journal article·2005-10

Nickel silicon thin film as barrier in under-bump-metallization by magnetronsputtering deposition for Pb-free chip packaging

Y. Li, J. Chen, C. Lazik, P. Wang, L. Yang, J. Yu, T. Sun, E. Ko

Journal of Materials Research· Volume 20· Issue 10
Publisher page

Abstract

In the search for a Pb-free compatible under-bump-metallization (UBM) barrier material, magnetron sputtering of a nonmagnetic nickel silicon alloy (NiSi) target was used to deposit a low-stress polycrystalline NiSi thin film. In the reaction with SnAg3.0Cu0.5 solder, NiSi was found to have greatly reduced reaction and intermetallics (IMC) formation rates compared with sputtered NiV. A continuous layer of IMCs in NiSi UBM-solder joint remains stable after 10 reflows and 1000 h thermal aging tests, resulting in preferred bulk solder failure mode in ball shearing/pull testing. Our results demonstrate that NiSi is a highly promising thin film barrier material suitable for Pb-free solder bumping.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (11)

Show source-provided references
1. 10.1557/JMR.2003.018310.1557/JMR.2003.0183 ↗
2. 10.1557/JMR.2004.017010.1557/JMR.2004.0170 ↗
3. Hansen · Constitution of Binary Alloys, · 1959
4. 10.1109/TEPM.2002.80164810.1109/TEPM.2002.801648 ↗
5. 10.1557/JMR.2002.023910.1557/JMR.2002.0239 ↗
6. 10.1063/1.143244310.1063/1.1432443 ↗
7. Poate · 1978
8. 10.1557/JMR.2003.029610.1557/JMR.2003.0296 ↗
9. 10.1016/S0927-796X(02)00007-410.1016/S0927-796X(02)00007-4 ↗
10. 10.1557/JMR.2002.003610.1557/JMR.2002.0036 ↗
11. 10.1016/S0927-796X(01)00029-810.1016/S0927-796X(01)00029-8 ↗