journal article·2020-10-27

Low-Temperature Fabrication (≤150 °C) of High-Quality Sputtered Silicon Oxide Thin Film with Hydrogen Plasma Treatment

Taewon Seo, Hyuk Park, Gilsu Jeon, Juyoung Yun, Seongmin Park, Suwon Seong, Yoonyoung Chung

ACS Applied Electronic Materials· Volume 2· Issue 10
Publisher page

Abstract

Low-temperature fabrication of thin-film dielectrics is essential for various applications including flexible/stretchable electronics, monolithic three-dimensional integrated circuits, and large-area sensors/displays. Silicon dioxide is one of the most extensively used dielectric materials, but conventional deposition methods such as plasma-enhanced chemical vapor deposition and atomic layer deposition require relatively high temperatures. In this study, a high-quality SiO2 thin film was fabricated at low temperatures below 150 °C using sputtering and hydrogen plasma treatment. The sputtered SiO2 thin film exhibited low leakage current (3 × 10–7 A/cm2 at 3 MV/cm) and a high breakdown field (11.33 MV/cm). After hydrogen plasma treatment was carried out under optimized conditions, the interface trap density between Si and sputtered SiO2 was minimized to 7 × 1011 cm–2 eV–1, which is comparable to the corresponding value for thermally grown SiO2. The results of X-ray photoelectron spectroscopy and secondary-ion mass spectroscopy confirmed that the hydrogen treatment effectively passivates dangling bonds and reduces the portion of oxygen-deficient species.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Semiconductor materials and devices · ZnO doping and properties · Thin-Film Transistor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Electrical Engineering, Pohang University of Science and Technology, Pohang, Gyeongbuk 37673, Korea

Funding

National Research Foundation of Korea · Pohang University of Science and Technology

References (50)

Show source-provided references
1. 10.1109/led.2011.216156810.1109/led.2011.2161568 ↗
2. 10.1088/0960-1317/12/1/31410.1088/0960-1317/12/1/314 ↗
3. Park, J. E.; Ku, J. H.; Lee, J. W.; Yang, J. H.; Chu, K. S.; Lee, S. H.; Park, M. H.; Lee, N. I.; Kang, H. K.; Suh, K. P.; Cho, B. H.; Kim, B. C.; Shin, C. H. Mass-productive ultra-low temperature ALD SiO2 process promising for sub-90nm memory and logic devices. International Electron Devices 2002 Meeting, Technical Digest, 2002; pp 229–232.
4. 10.1109/jphotov.2011.217329910.1109/jphotov.2011.2173299 ↗
5. 10.1063/1.141903510.1063/1.1419035 ↗
6. 10.1063/1.34031710.1063/1.340317 ↗
7. 10.1063/1.32509610.1063/1.325096 ↗
8. 10.1016/s0040-6090(98)01021-910.1016/s0040-6090(98)01021-9 ↗
9. 10.1063/1.332743010.1063/1.3327430 ↗
10. 10.1063/1.37078410.1063/1.370784 ↗
11. Park, J.H.; Tada, M.; Kuzum, D.; Kapur, P.; Yu, H.Y.; Saraswat, K. C. Low temperature (≤ 380° C) and high performance Ge CMOS technology with novel source/drain by metal-induced dopants activation and high-k/metal gate stack for monolithic 3D integration. 2008 IEEE International Electron Devices Meeting; IEEE, 2008; pp 1–4.10.1109/IEDM.2008.4796702 ↗
12. 10.1109/jproc.2012.219016810.1109/jproc.2012.2190168 ↗
13. 10.1063/1.10662610.1063/1.106626 ↗
14. 10.1063/1.10454710.1063/1.104547 ↗
15. 10.1016/s0042-207x(96)00175-310.1016/s0042-207x(96)00175-3 ↗
16. 10.1109/LED.2010.204997810.1109/LED.2010.2049978 ↗
17. 10.1021/cm030454610.1021/cm0304546 ↗
18. Adams A. C. · Solid State Technol. · 1983 · 26 · 135
19. 10.1063/1.333600910.1063/1.3336009 ↗
20. 10.1143/jjap.43.157110.1143/jjap.43.1571 ↗
21. 10.1149/1.141837910.1149/1.1418379 ↗
22. 10.1021/cm050624+10.1021/cm050624+ ↗
23. 10.1021/am302262510.1021/am3022625 ↗
24. 10.1039/c1jm12227d10.1039/c1jm12227d ↗
25. 10.1016/j.mser.2017.01.00310.1016/j.mser.2017.01.003 ↗
26. 10.1063/1.36357610.1063/1.363576 ↗
27. 10.1016/s0042-207x(02)00388-310.1016/s0042-207x(02)00388-3 ↗
28. 10.1016/j.jnucmat.2013.10.04310.1016/j.jnucmat.2013.10.043 ↗
29. 10.1016/0038-1101(62)90111-910.1016/0038-1101(62)90111-9 ↗
30. 10.1039/c4ra09077b10.1039/c4ra09077b ↗
31. 10.1109/led.2019.293135810.1109/led.2019.2931358 ↗
32. 10.1016/j.tsf.2013.03.06610.1016/j.tsf.2013.03.066 ↗
33. 10.1063/1.326957710.1063/1.3269577 ↗
34. 10.1109/ted.2019.292413510.1109/ted.2019.2924135 ↗
35. 10.4218/etrij.05.0204.002310.4218/etrij.05.0204.0023 ↗
36. 10.1109/led.2019.293135810.1109/led.2019.2931358 ↗
37. 10.1103/physrevb.38.608410.1103/physrevb.38.6084 ↗
38. Moulder, J. F. Handbook of X-ray Photoelectron Spectroscopy; Physical Electronics, 1995; pp 230–232.
39. 10.1116/1.57021810.1116/1.570218 ↗
40. 10.1103/physrevlett.43.168310.1103/physrevlett.43.1683 ↗
41. 10.1063/1.37212510.1063/1.372125 ↗
42. 10.1016/s0169-4332(97)80083-910.1016/s0169-4332(97)80083-9 ↗
43. 10.1016/j.optmat.2003.12.00410.1016/j.optmat.2003.12.004 ↗
44. 10.1116/1.57383310.1116/1.573833 ↗
45. 10.1002/pssr.20100437810.1002/pssr.201004378 ↗
46. 10.1063/1.144816910.1063/1.1448169 ↗
47. 10.1109/jphotov.2015.241913210.1109/jphotov.2015.2419132 ↗
48. 10.3390/ma506100510.3390/ma5061005 ↗
49. Ohdomari, I.; Oshima, M.; Hiraki, A. Control of Semiconductor Interfaces: Proceedings of the First International Symposium, on Control of Semiconductor Interfaces, Karuizawa, Japan, 8–12 November, 1993, 211; Elsevier, 2017.
50. 10.1088/0268-1242/4/12/00310.1088/0268-1242/4/12/003 ↗