Abstract

The isotherm wetting and spreading behaviors of polycrystalline TiC by molten Zr55Cu30Al10Ni5 alloy were investigated at 1133 to 1253 K in a vacuum by using a modified sessile drop method. The system displays good wettability with the initial and final stable contact angles of 44 to 50° and 10 to 14°, respectively, mildly depending on the temperature. The spreading kinetics follows well defined exponential functions and could be described by a molecular dynamic model. On the other hand, a ZrC reaction layer was formed at the interface. The wetting was primarily promoted by the Zr adsorption at the triple junction and then by the formation of the reaction layer.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Glass properties and applications · Phase-change materials and chalcogenides

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. 10.1016/j.cossms.2006.04.00510.1016/j.cossms.2006.04.005 ↗
2. 10.1557/jmr.2006.039310.1557/jmr.2006.0393 ↗
3. 10.1016/j.scriptamat.2004.05.00210.1016/j.scriptamat.2004.05.002 ↗
4. 10.1016/S1359-6454(02)00309-910.1016/S1359-6454(02)00309-9 ↗
5. 10.1016/j.cossms.2006.04.00410.1016/j.cossms.2006.04.004 ↗
6. 10.1021/j100605a00910.1021/j100605a009 ↗
7. 10.1016/0021-9797(79)90081-X10.1016/0021-9797(79)90081-X ↗
8. 10.1063/1.220855010.1063/1.2208550 ↗
9. Kistler · 1993 · 311–429
10. 10.1002/978352761982510.1002/9783527619825 ↗
11. 10.1111/j.1151-2916.2004.tb06376.x10.1111/j.1151-2916.2004.tb06376.x ↗
12. 10.1016/S1359-6454(03)00332-X10.1016/S1359-6454(03)00332-X ↗
13. Storms · 1967 · 8
14. Synthesis and mechanical properties of in situ ZrC reinforced bulk Zr amorphous matrix composites
15. 10.1016/j.scriptamat.2004.10.03110.1016/j.scriptamat.2004.10.031 ↗
16. 10.1007/s11661-008-9718-810.1007/s11661-008-9718-8 ↗
17. Xu · Wettability of molten Zr55Cu30Al10Ni5 on alumina and zirconia · 2007 · 26 · 213
18. 10.1557/JMR.2000.023210.1557/JMR.2000.0232 ↗
19. 10.1016/S1359-6454(97)00047-510.1016/S1359-6454(97)00047-5 ↗
20. 10.1016/j.msea.2006.07.04010.1016/j.msea.2006.07.040 ↗
21. Dynamics of wetting in reactive metal/ceramic systems
22. Bulk metallic glasses
23. 10.1017/S002211208600033210.1017/S0022112086000332 ↗
24. Blake · 1993 · 251–309
25. 10.1002/adem.20070030410.1002/adem.200700304 ↗
26. Wetting phenomena at high temperature (Part III)
27. Iida · 1993
28. 10.1016/S1359-6462(96)00431-910.1016/S1359-6462(96)00431-9 ↗
29. 10.1007/BFb011620010.1007/BFb0116200 ↗
30. 10.1016/j.jallcom.2007.08.04910.1016/j.jallcom.2007.08.049 ↗
31. Wetting behavior of Zr55Cu30Al10Ni5 melt on alumina
32. 10.1016/S1359-6454(00)00231-710.1016/S1359-6454(00)00231-7 ↗
33. 10.1002/adem.200800359)10.1002/adem.200800359) ↗
34. 10.1016/j.cis.2007.04.00910.1016/j.cis.2007.04.009 ↗
35. 10.1016/S1359-6454(99)00103-210.1016/S1359-6454(99)00103-2 ↗