Effect of annealing temperature on microstructure and mechanical property of Ti-0.3Mo-0.8Ni-0.01Y alloy

Haowei Liang, Meiyu Hou, Jie Li, Shuqi Deng, Sheng Huang, Han Xiao

Abstract

In this study, a novel near-α titanium alloy, Ti-0.3Mo-0.8Ni-0.01Y (TA10-0.01Y wt.%), was fabricated using a vacuum non-consumable arc-melting furnace. The effects of annealing temperature (670 °C, 770 °C, and 870 °C) on the microstructure and mechanical properties of TA10-0.01Y plates were systematically investigated. The results showed that the addition of trace Y increased the resistance to dislocation motion. After annealing at 670 °C and 770 °C, the microstructure transformed into equiaxed grains, whereas annealing at 870 °C produced a Widmanstätten structure. The tensile strength decreased from 510.2 MPa to 495.3 MPa and subsequently rose to 572.6 MPa, while the elongation increased from 25.3% to 35.1% and then dropped sharply to 7.6%. EBSD analysis revealed that the average grain size increased from 2.7 μm to 9.63 μm as the annealing temperature increased, accompanied by enhanced recrystallization driving force, eventually leading to complete recrystallization. Dispersed Y 2 O 3 particles suppressed grain-boundary migration and further impeded dislocation motion. This study provides important guidance for optimizing annealing temperature to develop high-performance near-α titanium alloys.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Shape Memory Alloy Transformations · Titanium Alloys Microstructure and Properties · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Current situation and development trend of titanium metal industry in China10.1007/s12613-022-2455-y ↗
2. High-strength titanium alloys for aerospace engineering applications: a review on melting-forging process10.1016/j.msea.2022.143260 ↗
3. Effect of cooling rate on microstructure evolution during α/β heat treatment of TA15 titanium alloy10.1016/j.matchar.2012.05.009 ↗
4. Influence of annealing treatment on α phase globularization, mechanical properties, and corrosion performance of hot-rolled Ti–0.3Mo–0.8Ni alloy melted by electron beam cold hearth technology10.1007/s11661-023-07065-1 ↗
5. Investigation on corrosion behavior of Zr-bearing TA10-based titanium alloys10.1016/j.corsci.2023.111354 ↗
6. Mechanical properties and corrosion behavior of electron beam cold hearth melting high strength and high corrosion resistant Ti-0.3Mo-0.8Ni alloy with different states
7. Microstructure evolution, mechanical properties, and corrosion resistance of hot rolled and annealed ti-mo-ni alloy10.3390/met13030566 ↗
8. Room temperature creep behavior of ti–nb–mo–sn based shape memory alloy for biomedical application10.1016/j.smmf.2023.100019 ↗
9. Improving mechanical property of Ti55531 alloy by yttrium dopant10.1016/j.jallcom.2022.167122 ↗
10. Formability improvement, cracking behavior and control of Y-modified Ti–43Al–4Nb–1Mo-0.1B alloys produced by selective laser melting10.1016/j.jallcom.2020.157172 ↗
11. Trace Y for as-cast Ti6Al4V to simultaneous enhance strength-ductility10.1016/j.jallcom.2023.169757 ↗
12. Effect of rare earth Ce addition on microstructure and mechanical properties of titanium alloy Ti-6Al-4V10.1016/j.matlet.2022.133244 ↗
13. Effect of oxide particles formed through addition of rare-earth metal on mechanical properties of biomedical β-Type titanium alloy10.2320/matertrans.MF201308 ↗
14. Development of beta-type ti-nb-zr-mo alloys for orthopedic applications
15. Microstructure observations in rare earth element Gd-modified Ti-44 at% Al10.1016/S0966-9795(99)00156-9 ↗
16. Effect of rare Earth element content on high cycle fatigue property of titanium alloys10.1088/1742-6596/1347/1/012005 ↗
17. Heterogeneous precipitate microstructure in titanium alloys for simultaneous improvement of strength and ductility10.1016/j.jmst.2022.02.025 ↗
18. Effects of annealing temperature and quenching medium on microstructure, mechanical properties as well as fatigue behavior of Ti-6Al-4V alloy10.1016/j.msea.2016.11.095 ↗
19. Effect of heat treatment on microstructure and mechanical properties of a new β high strength titanium alloy10.1016/j.matdes.2013.09.070 ↗
20. Effects of initial forming temperature on primary alpha evolution during radial-axial ring rolling for TA15 titanium alloy10.1016/j.proeng.2014.09.163 ↗
21. Effect of aging heat treatment on microstructure and tensile properties of a new β high strength titanium alloy10.1016/j.jallcom.2013.10.096 ↗
22. Effects of different annealing cooling methods on the microstructure and properties of TA10 titanium alloys10.1016/j.jmrt.2022.04.149 ↗
23. Dynamic and post-dynamic recrystallization under hot, cold and severe plastic deformation conditions10.1016/j.pmatsci.2013.09.002 ↗
24. Martensitic twinning transformation mechanism in a metastable IVB element-based body-centered cubic high-entropy alloy with high strength and high work hardening rate10.1016/j.jmst.2022.03.005 ↗
25. Sensitivity of heterogeneous microstructure evolution and preferential variant selection to thermomechanical conditions in a near α titanium alloy10.1016/j.jallcom.2023.169623 ↗
26. Yttrium segregation induced grain growth inhibition during recrystallisation in binary titanium alloys10.1016/j.msea.2020.139137 ↗
27. Trace Y for as-cast Ti6Al4V to simultaneous enhance strength-ductility10.1016/j.jallcom.2023.169757 ↗
28. Effect of Y content on precipitation behavior, oxidation and mechanical properties of As-Cast high-temperature titanium alloys10.3390/ma16134784 ↗
29. Effect of multilevel lamellar microstructures on notch high cycle fatigue damage micromechanism of TC21 alloy10.1016/j.ijfatigue.2025.109013 ↗
30. Influence of heat treatment conditions on the mechanical properties of Ti–6Al–4V alloy10.1080/00084433.2017.1412557 ↗
31. Yttrium segregation induced grain growth inhibition during recrystallisation in binary titanium alloys10.1016/j.msea.2020.139137 ↗
32. A β-solidifying TiAl alloy reinforced with ultra-fine Y-rich precipitates10.1016/j.scriptamat.2020.10.010 ↗
33. Grain size effects on stress-assisted grain boundary migration in polycrystalline Au thin films under tension10.1016/j.actamat.2025.121330 ↗
34. Deformation structures of pure titanium during shear deformation10.1007/s11661-009-0040-x ↗
35. Effect of temperature and strain rate on the deformation behavior of Ti5321 during hot-compression10.1016/j.jallcom.2021.159938 ↗
36. Dynamic restoration and deformation heterogeneity during hot deformation of a duplex-structure TC21 titanium alloy10.1016/j.msea.2017.11.127 ↗
37. Mechanisms of macrozone elimination and grain refinement of near α Ti alloy via the spheroidization of the Widmannstätten structure10.1016/j.actamat.2023.119339 ↗
38. Hierarchical structure and deformation behavior of a novel multicomponent β titanium alloy with ultrahigh strength10.1016/j.jmst.2021.08.031 ↗
39. Dynamic restoration and deformation heterogeneity during hot deformation of a duplex-structure TC21 titanium alloy10.1016/j.msea.2017.11.127 ↗
40. Rotation bending high cycle fatigue behaviors of TC21 alloy with bimodal microstructure10.1016/j.msea.2024.147397 ↗
41. Influence of multilevel lamellar microstructure on notch high cycle fatigue properties and crack initiation behavior of Ti-55531 alloy10.1016/j.jallcom.2024.177684 ↗
42. Influence of notch root radius on high cycle fatigue properties and fatigue crack initiation behavior of Ti-55531 alloy with a multilevel lamellar microstructure10.1016/j.jmrt.2023.04.211 ↗
43. β-Phase-Induced quasi-cleavage fracture mechanism by dual-phase high-strength titanium alloy at elevated temperature10.3390/cryst12091255 ↗
44. Hierarchically ordered coherent interfaces-driven ultrahigh specific-strength and toughness in a nano-martensite titanium alloy10.1016/j.actamat.2023.119540 ↗
45. Morozova A, Mishnev R, Belyakov A, Kaibyshev R. GRAINED cu-cr-zr ALLOYS AFTER n.d.
46. Effect of annealing on microstructure, texture and hardness of ITER-Specification tungsten analyzed by EBSD, vickers micro-hardness and nano-indentation techniques10.1016/j.jnucmat.2019.07.005 ↗
47. Optimization of quasi-β forging parameters to control trimodal microstructure parameters and performance of TC21 forgings10.1016/j.msea.2024.146824 ↗