Devitrification inhibitors in borosilicate glass and binary borosilicate glass composite

Jau-Ho Jean, Tapan K. Gupta

Journal of Materials Research· Volume 10· Issue 5
Publisher page

Abstract

Cristobalite is known to precipitate out of borosilicate glass (Corning 7740) and a binary glass mixture of borosilicate glass and high silica glass when these glasses are heated to elevated temperatures. To prevent cristobalite from forming in these glass systems, a devitrification inhibitor needs to be found. Among oxides selected for testing, both Al2O3 and Ga2O3 are found to prevent cristobalite from forming in these glass systems.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Glass properties and applications · Advanced ceramic materials synthesis · Silicon Nanostructures and Photoluminescence

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Jean · J. Mater. Res. · 1994 · 9 · 99910.1557/JMR.1994.0999 ↗
2. Frischat · 1975 · 42
3. 10.1557/JMR.1993.035610.1557/JMR.1993.0356 ↗
4. Imanaka · J. Fujitsu Sci. Tech. · 1989 · 25 · 73
5. Imanaka · J. Ceram. Soc, Jpn. Int. Ed. · 1987 · 95 · 1066
6. Volf · 1961 · 33
7. Volf · 1984
8. Kingery · 1976 · 99
9. Kingery · 1976
10. 10.1038/159162a010.1038/159162a0 ↗
11. 10.1557/JMR.1992.310310.1557/JMR.1992.3103 ↗
12. 10.1111/j.1151-2916.1993.tb03670.x10.1111/j.1151-2916.1993.tb03670.x ↗
13. Jean · IEEE CHMT-Part B: Adv. Packaging · 1994 · 17 · 228
14. Levin · 1964
15. 10.1557/JMR.1992.251410.1557/JMR.1992.2514 ↗
16. 10.2109/jcersj.97.31410.2109/jcersj.97.314 ↗
17. Robie · 1978
18. Volf · 1961 · 132
19. Volf · 1984
20. Kingery · 1976 · 87
21. 10.1557/JMR.1993.176710.1557/JMR.1993.1767 ↗
22. 10.1111/j.1151-2916.1969.tb15855.x10.1111/j.1151-2916.1969.tb15855.x ↗
23. MacDowell · 1990 · 365
24. 10.2109/jcersj.97.30910.2109/jcersj.97.309 ↗
25. Kreidle · 1983
26. Jones · 1956