The effects of electropulsing on the recrystallization behavior of rolled pure tungsten
Source abstract
Abstract
Electropulsing treatment (EPT) has been first applied to the recrystallization of a refractory metal—tungsten (W). We have three major observations: (i) the recrystallization temperature of a rolled pure W under EPT is ∼900 K higher than its conventional recrystallization temperature (1603 K); (ii) the time required for recrystallization is significantly reduced compared with that of conventional heat treatment (CHT); (iii) the recrystallized grains are also much finer than the ones under CHT. Based on quantitative analysis, we conclude that the huge increase of the recrystallization temperature of the rolled pure W under EPT is due to the high heating rate generated by EPT and high activation energy for vacancy diffusion of W, and the accelerated recrystallization and grain refinement have resulted from the coupling of thermal and electromigration effects of EPT at relatively high temperatures.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electromagnetic Effects on Materials · Microstructure and mechanical properties · Material Properties and Failure Mechanisms
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. 10.1103/PhysRevB.33.798310.1103/PhysRevB.33.7983 ↗
2. 10.1103/PhysRevB.2.308810.1103/PhysRevB.2.3088 ↗
3. Recrystallization and grain growth behavior of rolled tungsten under VDE-like short-pulse high-heat-flux loads
4. 10.1016/S0921-5093(00)01882-710.1016/S0921-5093(00)01882-7 ↗
5. Nabarro · 1989
6. 10.1103/PhysRevB.57.1118410.1103/PhysRevB.57.11184 ↗
7. Wang · 2008
8. 10.1016/j.jallcom.2011.01.05210.1016/j.jallcom.2011.01.052 ↗
9. 10.1016/S0036-9748(88)80340-510.1016/S0036-9748(88)80340-5 ↗
10. 10.1016/0036-9748(84)90522-210.1016/0036-9748(84)90522-2 ↗
11. 10.1002/047086827910.1002/0470868279 ↗
12. 10.1016/0036-9748(83)90183-710.1016/0036-9748(83)90183-7 ↗
13. 10.1080/0141861830823490110.1080/01418618308234901 ↗
14. 10.1063/1.36832710.1063/1.368327 ↗
15. 10.1016/j.jallcom.2009.07.11410.1016/j.jallcom.2009.07.114 ↗
16. 10.1016/0001-6160(86)90001-510.1016/0001-6160(86)90001-5 ↗
17. Djilkibaev · 1997
18. 10.1016/j.matlet.2003.11.03510.1016/j.matlet.2003.11.035 ↗
19. 10.1081/AMP-20002807010.1081/AMP-200028070 ↗
20. 10.1016/j.jmatprotec.2006.07.01910.1016/j.jmatprotec.2006.07.019 ↗
21. Yu · 2001
22. Zhou · 1988
23. Humphreys · 2004
24. 10.1007/s00339-007-4007-810.1007/s00339-007-4007-8 ↗
25. 10.1016/j.ijrmhm.2005.10.01210.1016/j.ijrmhm.2005.10.012 ↗
26. 10.1016/j.jnucmat.2004.04.00510.1016/j.jnucmat.2004.04.005 ↗
27. 10.1016/j.msea.2011.02.04610.1016/j.msea.2011.02.046 ↗
28. The structure and properties of 08G2S steel wire after electrostimulated drawing