Wear Properties of Hot-Extruded Pure Mg and Mg-1 wt.% SiC Nanocomposite
Source abstract
Abstract
This paper presents the wear properties of hot-extruded pure Mg and its composite reinforced with 1 wt.% SiC nanoparticles. Wear tests were performed under dry and oil sliding conditions using ball-on-flat configuration. It was found that the nanocomposites show much lower wear loss mainly due to hardness improvement caused by the nanoparticles and grain refinement. The wear loss gradually decreases as the sliding speed increases and then it begin to rise beyond a critical value. With the wear temperature improves from 25 to 190 °C, wear loss of nanocomposites reduces.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Magnesium Alloys: Properties and Applications · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. S.F. Hassan and M. Gupta, Development of High Performance Magnesium Nano-composites Using Nano-Al2O3 as Reinforcement, Mater. Sci. Eng. A, 2005, 392, p 163–16810.1016/j.msea.2004.09.047 ↗
2. C.S. Goh, J. Wei, L.C. Lee, and M. Gupta, Properties and Deformation Behaviour of Mg-Y2O3 Nanocomposites, Acta Mater., 2007, 55, p 5115–512110.1016/j.actamat.2007.05.032 ↗
3. K.K. Deng, X.J. Wang, Y.W. Wu, X.S. Hu, K. Wu, and W.M. Gan, Effect of Particle Size on Microstructure and Mechanical Properties of SiCp/AZ91 Magnesium Matrix Composite, Mater. Sci. Eng. A, 2012, 543, p 158–16310.1016/j.msea.2012.02.064 ↗
4. B.L. Mordike and T. Ebert, Magnesium Properties-Applications-Potentials, Mater. Sci. Eng. A, 2001, 302, p 37–4510.1016/S0921-5093(00)01351-4 ↗
5. S.J. Huang, Y.R. Jeng, V.I. Semenov, and Y.Z. Dai, Particle Size Effects of Silicon Carbide on Wear Behavior of SiCp-Reinforced Magnesium Matrix Composites, Tribol. Lett., 2011, 42, p 79–8710.1007/s11249-011-9751-4 ↗
6. P. Abachi, A. Masoudi, and K. Purazrang, Dry Sliding Wear Behavior of SiCp/QE22 Magnesium Alloy Matrix Composites, Mater. Sci. Eng. A, 2006, 435-436, p 653–65710.1016/j.msea.2006.08.020 ↗
7. C.Y.H. Lim, S.C. Lim, and M. Gupta, Wear Behaviour of SiCp-Reinforced Magnesium Matrix Composites, Wear, 2003, 255, p 629–63710.1016/S0043-1648(03)00121-2 ↗
8. R.A. Saravanan and M.K. Surappa, Fabrication and Characterisation of Pure Magnesium-30 vol.% SiCp Particle Composite, Mater. Sci. Eng. A, 2000, 276, p 108–11610.1016/S0921-5093(99)00498-0 ↗
9. W.L.E. Wong and M. Gupta, Simultaneously Improving Strength and Ductility of Magnesium Using Nano-size SiC Particulates and Microwaves, Adv. Eng. Mater., 2006, 8, p 735–74010.1002/adem.200500209 ↗
10. M. Habibnejad-Korayem, R. Mahmudi, H.M. Ghasemi, and W.J. Poole, Tribological Behavior of Pure Mg and AZ31 Magnesium Alloy Strengthened by Al2O3 Nano-particles, Wear, 2010, 268, p 405–41210.1016/j.wear.2009.08.031 ↗
11. M. Shanthi, Q.B. Nguyen, and M. Gupta, Sliding Wear Behaviour of Calcium Containing AZ31B/Al2O3 Nanocomposites, Wear, 2010, 269, p 473–47910.1016/j.wear.2010.04.034 ↗
12. H. Ferkel and B.L. Mordike, Magnesium Strengthened by SiC Nanoparticles, Mater. Sci. Eng. A, 2001, 298, p 193–19910.1016/S0921-5093(00)01283-1 ↗
13. X.C. Li, Y. Yang, and X.D. Cheng, Ultrasonic-Assisted Fabrication of Metal Matrix Nanocomposites, J. Mater. Sci., 2004, 39, p 3211–321210.1023/B:JMSC.0000025862.23609.6f ↗
14. F.J. Humpreys and M. Hatherly, Recrystallization and Related Annealing Phenomena, Pergamon, Oxford, 2004
15. J.F. Archard, Contact and Rubbing of Flat Surfaces, J. Appl. Phys., 1953, 24, p 981–98810.1063/1.1721448 ↗
16. S.C. Sharma, B. Anand, and M. Krishna, Evaluation of Sliding Wear Behavior of Feldspar Particle-Reinforced Magnesium Alloy Composites, Wear, 2000, 241, p 33–4010.1016/S0043-1648(00)00349-5 ↗
17. B.V.M. Kumar and B. Basu, Evolution in Friction and Wear of Mg-SiCp Composites: Influence of Fretting Duration, J. Mater. Res., 2005, 20, p 801–81210.1557/JMR.2005.0113 ↗
18. L.H. Qi, J.T. Guan, J. Liu, J.M. Zhou, and X.L. Wei, Wear Behaviors of Cf/Mg Composites Fabricated by Extrusion Directly Following Vacuum Pressure Infiltration Technique, Wear, 2013, 307, p 127–13310.1016/j.wear.2013.08.024 ↗
19. H. Choi, N. Alba-Baena, S. Nimityongskul, M. Jones, T. Wood, M. Sahoo, R. Lakes, S. Kou, and X.C. Li, Characterization of Hot Extruded Mg/SiC Nanocomposites Fabricated by Casting, J. Mater. Sci., 2011, 46, p 2991–299710.1007/s10853-010-5176-y ↗
20. C.Y.H. Lim, D.K. Leo, J.J.S. Ang, and M. Gupta, Wear of Magnesium Composites Reinforced with Nano-sized Alumina Particulates, Wear, 2005, 259, p 620–62510.1016/j.wear.2005.02.006 ↗