Effect of various interlayers in NiTi to TC4 dissimilar joints by magnetic pulse welding

Zhikang Ye, Timing Zhang, Yuhua Chen, Xiaolong Peng, Yunfa Deng, Shiyi Zhang, Yang Shen, Shanlin Wang, Jilin Xie

Abstract

Magnetic pulse welding (MPW) has gained wide attention recently. In this paper, the connection of NiTi/TC4 dissimilar materials was achieved by adding pure Al, Cu, and Ni interlayers using MPW technology, and microstructure characterization and mechanical property tests were conducted to evaluate the joints. The results show that the atomic diffusion in the welding process plays a key role in the interface formation process. The interfacial morphology of joints consists of wavy and flat interfaces, and the mechanical interlocking of the wavy interface gives the joints excellent mechanical properties. The joints with the pure Al interlayer have the best mechanical properties, and the tensile shear force is 2.168 kN; the fracture forms of joints with different interlayers are all ductile fractures. In addition, the calculation results of the edge-to-edge crystal matching model show that the side with the high interface mismatch rate is where the joint failure problem occurs frequently.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Shape Memory Alloy Transformations · Advanced Welding Techniques Analysis · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Laser joining of NiTi to Ti6Al4V using a Niobium interlayer10.1016/j.actamat.2015.12.021 ↗
2. Microstructure and mechanical properties of ultrasonic spot welding TiNi/Ti6Al4V dissimilar materials using pure Al coating10.1016/j.jmapro.2021.02.009 ↗
3. Phase transformation mechanisms of NiTi shape memory alloy during electromagnetic pulse welding of Al/NiTi dissimilar joints10.1016/j.msea.2024.146119 ↗
4. Wire-based electron beam additive manufacturing of NiTiNb shape memory alloy: microstructure, phase-transformation behavior and mechanical properties10.1016/j.msea.2024.146509 ↗
5. Microstructure and mechanical properties of dissimilar NiTi/Ti6Al4V joints via back-heating assisted friction stir welding10.1016/j.jmapro.2021.01.024 ↗
6. Additive manufacturing and mechanical properties of TC4/Inconel 625 functionally graded materials by laser engineered net shaping10.1016/j.msea.2022.144370 ↗
7. Microstructure and mechanical properties of TC4/NiTi bionic gradient heterogeneous alloy prepared by multi-wire arc additive manufacturing10.1016/j.msea.2023.144678 ↗
8. Multi-material wire arc additive manufacturing of a bio-inspired heterogeneous layered NiTi/Nb/Ti6Al4V structure: microstructural evolutions and mechanical properties10.1016/j.msea.2023.145896 ↗
9. Welding and joining of NiTi shape memory alloys: a review10.1016/j.pmatsci.2017.04.008 ↗
10. Fiber laser welding of NiTi to Ti-6Al-4V10.1007/s00170-015-7307-8 ↗
11. Simultaneous enhancement of mechanical and shape memory properties by heat-treatment homogenization of Ti2Ni precipitates in TiNi shape memory alloy fabricated by selective laser melting10.1016/j.jmst.2021.06.019 ↗
12. Strengthening synergies of various interlayers in NiTi toTi6Al4V dissimilar laser joints10.1016/j.jmatprotec.2024.118516 ↗
13. Laser welding of NiTi wires10.1016/j.msea.2006.11.179 ↗
14. Effect of interlayer thickness on microstructure and mechanical properties of as welded Ti6Al4V/Cu/NiTi joints10.1016/j.matlet.2014.06.141 ↗
15. Interfacial microstructure and bonding mechanism of the Al/Ti joint by magnetic pulse welding10.1016/j.scriptamat.2021.114434 ↗
16. Microstructure, mechanical properties and transformation behavior of friction stir welded Ni50.7Ti49.3 alloy10.1016/j.matdes.2020.108491 ↗
17. Process defect analysis and visual detection of aluminum/copper cable joints with magnetic pulse crimping10.1016/j.tws.2024.112110 ↗
18. Innovative design of a separatable coil for tube frame structure in magnetic pulse crimping10.1016/j.jmapro.2024.07.079 ↗
19. Interfacial microstructure and mechanical properties of the Al/Ti joint by magnetic pulse welding10.1016/j.matchar.2022.112462 ↗
20. L12-(Al,Si)3Ti + TiC hybrids reinforced laser welded SiCp/2A14Al joint with extraordinary strength10.1016/j.matchar.2023.113295 ↗
21. Spatial stability analysis of emergent wavy interfacial patterns in magnetic pulsed welding10.1016/j.cirp.2014.03.023 ↗
22. Microstructures and mechanical properties of the welded AA5182/HC340LA joint by magnetic pulse welding10.1016/j.matchar.2018.02.018 ↗
23. Interface characteristics and performance of magnetic pulse welded copper-Steel tubes10.1016/j.jmatprotec.2017.03.001 ↗
24. Laser welding of Ti–6Al–4V to nitinol[J]10.1016/j.matdes.2014.04.078 ↗
25. Enthalpy of formation of Al–Fe–Si alloys II (τ6, τ2, τ3, τ8, τ4)10.1016/S0925-8388(00)00682-4 ↗
26. Edge-to-edge matching and its applications10.1016/j.actamat.2004.11.007 ↗
27. Edge-to-edge matching model for predicting orientation relationships and habit planes—the improvements10.1016/j.scriptamat.2005.01.040 ↗