Effect of Grain Size Distribution on Processing Maps for Isothermal Compression of Inconel 718 Superalloy
Source abstract
Abstract
Cylindrical specimens of Inconel 718 alloys with three types of grain size distribution were used in the compression tests and processing maps were developed in 940-1040 °C and 0.001-10 s−1. The equiaxed fine grain is more effective on the dynamic softening behavior. For partial recrystallized microstructure, the peak efficiency of power dissipation occurs at the strain rate of 0.001 s−1, and the temperature range of 1000-1020 °C. In order to obtain homogeneous microstructure with fine grains, the partial recrystallized microstructure should be deformed at the low temperature and slow strain rates. The area fraction of instability domains decreases with strain increasing. The peak efficiency of power dissipation increases with average grain size decreasing. The efficiency of power dissipation will be stimulated by the precipitation of δ phase at slow strain rate of 0.001-0.01 s−1, and the initial deformed substructure at the strain rate of 0.1-1 s−1. Equiaxed fine grain is the optimum state for forging process and dynamic recrystallization. The grain size distribution has slight influence on the microstructure evolution at high temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallurgy and Material Forming · High Temperature Alloys and Creep · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Y.V.R.K. Prasad et al., Modeling of Dynamic Material Behavior in Hot Deformation: Forging of Ti-6242, Metall. Trans. A, 1984, 15(10), p 1883–189210.1007/BF02664902 ↗
2. Y. Zhu et al., Characterization of Hot Deformation Behavior of As-Cast TC21 Titanium Alloy Using Processing Map, Mater. Sci. Eng. A, 2011, 528(3), p 1757–176310.1016/j.msea.2010.11.015 ↗
3. I. Sen, R.S. Kottada, and U. Ramamurty, High Temperature Deformation Processing Maps for Boron Modified Ti-6Al-4V Alloys, Mater. Sci. Eng. A, 2010, 527(23), p 6157–616510.1016/j.msea.2010.06.044 ↗
4. Q.L. Pan et al., Characterization of Hot Deformation Behavior of Ni-Base Superalloy Rene’41 Using Processing Map, Mater. Sci. Eng. A, 2013, 585, p 371–37810.1016/j.msea.2013.07.066 ↗
5. Y. Liu et al., Effect of True Strains on Processing Map for Isothermal Compression of Ni-20.0Cr-2.5Ti-1.5Nb-1.0Al Ni-Base Superalloy, J. Alloy. Compd., 2014, 612, p 56–6310.1016/j.jallcom.2014.05.165 ↗
6. Y. Kong et al., Hot Deformation Characteristics and Processing Map of Nickel-Based C276 Superalloy, J. Alloy. Compd., 2015, 622, p 738–74410.1016/j.jallcom.2014.10.118 ↗
7. A. Momeni and K. Dehghani, Hot Working Behavior of 2205 Austenite–Ferrite Duplex Stainless Steel Characterized by Constitutive Equations and Processing Maps, Mater. Sci. Eng. A, 2011, 528(3), p 1448–145410.1016/j.msea.2010.11.020 ↗
8. S.V.S.N. Murty, S. Torizuka, and K. Nagai, Microstructural Evolution During Simple Heavy Warm Compression of a Low Carbon Steel: Development of a Processing Map, Mater. Sci. Eng. A, 2005, 410-411, p 319–32310.1016/j.msea.2005.08.173 ↗
9. T. Zhong et al., Processing Maps, Microstructure Evolution and Deformation Mechanisms of Extruded AZ31-DMD During Hot Uniaxial Compression, Mater. Sci. Eng. A, 2013, 559, p 773–78110.1016/j.msea.2012.09.023 ↗
10. X. Shang et al., Optimizing and Identifying the Process Parameters of AZ31 Magnesium Alloy in Hot Compression on the Base of Processing Maps, J. Alloy. Compd., 2015, 629, p 155–16110.1016/j.jallcom.2014.12.251 ↗
11. M. Zhang et al., Characterization of Hot Deformation Behavior of a P/M Nickel-Base Superalloy Using Processing Map and Activation Energy, Mater. Sci. Eng. A, 2010, 527(24-25), p 6771–677910.1016/j.msea.2010.07.039 ↗
12. M.C. Somani et al., Mechanical Processing and Microstructural Control in Hot Working of Hot Isostatically Pressed P/M IN-100 Superalloy, Mater. Sci. Eng. A, 1998, 245(1), p 88–9910.1016/S0921-5093(97)00698-9 ↗
13. P.K. Sagar, Effect of Alloying Elements and Microstructure on the Processing Parameters of α2 Aluminide Alloys, Mater. Sci. Eng. A, 2006, 434(1-2), p 259–26810.1016/j.msea.2006.06.134 ↗
14. C.Y. Wang et al., Processing Maps For Hot Working of ZK60 Magnesium Alloy, Mater. Sci. Eng. A, 2007, 464(1-2), p 52–5810.1016/j.msea.2007.03.003 ↗
15. Y. Wang et al., Characterization of Dynamic Recrystallisation in As-Homogenized Mg-Zn-Y-Zr Alloy Using Processing Map, J. Mater. Sci., 2006, 41(12), p 3603–360810.1007/s10853-005-5564-x ↗
16. Y. Wang et al., Hot Working Characteristics and Dynamic Recrystallization of Delta-Processed Superalloy 718, J. Alloy. Compd., 2009, 474(1-2), p 341–34610.1016/j.jallcom.2008.06.079 ↗
17. W.S. Lee et al., Effects of Temperature and Strain Rate on Deformation Behaviour of Inconel 718 Alloy, Mater. Chem. Phys., 2011, 129(3), p 832–83910.1016/j.matchemphys.2011.05.019 ↗
18. A. Rao, M. Srinivas, and D.S. Sarma, Effect of Thermomechanical Working on the Microstructure and Mechanical Properties of Hot Isostatically Pressed Superalloy Inconel 718, Mater. Sci. Eng. A, 2004, 383(2), p 201–21210.1016/j.msea.2004.05.062 ↗
19. N. Srinivasan and Y.V.R.K. Prasad, Microstructural Control in Hot Working of IN-718 Superalloy Using Processing Map, Metall. Mater. Trans. A, 1994, 25(10), p 2275–228410.1007/BF02652327 ↗
20. S.V.S.N. Murty and B.N. Rao, On the Flow Localization Concepts in the Processing Maps of IN718, Mater. Sci. Eng. A, 1999, 267(1), p 159–16110.1016/S0921-5093(99)00122-7 ↗
21. S.V.S.N. Murty and B.N. Rao, On the Development of Instability Criteria During Hotworking with Reference to IN 718, Mater. Sci. Eng. A, 1998, 254, p 76–8210.1016/S0921-5093(98)00764-3 ↗
22. F. Sui et al., Processing Map for Hot Working of Inconel 718 Alloy, J. Mater. Process. Technol., 2011, 211(3), p 433–44010.1016/j.jmatprotec.2010.10.015 ↗
23. K. Wang et al., Effect of the δ Phase on the Deformation Behavior in Isothermal Compression of Superalloy GH4169, Mater. Sci. Eng. A, 2011, 528(13-14), p 4723–473110.1016/j.msea.2011.02.081 ↗
24. D. Wen et al., Hot Deformation Behavior and Processing Map of a Typical Ni-Based Superalloy, Mater. Sci. Eng. A, 2014, 591, p 183–19210.1016/j.msea.2013.09.049 ↗
25. D. Cai et al., Dissolution Kinetics of δ Phase and its Influence on the Notch Sensitivity of Inconel 718, Mater. Charact., 2007, 58(3), p 220–22510.1016/j.matchar.2006.04.020 ↗
26. P. Zhang et al., Plastic Deformation Behavior and Processing Maps of a Ni-Based Superalloy, Mater. Des., 2015, 65, p 575–58410.1016/j.matdes.2014.09.062 ↗
27. Q. Guo et al., Nucleation Mechanisms of Dynamic Recrystallization in Inconel 625 Superalloy Deformed with Different Strain Rates, Rare Met., 2012, 31(3), p 215–22010.1007/s12598-012-0494-7 ↗
28. D. Samantaray, S. Mandal, and A.K. Bhaduri, Characterization of Deformation Instability in Modified 9Cr-1Mo Steel During Thermo-Mechanical Processing, Mater. Des., 2011, 32(2), p 716–72210.1016/j.matdes.2010.07.038 ↗
29. D. Ohadi, M.H. Parsa, and H. Mirzadeh, Development of Dynamic Recrystallization Maps Based on the Initial Grain Size, Mater. Sci. Eng. A, 2013, 565, p 90–9510.1016/j.msea.2012.12.030 ↗
30. H. Mirzadeh, M.H. Parsa, and D. Ohadi, Hot deformation Behavior of Austenitic Stainless Steel for a Wide Range of Initial Grain Size, Mater. Sci. Eng. A, 2013, 569, p 54–6010.1016/j.msea.2013.01.050 ↗
31. M. Elwahabi et al., Effect of Initial Grain Size on Dynamic Recrystallization in High Purity Austenitic Stainless Steels, Acta Mater., 2005, 53(17), p 4605–461210.1016/j.actamat.2005.06.020 ↗
32. R.P. Guest and S. Tin, The Dynamic and Metadynamic Recrystallisation of the in 718, in Superalloys 718, 625, 706 and Derivatives 2005, TMS, Warrendale, 2005, p 625–706
33. B. Marty et al., Recrystallization and Work-Hardening Prediction During Forging Process of Inconel 718, Superalloys, 1997, 718, p 625–706
34. K. Wang, M.Q. Li, and C. Li, δ and Austenite Phases Evolution and Model in Solution Treatment of Superalloy GH4169, Mater. Sci. Technol., 2013, 29(3), p 346–35010.1179/1743284712Y.0000000144 ↗