journal article·2022-09Open access

Effect of organic film on magnetite deposition behavior of alloy 690 steam generator tubes in simulated PWR secondary system

Yong-Beom Lee, Soon-Hyeok Jeon, Byung Joon Bae, Do Haeng Hur, Jong Hyeon Lee

Abstract

The purpose of this study is to elucidate the effect of a film forming amine (FFA) on the magnetite deposition behavior of Alloy 690 tube in the secondary coolant system of pressurized water reactors. By the addition of octadecylamine (ODA), which is a FFA, an organic film with a petal-like form was evenly formed on the surface of the steam generator (SG) tube. Regardless of the addition of ODA, all simulated deposits were verified as magnetite and had a polyhedral or spherical shape. The amount of deposits on the film-formed SG tube was reduced by approximately 58% compared to the deposits on the as-received SG tube. The influence of the film-formed surface of the SG tube is discussed from the point of view of wettability, zeta potentials, and resistance of the electric double layer.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aerosol Filtration and Electrostatic Precipitation · Cyclone Separators and Fluid Dynamics · Recycling and Waste Management Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (73)

Show source-provided references
1. Odar · 2017
2. The chemistry and properties of organic boiler feedwater additives based on film-forming amines and their use in steam generators
3. Betova · 2014
4. Fruzzetti · 2019
5. Studying the processes relating to oxidation of organic substances contained in the coolant of thermal and nuclear power stations10.1134/S0040601510070037 ↗
6. Corrosion behavior of carbon steel coated with octadecylamine in the secondary circuit of a pressurized water reactor10.1007/s11665-017-3035-6 ↗
7. Sipilä · 2014
8. Fouling of nuclear steam generators: fundamental studies, operating experience and remedial measures using chemical additives10.12943/ANR.2013.00007 ↗
9. Choi · 2016
10. Environmental implications of hydroxyl radicals (OH)10.1021/cr500310b ↗
11. Kaur · 2019 · 129
12. Iron oxide catalysts: fenton and fenton-like reactions-a review10.1180/claymin.2012.047.3.01 ↗
13. Experimental study on critical heat flux of highly efficient soft hydrophilic CuO-chitosan nanofluid templates10.1016/j.ijheatmasstransfer.2016.04.096 ↗
14. Dependence of bubble behavior in subcooled boiling on surface wettability10.1016/j.nucengdes.2010.03.016 ↗
15. Wettability and boiling heat transfer study of black silicon surface produced using the plasma immersion ion implantation method10.1016/j.applthermaleng.2016.01.051 ↗
16. Factors affecting zeta potential of iron oxides10.1080/08827508.2011.604697 ↗
17. Measuring surface zeta potential using phase analysis light scattering in a simple dip cell arrangement10.1016/j.colsurfa.2011.12.065 ↗
18. Zeta potential
19. Effect of aluminum oxide coated on fuel cladding surface on crud deposition in simulated PWR primary water10.1016/j.anucene.2018.08.022 ↗
20. Synthesis of nanocrystalline iron oxide particles in the iron(III) acetate/alcohol/acetic acid system10.1002/ejic.200700986 ↗
21. Sonochemical synthesis and characterization of pure nanometer-sized Fe3O4 particles10.1016/S0921-5093(00)00647-X ↗
22. Surface analysis of titanium cleaning and activation processes: non-thermal plasma versus other techniques10.1007/s11090-014-9552-2 ↗
23. Solvent-free one-step covalent functionalization of graphene oxide and nanodiamond with amines10.1039/C6RA22658B ↗
24. The adsorption and decomposition of methylamine on Pd{11110.1016/0039-6028(94)00817-5 ↗
25. Cleavage of NH bonds by active oxygen on Ag(111). Ⅱ. selective oxidation of ethylamine to acetonitrile10.1016/0039-6028(90)90154-Z ↗
26. Adhesion of vapour phase deposited ultra-thin film polymide films on polycrystalline silver10.1016/0039-6028(88)90276-2 ↗
27. Structure and chemical state of octadecylamine self-assembled monolayers on mica10.1021/jp203871g ↗
28. Electrostatic induced molecular tilting in self-assembled monolayers of n-octadecylamine on mica10.1021/jp300829g ↗
29. Short-time oxidation of Alloy 690 in high-temperature and high-pressure steam and water10.1016/S1005-0302(12)60098-X ↗
30. Electrochemical and XPS investigation of the corrosion behavior of Alloy 690 at high-temperature water10.1007/s10008-015-2856-1 ↗
31. Analysis of XPS spectra of Fe2+ and Fe3+ ions in oxide materials10.1016/j.apsusc.2007.09.063 ↗
32. Preparation and structure of graphite oxide functionalized with 1-aminopyrene10.7209/tanso.2016.57 ↗
33. Hydrogen effects on the electronic and microstructural properties of Ce, Ni and CeNi2 intermetallic compound10.1016/0039-6028(94)90478-2 ↗
34. X-ray photoelectron spectroscopy investigation of pumice-supported nickel catalysts10.1002/sia.740230408 ↗
35. ESCA investigation of some NiO/SiO2 and NiO-Al2O3/SiO2 catalysts10.1016/0368-2048(79)80023-7 ↗
36. X-ray photoelectron spectroscopy of some nickel dithiolate complexes10.1021/ja00769a073 ↗
37. Characterization of β-Ni(OH)2 by XPS10.1116/1.1247754 ↗
38. Combination analysis of metal oxide using EDCA, AES, and SIMS10.1116/1.569543 ↗
39. Surface chemistry of chromia-pillared tin and zirconium phosphate materials: an X-ray photoelectron spectroscopic study10.1039/jm9920201175 ↗
40. Photoreduction of hexavalent chromium during X-ray photoelectron spectroscopy analysis of electrochemical and thermal films10.1149/1.2085340 ↗
41. Polyvanadochromic acid
42. A study of the electronic structure of Fe3C, Fe3Al, and Fe3Si by X-ray photoelectron spectroscopy10.1016/0368-2048(75)80039-9 ↗
43. X-ray photoelectron spectroscopic studies of iron oxides10.1021/ac50019a016 ↗
44. Evaluation of octadecylamine for the corrosion inhibition of Incoloy 80010.1080/1478422X.2020.1815950 ↗
45. Elucidating the effect of precursor decomposition time on the structural and optical properties of copper(i) nitride nanocubes10.1039/C9RA09546B ↗
46. Structural properties and Raman spectroscopy of lipid Langmuir monolayers at the air-water interface10.1016/j.colsurfb.2004.12.021 ↗
47. Quantitative correlation of Raman spectral indicators in determining conformational order in alkyl chains10.1021/jp014311n ↗
48. Surface Raman scattering of self-assembled monolayers from 1-alkanethiols at Ag10.1021/ja00010a001 ↗
49. Nondestructive characterization of the polycarbonate-octadecylamine interface by surface enhanced Raman spectroscopy10.1016/j.polymertesting.2018.11.023 ↗
50. Adsorption behaviour of film-forming amine on pre-oxidized carbon steel surface10.1016/j.net.2021.10.025 ↗
51. Effect of octadecylamine concentration on adsorption on carbon steel surface10.1016/j.net.2020.03.026 ↗
52. Evaluation of octadecylamine for the corrosion inhibition of Incoloy 80010.1080/1478422X.2020.1815950 ↗
53. Impedance analysis of film-forming amines for the corrosion protection of a carbon steel10.1016/j.electacta.2018.06.189 ↗
54. Elimelech · 1995
55. Reduced intercalation energy barrier by rich structural water in spinel ZnMn2O4 for high-rate zinc-ion batteries10.1021/acsami.1c05150 ↗
56. Impedance of rough capacitive electrodes10.1016/0022-0728(93)02949-I ↗
57. Varrin · 1996
58. Micro-galvanic corrosion of steam generator materials within pores of magnetite flakes in alkaline solutions10.3390/met8110899 ↗
59. Thermal conductivity of porous materials10.1557/jmr.2013.179 ↗
60. Magnetite-accelerated stress corrosion cracking of alloy 600 in water containing 100 ppm lead oxide at 315 °C10.1016/j.jnucmat.2019.05.024 ↗
61. A detailed model of localized concentration processes in porous deposits of SGs
62. Predicting steam generator crevice chemistry
63. Effect of bare metal surface on the dissolution in aqueous citrate solutions of magnetite films on carbon steel10.1023/A:1018471617720 ↗
64. Synergistic effect of chloride ions and magnetite on the corrosion of Alloy 690 in alkaline solutions10.1016/j.corsci.2017.10.017 ↗
65. Simulation of porous magnetite deposits on steam generator tubes in circulating water at 270 °C10.3390/cryst10090729 ↗
66. Review—factors influencing sulfur induced corrosion on the secondary side in pressurized water reactors (PWRs)10.1149/2.0531902jes ↗
67. formation and consolidation of hard sludge under secondary circuit conditions
68. Factors affecting the consolidation of steam generator sludge10.5006/C1993-93386 ↗
69. Physical and chemical factors affecting sludge consolidation
70. Characteristics of steam generator tube deposits in an operating pressurized water reactor10.1016/j.jnucmat.2018.05.001 ↗
71. Fruzzetti · 2003
72. Role of surface chemistry in crud deposition on heat transfer surface10.5006/0010-9312-35.8.345 ↗
73. Determining zeta potential of magnetite particles in PWR secondary side water treated with ammonia or ethanolamine by using streaming potential technique