journal article·2013-07

Microstructure and Wear Behavior of High-Cr WCI Matrix Surface Composite Reinforced with Cemented Carbide Rods

Shuzeng Hou, Chonggao Bao, Zhiyun Zhang, Yaping Bai

Publisher page

Abstract

The present article reports a new superior wear resistance surface composite prepared by a vacuum evaporative pattern casting-in process. This surface composite was constructed with reinforcing cemented carbide rod (CCR) array within high-Cr white cast iron (WCI) matrix. Three reaction zones that formed around the CCRs were characterized and established the good metallurgical bonding between CCRs and matrix. In addition, some compound carbide containing Fe, Cr, W, and Co elements were formed in the reaction zones, owing to the partial dissolution of the CCRs and the resulting interdiffusion of elements such as W, Co, C, Fe, and Cr. The wear behavior of the composite was evaluated and compared with unreinforced high-Cr WCI by means of a three-body abrasive wear tester. The results showed that the wear resistance of the composite was significantly higher than that of the unreinforced high-Cr WCI. The exciting wear resistance can be ascribed to protective effect introduced by the CCRs during wear process and the good metallurgical bonding between CCRs and matrix.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Metal and Thin Film Mechanics · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. C.K. Kim, S. Lee, and J.Y. Jung, Effects of Heat Treatment on Wear Resistance and Fracture Toughness of Duo-Cast Materials Composed of High-Chromium White Cast Iron and Low-Chromium Steel, Metall. Mater. Trans. A, 2006, 37A(3), p 633–64310.1007/s11661-006-0035-9 ↗
2. H. Oh, S. Lee, J.Y. Jung, and S. Ahn, Correlation of Microstructure with the Wear Resistance and Fracture Toughness of Duocast Materials Composed of High-Chromium White Cast Iron and Low-Chromium Steel, Metall. Mater. Trans. A, 2001, 32A(3), p 515–52410.1007/s11661-001-0068-z ↗
3. K. Kambakas and P. Tsakiropoulos, Solidification of High-Cr White Cast Iron-WC Particle Reinforced Composites, Mater. Sci. Eng. A, 2005, 413–414, p 538–54410.1016/j.msea.2005.08.215 ↗
4. I. Fernández and F.J. Belzunce, Wear and Oxidation Behaviour of High-Chromium White Cast Irons, Mater. Charact., 2008, 59(6), p 669–67410.1016/j.matchar.2007.05.021 ↗
5. Y.F. Li and Y.M. Gao, Three-Body Abrasive Wear Behavior of CC/High-Cr WCI, Composite and Its Interfacial Characteristics, Wear, 2010, 268(3–4), p 511–518
6. Z.L. Li, Y.H. Jiang, R. Zhou, D.H. Lu, and R.F. Zhou, Dry Three-Body Abrasive Wear Behavior of WC Reinforced Iron Matrix Surface Composites Produced by V-EPC Infiltration Casting Process, Wear, 2007, 262(5–6), p 649–654
7. U. Beste, S. Jacobson, and S. Hogmark, Rock Penetration into Cemented Carbide Drill Buttons During Rock Drilling, Wear, 2008, 264(11–12), p 1142–115110.1016/j.wear.2007.01.029 ↗
8. C.M. Fernandes, A.M.R. Senos, M.T. Vieira, and J.M. Antunes, Mechanical Characterization of Composites Prepared from WC Powders Coated with Ni Rich Binders, Int. J. Refract. Met. Hard Mater., 2008, 26(5), p 491–49810.1016/j.ijrmhm.2007.12.001 ↗
9. U. Beste and S. Jacobson, A New View of the Deterioration and Wear of WC/Co Cemented Carbide Rock Drill Buttons, Wear, 2008, 264(11–12), p 1129–114110.1016/j.wear.2007.01.030 ↗
10. L.B. Chen, Y.H. He, B.Y. Huang, and Y.X. Liu, Recycling Process of Tungsten Alloy Scrap, Powder Metall. Technol., 2003, 21(3), p 169–174 (in Chinese)
11. L. Luo, L. Kejun, A. Shibayama, W. Yen, T. Fujita, O. Shindod, and A. Katai, Recovery of Tungsten and Vanadium from Tungsten Alloy Scrap, Hydrometallurgy, 2004, 72(1–2), p 1–810.1016/S0304-386X(03)00121-X ↗
12. A.F. Guillermet, Thermodynamic Properties of the Co-W-C System, Metall. Trans. A, 1989, 20A(5), p 935–95610.1007/BF02651660 ↗
13. A.F. Guillermet, The Co-Fe-Ni-W-C Phase-Diagram—A Thermodynamic Description and Calculated Sections for (Co-Fe-Ni) Bonded Cemented WC Tools, Z. Metallkunde, 1989, 80(2), p 83–94
14. C.B. Pollock and H.H. Stadelma, Eta Carbides in Fe-W-C and Co-W-C Systems, Metall. Trans., 1970, 1(4), p 76710.1007/BF02811752 ↗
15. M. Bergstrom, Eta-Carbides in Quaternary System Fe-W-C-Cr at 1250 Degrees Celsius, Mater. Sci. Eng., 1977, 27(3), p 271–28610.1016/0025-5416(77)90210-5 ↗
16. M. Bergstrom, Eta-Carbides in Ternary System Fe-W-C at 1250 Degrees Celsius, Mater. Sci. Eng., 1977, 27(3), p 257–26910.1016/0025-5416(77)90209-9 ↗
17. J. Rodelas, G. Hilmas, and R.S. Mishra, Sinterbonding Cobalt-Cemented Tungsten Carbide to Tungsten Heavy Alloys, Int. J. Refract. Met. Hard Mater., 2009, 27(5), p 835–84110.1016/j.ijrmhm.2009.03.001 ↗
18. D. Lou, J. Hellman, D. Luhulima, J. Liimatainen, and V.K. Lindroos, Interactions Between Tungsten Carbide (WC) Particulates and Metal Matrix in WC-Reinforced Composites, Mater. Sci. Eng. A, 2003, 340(1–2), p 155–16210.1016/S0921-5093(02)00173-9 ↗
19. P.Q. Xu, Dissimilar Welding of WC-Co Cemented Carbide to Ni42Fe50.9C0.6Mn3.5Nb3 Invar Alloy by Laser-Tungsten Inert Gas Hybrid Welding, Mater. Des., 2011, 32(1), p 229–23710.1016/j.matdes.2010.06.006 ↗
20. P.Q. Xu, X.J. Zhao, D.X. Yang, and S. Yao, Study on Filler Metal (Ni-Fe-C) During GTAW of WC-30Co to 45’’ Carbon Steel, J. Mater. Sci., 2005, 40(24), p 6559–656410.1007/s10853-005-1547-1 ↗
21. C.M. Fernandes, A.M.R. Senos, and M.T. Vieira, Control of Eta Carbide Formation in Tungsten Carbide Powders Sputter-Coated with (Fe/Ni/Cr), Int. J. Refract. Met. Hard Mater., 2007, 25(4), p 310–31710.1016/j.ijrmhm.2006.07.004 ↗
22. R.C.D. Richardson, The Wear of Metals by Hard Abrasives, Wear, 1967, 10(4), p 291–30910.1016/0043-1648(67)90093-2 ↗
23. J. Pirso, M. Viljus, K. Juhani, and M. Kuningas, Three-Body Abrasive Wear of TiC-NiMo Cermets, Tribol. Int., 2010, 43(1–2), p 340–34610.1016/j.triboint.2009.06.014 ↗
24. J. Pirso, M. Viljus, S. Letunovitš, K. Juhani, and R. Joost, Wear, 2011, 271(11–12), p 2868–287810.1016/j.wear.2011.06.005 ↗
25. P.H. Shipway and J.J. Hogg, Dependence of Microscale Abrasion Mechanisms of WC-Co, Hardmetals on Abrasive Type, Wear, 2005, 259(1–6), p 44–5110.1016/j.wear.2004.12.021 ↗
26. M.G. Gee, A. Gant, and B. Roebuck, Wear Mechanisms in Abrasion and Erosion of WC/Co and Related Hardmetals, Wear, 2007, 263(SI), p 137–148
27. J. Pirso, S. Letunovitš, and M. Viljusb, Friction and Wear Behaviour of Cemented Carbides, Wear, 2004, 257(3–4), p 257–26510.1016/j.wear.2003.12.014 ↗
28. J. Larsen-Basse and E.T. Koyanagl, Abrasion of WC-Co Alloys by Quarts, J. Lubr. Technol., 1979, 101(2), p 208–21110.1115/1.3453325 ↗
29. S.V. Prasad and T.H. Kosel, Wear, A Study of Carbide Removal Mechanisms during Quartz Abrasion I: In Situ Scratch Test Studies, Wear, 1983, 92(2), p 253–26810.1016/0043-1648(83)90199-0 ↗