The friction and wear behaviors of TiAl matrix self-lubricating composites (TMSC) with MoO3 tabular crystal (MTC) against GCr15 steel ball are tested using a constant load of 10 N and a constant speed of 0.2 m/s from room temperature to 600 °C. The result shows that, during the sliding friction and wear process, the MTC which has the microstructure of multiple layers could reduce the shear stress, leading to the reduction of friction coefficient. Meanwhile, TMSC with MTC exhibits the excellent tribological performance over a wide temperature range, if compared to TiAl based alloy. Moreover, MTC can improve the tribological properties of TMSC obviously below 400 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. A. Rastkar and B. Shokri, A Multi-Step Process of Oxygen Diffusion to Improve the Wear Performance of a Gamma-Based Titanium Aluminide, Wear, 2008, 264(11-12), p 973–97910.1016/j.wear.2007.07.001 ↗
2. G. Das, H. Kestler, H. Clemens, and P. Bartolotta, Sheet Gamma TiAl: Status and Opportunities, JOM, 2004, 56(11), p 42–4510.1007/s11837-004-0251-y ↗
3. G. Das, P.A. Bartolotta, H. Kestler and H. Clemens, Gamma Titanium Aluminides, Y. W. Kim, H. Clemens, and A. H. Rosenberger, Eds. (Berlin), Springer, 2003
4. T. Tetsui and S. Ono, Endurance and Composition and Microstructure Effects on Endurance of TiAl Used in Turbochargers, Intermetallics, 1999, 7(6), p 689–69710.1016/S0966-9795(98)00085-5 ↗
5. K. Gebauer, Performance, Tolerance and Cost of TiAl Passenger Car Valves, Intermetallics, 2006, 14(4), p 355–36010.1016/j.intermet.2005.08.009 ↗
6. F. Apple and R. Wagner, Microstructure and Deformation of Two-Phase γ-titanium Aluminides, Mater. Sci. Eng. R, 1998, 22(5), p 187–26810.1016/S0927-796X(97)00018-1 ↗
7. A. Rastkar, A. Bloyce, and T. Bell, Sliding Wear Behaviour of Two Gamma-Based Titanium Aluminides, Wear, 2000, 240(1-2), p 19–2610.1016/S0043-1648(00)00334-3 ↗
8. C. Li, J. Xia, and H. Dong, Sliding Wear of TiAl Intermetallics Against Steel and Ceramics of Al2O3, Si3N4 and WC/Co, Wear, 2006, 261(5-6), p 693–70110.1016/j.wear.2006.01.044 ↗
9. K. Miyoshi, B. Lerch, and S. Draper, Fretting Wear of Ti-48Al-2Cr-2Nb, Tribol. Int., 2003, 36(2), p 145–15310.1016/S0301-679X(02)00142-1 ↗
10. W. Wang, K. Liu, and M.H. Jiao, Thermal and Non-Newtonian Analysis on Mixed Liquid-Solid Lubrication, Tribol. Int., 2007, 40(7), p 1067–107410.1016/j.triboint.2006.10.004 ↗
11. H. Lee, N. Lee, Y. Seo, J. Eom, and S.W. Lee, Comparison of Frictional Forces on Graphene and Graphite, Nanotechnology, 2009, 20, p 5701–5706
12. T. Filleter, J.L. McChesney, A. Bostwick, E. Rotenberg, K.V. Emtsev, T.H. Seyller, K. Horn, and R. Bennewitz, Friction and Dissipation in Epitaxial Graphene Films, Phys. Rev. Lett., 2009, 102, p 6102–610510.1103/PhysRevLett.102.086102 ↗
13. S. Mahathanabodee, T. Palathai, S. Raadnui, R. Tongsri, and N. Sombatsompop, Dry Sliding Wear Behavior of SS316L Composites Containing h-BN and MoS2 Solid Lubricants, Wear, 2014, 316(1-2), p 37–4810.1016/j.wear.2014.04.015 ↗
14. X.M. Fan, X.W. Yin, S.S. He, L.T. Zhang, and L.F. Cheng, Friction and Wear Behaviors of C/C-SiC Composites Containing Ti3SiC2, Wear, 2012, 274-275(27), p 188–19510.1016/j.wear.2011.08.029 ↗
15. Y.Z. Lyu, Y. Zhu, and U. Olofsson, Wear Between Wheel and Rail: A Pin-on-Disc Study of Environmental Conditions and Iron Oxides, Wear, 2015, 328-329, p 277–28510.1016/j.wear.2015.02.057 ↗
16. D.F. Lu and K. Chen, Preparation of SiC Tabular Crystal by Grinding, J. South China Univ. Technol., 1996, 24, p 16–22
17. Z.J. Zhou, Y.J. Gou, and Z.F. Yang, Friction and Wear Characteristics of Y-TZP/Alumina (Platelet) Composites, Tribology, 2007, 27, p 166–171
18. D.S. Xiong, Lubrication Behavior of Ni-Cr Based Alloys Containing MoS2 at High Temperature, Wear, 2001, 251(1-12), p 1094–109910.1016/S0043-1648(01)00803-1 ↗
19. M. Chhowalla and G.A. Maratunga, Thin Films of Fullerene-Like MoS2 Nanoparticles with Ultra-Low Friction and Wear, Nature, 2000, 407(6801), p 164–16710.1038/35025020 ↗
20. H.C. Zeng, Vapour Phase Growth of Orthorhombic Molybdenum Trioxide Crystals at Normal Pressure of Purified Air, J. Cryst. Growth, 1998, 186(3), p 393–40210.1016/S0022-0248(97)00493-4 ↗
21. S. Balakumar and H.C. Zeng, Growth Modes in Vapour-Phase Prepared Orthorhombic Molybdenum Trioxide Crystals, J. Cryst. Growth, 1999, 197(1-2), p 186–19410.1016/S0022-0248(98)00924-5 ↗