journal article·2020-03

Decomposition of Supersaturated Solid Solution during Non-isothermal Aging and Its Effect on the Physical Properties and Microstructure of the Ag-Cu7.5 Alloy

Grzegorz Wloch, Krystian Sokolowski, Pawel Ostachowski, Anna Wicher, Jakub Sobota

Publisher page

Abstract

The aim of the study was to examine the effect of supersaturated solid solution decomposition during non-isothermal aging on the microstructure and selected physical and mechanical properties of the Ag-7.5 wt.% Cu alloy. The decomposition mechanism was determined by complex research methods, i.e., physical properties testing, microstructure examinations, as well as hardness measurement. Decomposition of Ag-Cu7.5 supersaturated solid solution during heating has two stages. The first stage involves a significant increase in hardness and has no effect on electrical conductivity. During the second stage, growth of discontinuous precipitates and an increase in hardness and electrical conductivity are observed. Discontinuous precipitation cells consist of βCu rods and plates surrounded by αAg phase. Obtained activation energy of this microstructural evolution is lower than its values presented in the literature.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Solidification and crystal growth phenomena · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. A.L. Norbury, The Effect of Quenching and Tempering on the Mechanical Properties of Standard Silver, J. Inst. Met., 1928, 39, p 145–172
2. V.N. Ageew, M. Hansen, and G. Sachs, Entmischung und Eigenschaftsanderungen ubersattigter Silber-Kupferlegierungen, Z. Angew. Phys., 1930, 66, p 350–376 ((in German))
3. C.S. Barrett, H.F. Kaiser, and R.F. Mehl, Studies Upon the Widmanstatten Structure VII: The Copper–Silver System, Trans. Am. Inst. Min. Metall. Pet. Eng., 1935, 117, p 39–60
4. W.F. Cox and C. Sykes, Precipitation in the Alloys of Copper and Silver during Age-Hardening, J. Inst. Met., 1940, 66, p 381–387
5. M.L.V. Gayler and W.E. Carrington, Metallographic Study of the Precipitation of Copper from a Silver-Rich Silver-Copper Alloy, J. Inst. Met., 1947, 73, p 625–639
6. W. Scharfenberger, G. Schmitt, and H. Borchers, Uber die Kinetik der Diskontinuierlichen Ausscheidung der Silberlegierung mit 7, 5 Gew-%Cu, Z. Metall., 1972, 63, p 553–560 (in German)
7. F.W. Jones, P. Leech, and C. Sykes, Precipitation in Single Crystals of Silver-Rich and Copper-Rich Alloys of the Silver–Copper System, Proc. R. Soc. A, 1942, 181, p 154–168. https://doi.org/10.1098/rspa.1942.006810.1098/rspa.1942.0068 ↗
8. W. Leo, Elektronenmikroskopische Untersuchungen zur Ausscheidung in aushärtbaren Silber-Kupfer-Legierungen, Z. Metall., 1967, 58, p 456–461
9. R.G. Rose, The Precipitation of Copper from a Silver-5,5% Copper Solid Solution at 220 °C, Acta Metall., 1957, 5, p 404–405. https://doi.org/10.1016/0001-6160(57)90010-X10.1016/0001-6160(57)90010-X ↗
10. W. Gust, B. Predel, and K. Diekstall, Experimentelle Ermittlung von drei metastabilen löslichkeitslinien auf der Ag-seite des zustandsdiagramms Ag-Cu, Acta Metall., 1978, 26, p 241–245. https://doi.org/10.1016/0001-6160(78)90124-410.1016/0001-6160(78)90124-4 ↗
11. S.B. Youssef, Resistometric Study of Ag-8 at % Cu Alloy Aged in the Temperature Range 0.4-0.65 Tm, Phys. B, 1996, 228(3-4), p 337–34110.1016/S0921-4526(96)00497-8 ↗
12. S. Colombo, P. Battaini, and G. Airoldi, Precipitation Kinetics in Ag—7.5 wt.% Cu Alloy Studied by Isothermal DSC and Electrical-Resistance Measurements, J. Alloys Compd., 2007, 437(1-2), p 107–112. https://doi.org/10.1016/j.jallcom.2006.07.07610.1016/j.jallcom.2006.07.076 ↗
13. D. Hamana and L. Boumaza, Precipitation Mechanism in Ag—8 wt.% Cu Alloy, J. Alloys Compd., 2009, 477(1-2), p 217–223. https://doi.org/10.1016/j.jallcom.2008.10.06310.1016/j.jallcom.2008.10.063 ↗
14. A. Korbel, W. Bochniak, in Method of Plastic Forming of Materials, European Patent, EP0711210B1 (2000)
15. A. Korbel, W. Bochniak, P. Ostachowski, and L. Błaż, Visco-Plastic Flow of Metal in Dynamic Conditions of Complex Strain Scheme, Metall. Mater. Trans. A, 2011, 42(9), p 2881–2897. https://doi.org/10.1007/s11661-011-0688-x10.1007/s11661-011-0688-x ↗
16. B. Predel, Phase Equilibria, Crystallographic and Thermodynamic Data of Binary Alloys, Springer, Berlin, 1998
17. Website of DSC Curve Solutions (DCS®) and Non-isothermal Kinetics. http://www.caotechnology.com.au/nonisothermal.htm. Accessed on 16 July 2018
18. D. Hamana, M. Hachouf, L. Boumaza, and Z.E.A. Biskri, Precipitation Kinetics and Mechanism in Cu-7 wt.% Ag Alloy, Mater. Sci. Appl., 2011, 2(7), p 899–910. https://doi.org/10.4236/msa.2011.2712010.4236/msa.2011.27120 ↗
19. I. Manna, S.K. Pabi, and W. Gust, Discontinuous Reactions in Solids, Int. Mater. Rev., 2013, 46, p 53–91. https://doi.org/10.1179/09506600110152840210.1179/095066001101528402 ↗
20. W. Gust, B. Predel, and K. Diekstall, Zur diskontinuierlichen Ausscheidung in Silber-6.2 at.%-Kupfer-Dreikristallen, Z. Metall., 1978, 69, p 75–80 (in German)
21. W. Gust, B. Predel, and K. Diekstall, Zur diskontinuierlichen Ausscheidung in Silber-6.2 at.%-Kupfer-Dreikristallen, Z. Metall., 1978, 69, p 445–449 (in German)
22. A. Pawlowski and P. Zieba, Diffusion Processes During Discontinuous Precipitation, Arch. Metall., 1990, 35, p 401–407
23. D.B. Williams and E.P Butler, Grain Boundary Discontinuous Precipitation Reactions, Int. Mater. Rev., 1981, 26, p 153–183. https://doi.org/10.1179/imtr.1981.26.1.15310.1179/imtr.1981.26.1.153 ↗