Effect of La and Y on Crystallization Temperatures of Hafnia and Zirconia

Sergey V. Ushakov, Crystalyn E. Brown, Alexandra Navrotsky

Journal of Materials Research· Volume 19· Issue 3
Publisher page

Abstract

Crystallization of amorphous Y- and La-doped HfO2 and ZrO2 nanophase powders was studied using thermal analysis and high-temperature x-ray diffraction. Substantial increase of crystallization temperature of amorphous hafnium and zirconium oxides could be achieved by alloying with La2O3. The crystallization temperature of Hf2La2O7 composition is higher than 900 °C, which makes it a candidate for advanced gate dielectrics. In contrast, Y-doping did not significantly raise the crystallization temperature.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Semiconductor materials and devices · Electronic and Structural Properties of Oxides · Ferroelectric and Piezoelectric Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. 10.1557/JMR.2002.023410.1557/JMR.2002.0234 ↗
2. 10.1063/1.136106510.1063/1.1361065 ↗
3. Wang · Mater. Sci. Eng. A · 1998 · 253M · 106
4. 10.1103/PhysRevB.66.05410810.1103/PhysRevB.66.054108 ↗
5. Pitcher · J. Amer. Cer. Soc.
6. 10.1111/j.1151-2916.1975.tb11476.x10.1111/j.1151-2916.1975.tb11476.x ↗
7. 10.1016/0272-8842(85)90002-110.1016/0272-8842(85)90002-1 ↗
8. 10.1107/S056773947600155110.1107/S0567739476001551 ↗
9. 10.1002/1521-3951(200107)226:1<57::AID-PSSB57>3.0.CO;2-L10.1002/1521-3951(200107)226:1<57::AID-PSSB57>3.0.CO;2-L ↗
10. 10.1038/3502324310.1038/35023243 ↗
11. 10.1016/0390-5519(75)90032-010.1016/0390-5519(75)90032-0 ↗
12. Ushakov · 2003 · 745 · 3
13. 10.1016/S0167-9317(03)00291-010.1016/S0167-9317(03)00291-0 ↗
14. 10.1016/S0022-3093(02)00977-810.1016/S0022-3093(02)00977-8 ↗
15. 10.1016/S0022-3093(99)00690-010.1016/S0022-3093(99)00690-0 ↗