Investigations of impact force of the Al–Fe–Cr–Ti alloy by high-velocity compaction
Source abstract
Abstract
Aluminum alloy materials are the primary choice for lightweight components. High-velocity compaction (HVC) enhances the density of diverse materials. This study utilizes HVC to enhance the density of aluminum alloy. This work examined the influence of compaction velocity, response time (Γ), compaction times, and height-diameter ratio on the impact force of HVC. The maximum force increased linearly with higher compaction velocity, reaching up to 700 kN when the compaction velocity was 9.4 m/s, alongside achieving a peak relative density of 95%. Investigation into the influence of compaction times on the impact force of HVC revealed that the state of powders were critical factors affecting the magnitude of impact force. When the total compaction energy was consistent, the maximum force from double strokes was observed to be lower compared to single stroke. Furthermore, in double strokes with the same second stroke of 55 mm, it was noted that the maximum force increased with higher velocity during the initial compaction. Additionally, both the maximum force and green density decreased as the height-diameter ratio increased. When the height-diameter was 0.4, the maximum force and green density were higher 251 kN, 0.22 g/cm3 than that of 1.2.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Powder Metallurgy Techniques and Materials · Metal Alloys Wear and Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Microstructural, chemical, and mechanical characterization of extruded Al-Cu-Li rods10.1016/j.matchar.2023.113048 ↗
2. Development and tribological investigation of B4C reinforced AA5082 Aluminum alloy cast composites for automotive applications10.1088/2631-8695/ad1f10 ↗
3. Sinter-swage processing of an Al-Si-Mg-Cu powder metallurgy alloy10.1080/00084433.2021.2023286 ↗
4. Parametric study on the dry sliding wear behaviour of AA6082–T6/TiB2 in situ composites using response surface methodology10.1007/s40430-018-1235-0 ↗
5. Microstructure and mechanical properties of Al-Mg-Li-Sc-Zr alloy processed by spray deposition and thermo-mechanical processes10.1016/j.matchar.2020.110614 ↗
6. Microstructural evolution, precipitation and mechanical properties of ultrafine-grained and coarse-grained 2024 aluminum alloys fabricated by powder metallurgy10.1557/s43578-022-00490-9 ↗
7. Parametric study of the dry sliding wear behaviour of AA6082-T6/SiC and AA6082-T6/B4C composites using RSM10.1007/s12206-018-0105-5 ↗
8. Effects of process parameters on cold spray deposition of Al-6061 alloy10.1007/s11666-022-01456-3 ↗
9. Press-and-sinter processing of a PM counterpart to wrought aluminum 261810.1016/j.jmatprotec.2015.11.011 ↗
10. Thixotropic deformation behavior, rapid spheroidization and solid-liquid homogenization of semi-solid Al0.8Co0.5Cr1.5CuFeNi HEA with multilevel microstructure10.1016/j.scriptamat.2023.115384 ↗
11. Advancements in microstructure, texture characterization, and mechanical properties of powder metallurgy Al-Si-Mg-Fe alloy for engineering applications10.1016/j.jallcom.2023.172941 ↗
12. Deformation behavior, microstructure evolution, phase transformation and plastic instability origin of powder metallurgy Al0.8Co0.5Cr1.5CuFeNi alloy during high temperature deformation10.1016/j.msea.2022.144373 ↗
13. Effect of sintering process on microstructure and properties of Al–Si alloy made by powder metallurgy for electronic packaging application10.1088/2053-1591/acd990 ↗
14. Microstructure evolution and densification behaviour of powder metallurgy Al-Cu-Mg-Si alloy10.1080/00325899.2020.1719688 ↗
15. Role of pre-strain on the corrosion behaviour of Al-Zn-Mg P/M alloy
16. Influence of process conditions on the mechanical and microstructural features of milled Al sintered with rapid heating
17. Metallurgical assessment of an emerging Al-Zn-Mg-Cu P/M alloy10.1016/j.msea.2009.05.039 ↗
18. On hot deformation of aluminium–silicon powder metallurgy alloys10.1179/003258910X12678035166773 ↗
19. Experimental and numerical investigations on electromagnetic powder compaction of aluminium 6061 alloy powder10.1016/j.powtec.2022.117579 ↗
20. A review on high velocity compaction mechanism of powder metallurgy10.1177/00368504211016945 ↗
21. Development of a high-velocity compaction process for polymer powders10.1016/j.polymertesting.2005.06.008 ↗
22. Simulation of high-velocity compaction process with relaxation assists using the discrete element method10.1016/j.powtec.2011.10.054 ↗
23. High velocity compaction of ferrous powder10.1016/j.powtec.2008.12.007 ↗
24. Tribological behaviour of Ti/HA and Ti/SiO2 functionally graded materials fabricated at different strain rates
25. High-velocity compaction of titanium powder and process characterization10.1016/j.powtec.2010.12.026 ↗
26. Thermal properties of Mg-B4C micro and nanocomposites fabricated by static and dynamic compaction methods10.1007/s12666-022-02590-w ↗
27. A novel approach to predict green density by high-velocity compaction based on the materials informatics method10.1007/s12613-019-1724-x ↗
28. Predicting tablet tensile strength with a model derived from the gravitation-based high-velocity compaction analysis data10.1016/j.ijpharm.2019.05.024 ↗
29. Examining mechanical properties of various pharmaceutical excipients with the gravitation-based high-velocity compaction analysis method10.1016/j.ijpharm.2018.01.048 ↗
30. A control method of high impact energy and cosimulation in powder high-velocity compaction10.1155/2018/9141928 ↗
31. Effect of die wall lubrication on high velocity compaction behavior and sintering properties of Fe-based PM alloy10.24425/amm.2020.132806 ↗
32. High-velocity powder compaction: an experimental investigation, modelling, and optimization
33. Fabrication of high-density Zn-bonded Sm-Fe-N bulk magnets via high-velocity compaction10.2320/matertrans.MT-M2021121 ↗
34. Experimental and 3D MPFEM simulation study on the green density of Ti–6Al–4V powder compact during uniaxial high velocity compaction10.1016/j.jallcom.2019.153226 ↗
35. Comparisons between 2D and 3D MPFEM simulations in modeling uniaxial high velocity compaction behaviors of Ti-6Al-4V powder
36. Quantitative investigation on force chain lengths during high velocity compaction of ferrous powder10.1142/S0217984919501136 ↗
37. Numerical investigation into the densification of ferrous powder in high velocity compaction10.1088/1402-4896/ab8580 ↗
38. Experimental investigation on stress and die-wall frictional characteristics of metal powder during high-velocity compaction
39. Characteristic analysis of the stress propagation of metal powder in high velocity compaction using DEM10.7566/JPSJ.89.044602 ↗
40. Investigation of the flow and force chain characteristics of metal powder in high-velocity compaction based on a discrete element method10.1007/s40042-021-00241-9 ↗
41. Study on the impact force and green properties of high-velocity compacted aluminum alloy powder10.1007/s12613-012-0678-z ↗
42. A study of the functionally graded (Magnesium/Titanium dioxide) material's mechanical and tribological characteristics fabricated at various compaction loading rates10.1007/s12666-023-03072-3 ↗
43. Effects of compaction velocity on the sinterability of Al-Fe-Cr-Ti PM alloy10.3390/ma12183005 ↗
44. Effect of multiple impacts on high velocity pressed iron powder10.1016/j.powtec.2009.05.028 ↗
45. Miner rule considering fuzziness of stress damage under different load sequences
46. The effect of particle size on microstructure, relative density and indentation load of Mg-B4C composites fabricated at different loading rates10.1177/0021998319896009 ↗
47. Effects of annealing on high velocity compaction behavior and mechanical properties of iron-base PM alloy10.1016/j.powtec.2015.10.040 ↗
48. Effect of impact force on Ti-10Mo alloy powder compaction by high velocity compaction technique
49. Metallurgical assessment of a hypereutectic aluminum-silicon P/M alloy10.1016/j.jmatprotec.2009.07.007 ↗