1016/j.jmst.2022.06.011 ↗
7. Damage tolerant design of additively manufactured metallic components subjected to cyclic loading: state of the art and challenges
8. Fatigue cracking of additively manufactured materials-process and material perspectives10.3390/app10165556 ↗
9. Designing for damage tolerance in aerospace: a hybrid material technology10.1016/j.matdes.2014.06.068 ↗
10. Corrosion and the threat to aircraft structural integrity
11. Reviews on factors affecting fatigue behavior of high-Mn steels10.1007/s12540-017-7459-1 ↗
12. Stress corrosion cracking: characteristics, mechanisms and experimental study10.1007/s00170-017-0709-z ↗
13. Stress corrosion cracking10.1016/0022-3697(87)90120-X ↗
14. Rebak · 2011 · 273
15. A novel approach to the determination of the threshold for stress corrosion cracking (KISCC) using round tensile specimens
16. Dynamic response of conventional and hot isostatically pressed Ti-6Al-4V alloys: experiments and modeling10.1016/S0167-6636(01)00063-1 ↗
17. Structure and mechanical properties of Ti-6Al-4V alloy after zirconium addition10.1016/j.msea.2012.05.043 ↗
18. An overview on the use of titanium in the aerospace industry10.1016/0921-5093(96)10233-1 ↗
19. Revealing martensitic transformation and α/β interface evolution in electron beam melting three dimensional printed Ti-6Al-4V
20. Corrosion and tribocorrosion behaviour of Ti-6Al-4V produced by selective laser melting and hot pressing in comparison with the commercial alloy10.1016/j.jmatprotec.2018.11.008 ↗
21. The effect of strain rate on stress corrosion performance of Ti-6Al-4V alloy produced by additive manufacturing process10.1016/j.jmrt.2020.02.035 ↗
22. Heat treatment degrading the corrosion resistance of selective laser melted Ti-6Al-4V alloy10.1149/2.1481707jes ↗
23. Phenomenological observations on mechanical and corrosion properties of thixoformed 357 alloys: a comparison with permanent mold cast 357 alloys10.1007/s11661-002-0064-y ↗
24. Effect of stabilization annealing on SCC susceptibility of β-annealed Ti-6Al-4V alloy in 0.6 M NaCl solution10.1007/s12540-017-7303-7 ↗
25. The influence of chloride and sulphate ions on the corrosion behavior of Ti and Ti-6Al-4V alloy in oxalic acid10.1016/j.electacta.2008.12.060 ↗
26. Corrosion behavior of additive manufactured Ti-6Al-4V alloy in NaCl solution10.1007/s11661-017-4087-9 ↗
27. Influence of NaCl environment on stress corrosion cracking of additive manufactured Ti-6Al-4V alloy10.1016/j.engfailanal.2021.105515 ↗
28. Effect of annealing and crack orientation on fatigue crack propagation of Ti64 alloy fabricated by direct energy deposition process10.1007/s12540-021-01087-3 ↗
29. Some distinct features of transformative high entropy alloys for metal additive manufacturing10.3389/fmats.2022.873911 ↗
30. Anisotropic tensile behavior of Ti-6Al-4V components fabricated with directed energy deposition additive manufacturing10.1016/j.actamat.2014.12.054 ↗
31. Fabrication of large Ti-6Al-4V structures by direct laser deposition10.1016/j.jallcom.2014.12.234 ↗
32. Porosity effect on tensile behavior of Ti-6Al-4V specimens produced by laser engineered net shaping technology
33. Environment-assisted fatigue crack propagation (EAFCP) behavior of Ti64 alloy fabricated by direct energy deposition (DED) process10.1007/s11661-022-06765-4 ↗
34. Effects of Cr and Fe addition on microstructure and tensile properties of Ti-6Al-4V prepared by direct energy deposition10.1007/s12540-018-0148-x ↗
35. Uncovering the coupled impact of defect morphology and microstructure on the tensile behavior of Ti-6Al-4V fabricated via laser powder bed fusion10.1016/j.jmatprotec.2021.117113 ↗
36. Influence of defects on mechanical properties of Ti-6Al-4V components produced by selective laser melting and electron beam melting10.1016/j.matdes.2015.07.147 ↗
37. Investigation of electrochemical corrosion behavior of additive manufactured Ti-6Al-4V alloy for medical implants in different electrolytes10.1016/j.jallcom.2020.154620 ↗
38. The effect of hot isostatic pressure on the corrosion performance of Ti-6Al-4V produced by an electron beam melting additive manufacturing process
39. Effect of powder recycling on environment-assisted fracture of Inconel 718 alloy fabricated by laser powder bed fusion10.1007/s11661-021-06514-z ↗
40. Increasing of the corrosion resistance of the Ti-6Al-4V alloy by high thickness anodic oxidation10.1007/BF00701236 ↗
41. Effect of build geometry on the β-grain structure and texture in additive manufacture of Ti-6Al-4V by selective electron beam melting10.1016/j.matchar.2013.07.012 ↗
42. On the texture formation of selective laser melted Ti-6Al-4V10.1007/s11661-014-2218-0 ↗