journal article·2024-06

Applying High-Pressure Torsion to Deformation of a Recrystallized τ-MnAl Alloy: Results and Problems

A. S. Fortuna, M. V. Gorshenkov, S. O. Rogachev, R. V. Sundeev, A. I. Laptev

Publisher page

Abstract

In this study, the effect of high-pressure torsion (HPT) on the structure, phase composition and magnetic properties of ferromagnetic MnAl-C alloy were investigated. τ-phase MnAl disks were treated in two different initial conditions: first, a disk was deformed for 20 revolutions in “as-transformed” state, and second, the deformed disk was recrystallized and then deformed for 20 revolutions again. Repeated deformation produced a coercive force of 2.0 kOe which is significantly lower than the one obtained earlier after first HPT deformation (3.7 kOe). It was demonstrated that the low level of the coercive force was associated with the failure to achieve the specified strain during HPT and with deformation inhomogeneity both in depth and along the radius of the sample. This behavior of the material during HPT was due to the high hardness of the τ-MnAl-C ferromagnetic alloy. The article suggests variants for improving the machinability of the alloy to achieve the required strain.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic Properties of Alloys · Microstructure and Mechanical Properties of Steels · Metallic Glasses and Amorphous Alloys

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. J.M.D. Coey, Permanent Magnets: Plugging the Gap, Scr. Mater., 2012, 67, p 524–529. https://doi.org/10.1016/j.scriptamat.2012.04.03610.1016/j.scriptamat.2012.04.036 ↗
2. S. Kontos, A. Ibrayeva, J. Leijon, G. Mörée, A.E. Frost, L. Schönström, K. Gunnarsson, P. Svedlindh, M. Leijon, and S. Eriksson, An Overview of MnAl Permanent Magnets with a Study on Their Potential in Electrical Machines, Energies, 2020, 13, p 5549. https://doi.org/10.3390/en1321554910.3390/en13215549 ↗
3. S. Kojima, K. Kojima, S. Mitani, and T. Kubo, Permanent Magnet, Synopses1978 Autumn Meet Japan, Inst. Met., 1978, 1978, p 245.
4. T. Ohtani, N. Kato, S. Kojima, K. Kojima, Y. Sakamoto, I. Konno, M. Tsukahara, and T. Kubo, Magnetic Properties of Mn-Al-C Permanent Magnet Alloys, IEEE Trans. Magn., 1977, 13, p 1328–1330. https://doi.org/10.1109/tmag.1977.105957410.1109/tmag.1977.1059574 ↗
5. L. Feng, J. Freudenberger, T. Mix, K. Nielsch, and T.G. Woodcock, Rare-earth-Free MnAl-C-Ni Permanent Magnets Produced by Extrusion of Powder Milled from Bulk, Acta Mater., 2020, 199, p 155–168. https://doi.org/10.1016/j.actamat.2020.08.03110.1016/j.actamat.2020.08.031 ↗
6. H. Dehghan, S.A. Seyyed Ebrahimi, and M. Nosko, Mater, Strain-Induced Phase Transformation of an Mn-Al Alloy during Hot Compression, Sci. Eng: A., 2019, 751, p 271–282. https://doi.org/10.1016/j.msea.2019.02.08210.1016/j.msea.2019.02.082 ↗
7. L. Feng, J. Freudenberger, K. Nielsch, and T.G. Woodcock, Enhanced Thermal Stability of the -Phase in MnAl-C Alloys with Ni Additions, J. Alloys Compd., 2022, 897, p 163248. https://doi.org/10.1016/j.jallcom.2021.16324810.1016/j.jallcom.2021.163248 ↗
8. P.Z. Si, H.D. Qian, C.J. Choi, J. Park, and H.L. Ge, A Novel Method for Measuring the Phase Transformation Temperature and Enhanced Coercivity in Cold-Rolled MnAlCx (x = 0–5) Alloys, J. Magn. Magn. Mater., 2018, 451, p 540–545. https://doi.org/10.1016/j.jmmm.2017.11.09410.1016/j.jmmm.2017.11.094 ↗
9. J. Rial, P. Švec, P. Švec Sr., A. Bollero, and S. Deledda, Coercivity Development in MnAl Ribbons by Microstructural Modifications Achieved Through Cold-Rolling Process, J. Magn. Magn. Mater., 2021, 529, p 167826. https://doi.org/10.1016/j.jmmm.2021.16782610.1016/j.jmmm.2021.167826 ↗
10. V.V. Popov Jr., F. Maccari, I.A. Radulov, A. Kovalevsky, A. Katz-Demyanetz, and M. Bamberger, Microstructure and Magnetic Properties of Mn-Al-C Permanent Magnets Produced by Various Techniques, Manuf. Rev., 2021, 8, p 10. https://doi.org/10.1051/mfreview/202100810.1051/mfreview/2021008 ↗
11. Y. Jia, Y. Wu, S. Zhao, S. Zuo, K.P. Skokov, O. Gutfleisch, C. Jiang, and H. Xu, L10 Rare-Earth-FRee Permanent Magnets: The Effects of Twinning Versus Dislocations in Mn-Al Magnets, Phys. Rev. Mater., 2020, 4, p 094402. https://doi.org/10.1103/PhysRevMaterials.4.09440210.1103/PhysRevMaterials.4.094402 ↗
12. M.V. Gorshenkov, D.Y. Karpenkov, R.V. Sundeev, V.V. Cheverikin, and I.V. Shchetinin, Magnetic Properties of Mn-Al Alloy After HPT Deformation, Mater. Lett., 2020, 272, p 127864. https://doi.org/10.1016/j.matlet.2020.127864410.1016/j.matlet.2020.1278644 ↗
13. A.S. Fortuna, M.V. Gorshenkov, and R.V. Sundeev, The Effect of High-Pressure Torsion on the Structure and Long-Range Order of Ferromagnetic s-MnAl Alloy, Mater. Lett., 2021, 296, p 129888. https://doi.org/10.1016/j.matlet.2021.12988810.1016/j.matlet.2021.129888 ↗
14. F. Bittner, J. Freudenberger, L. Schultz, and T.G. Woodcock, The Impact of Dislocations on Coercivity in L10-MnAl, J. Alloy. Compd., 2017, 704, p 528–536. https://doi.org/10.1016/j.jallcom.2017.02.02810.1016/j.jallcom.2017.02.028 ↗
15. M. Gusenbauer, A. Kovacs, H. Oezelt, J. Fischbacher, P. Zhao, T.G. Woodcock, and T. Schrefl, Insights into MnAl-C Nano-Twin Defects by Micromagnetic Characterization, J. Appl. Phys., 2021, 129, p 093902. https://doi.org/10.1063/5.003538710.1063/5.0035387 ↗
16. A.S. Fortuna, M.V. Gorshenkov, V.V. Cheverikin, and R.V. Sundeev, Influence of Annealing on the Microstructure and Magnetic Properties of the -MnAl Alloy Deformed by High Pressure Torsion, J. Alloys Compd., 2022, 901, p 163424. https://doi.org/10.1016/j.jallcom.2021.16342410.1016/j.jallcom.2021.163424 ↗
17. E.V. Shelekhov and T.A. Sviridova, Programs for X-ray Analysis of Polycrystals, Met. Sci. Heat Treat., 2000, 42, p 309–313. https://doi.org/10.1007/BF0247130610.1007/BF02471306 ↗
18. H. Fang, S. Kontos, J. Ångström, J. Cedervall, P. Svedlindh, K. Gunnarsson, and M. Sahlberg, Directly Obtained -Phase MnAl, a High Performance Magnetic Material for Permanent Magnets, J. Solid State Chem., 2016, 237, p 300–306. https://doi.org/10.1016/j.jssc.2016.02.03110.1016/j.jssc.2016.02.031 ↗
19. J.Z. Wei, Z.G. Song, Y.B. Yang, S.Q. Liu, H.L. Du, J.Z. Han, D. Zhou, C.S. Wang, Y.C. Yang, A. Franz, D. Többens, and J.B. Yang, −MnAl with High Coercivity and Saturation Magnetization, AIP Adv., 2014, 4, p 127113. https://doi.org/10.1063/1.490377310.1063/1.4903773 ↗
20. A. Aharoni, Demagnetizing Factors for Rectangular Ferromagnetic Prisms, J. Appl. Phys., 1998, 83, p 3432.10.1063/1.367113 ↗
21. J. Thielsch, F. Bittner, and T.G. Woodcock, Magnetization Reversal Processes in Hot-Extruded -MnAl-C, J. Magn. Magn. Mater., 2017, 426, p 25–31. https://doi.org/10.1016/j.jmmm.2016.11.04510.1016/j.jmmm.2016.11.045 ↗
22. B.B. Straumal, V. Pontikis, A.R. Kilmametov, A.A. Mazilkin, S.V. Dobatkin, and B. Baretzky, Competition Between Precipitation and Dissolution in Cu-Ag Alloys under High Pressure Torsion, Acta Mater., 2017, 122, p 60–71. https://doi.org/10.1016/j.actamat.2016.09.02410.1016/j.actamat.2016.09.024 ↗
23. A.M. Glezer, I.A. Timshin, I.V. Shchetinin, M.V. Gorshenkov, R.V. Sundeev, and A.G. Ezhova, Unusual Behavior of Long-Range order Parameter in Fe3Al Superstructure under Severe Plastic Deformation in Bridgman Anvils, J. Alloys Compd., 2018, 744, p 791–796. https://doi.org/10.1016/j.jallcom.2018.02.12410.1016/j.jallcom.2018.02.124 ↗
24. Y. Jia, H. Ding, Y. Wu, J. Wang, H. Wu, T. Ma, S. Zhao, K.P. Skokov, A. Aubert, F. Maccari, O. Gutfleisch, Y. Xu, J. Niu, B. Qiao, S. Zhao, and C. Jiang, On the ε → Phase Transformation and Twinning in L10−MnAl Alloys, Acta Mater., 2022, 232, p 117892. https://doi.org/10.1016/j.actamat.2022.11789210.1016/j.actamat.2022.117892 ↗
25. F. Bittner, L. Schultz, and T.G. Woodcock, Twin-Like Defects in L10 Ordered s-MnAl-C Studied by EBSD, Acta Mater., 2015, 101, p 48–54. https://doi.org/10.1016/j.actamat.2015.08.04410.1016/j.actamat.2015.08.044 ↗
26. G. Faraji, H.S. Kim, H.T. Kashi, Severe Plastic Deformation Methods, 1st edition, in Processing and Properties, Elsevier, 2018, p 38–42.10.1016/B978-0-12-813518-1.00020-5 ↗
27. K. Edalati, Z. Horita, and T.G. Langdon, The Significance of Slippage in Processing by High-Pressure Torsion, Scr. Mater., 2009, 60, p 9–12. https://doi.org/10.1016/j.scriptamat.2008.08.04210.1016/j.scriptamat.2008.08.042 ↗
28. S.O. Rogachev, S.A. Nikulin, V.M. Khatkevich, R.V. Sundeev, and D.A. Kozlov, High-Pressure Torsion Deformation Process of Bronze/Niobium Composite, Trans. Nonferrous Met. Soc. China., 2019, 29, p 1689–1695. https://doi.org/10.1016/S1003-6326(19)65075-210.1016/S1003-6326(19)65075-2 ↗
29. Y. Sakka, M. Nakamura, and K. Hoshimoto, Rapid Quenching and Properties of Hard Magnetic Materials in MnAI-X (X = Ti, Cu, Ni, C, B) Systems, J. Mater. Sci., 1989, 24, p 4331–4338.10.1007/BF00544507 ↗
30. K. Lee, S.-J. Park, J. Lee, J. Moon, J.-Y. Kang, D.-I. Kim, J.-Y. Suh, and H.N. Han, Effect of Aging Treatment on Microstructure and Intrinsic Mechanical Behavior of Fe–31.4Mn–11.4Al–0.89C Lightweight Steel, J. Alloys Compd., 2016, 656, p 805–811. https://doi.org/10.1016/j.jallcom.2015.10.01610.1016/j.jallcom.2015.10.016 ↗