journal article·2017-10

Pretreatment Influence on Titanium Surface Properties After Gas Nitriding

I. M. Pohrelyuk, S. M. Lavrys, O. M. Sakharuk, I. V. Stasyshyn, O. V. Penkovyi

Publisher page

Abstract

Influence of an initial mechanical treatment (grinding, polishing) on geometry and physical–mechanical parameters of a commercially pure titanium (Grade 2) surface after thermodiffusive saturation by nitrogen was studied. Microstructure analysis has shown that mechanism of formation and growth of a nitride film depends on the initial mechanical treatment. Nitriding under temperature of 750 °C does not influence practically the quality of ground surfaces and decreases it on one class for polished one. For higher saturation temperatures, surface quality has little dependence from the initial treatment. The best set of geometry and physical–mechanical characteristics belongs to the surface, which was initially polished and nitrided subsequently under 750 °C temperature, which provides its high wear resistance.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Titanium Alloys Microstructure and Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. P.K. Ajikumar, M. Kamruddin, P. Shankar, R. Gouda, A.K. Balamurugan, R. Nithya, A.K. Tyagi, V. Jayaram, S.K. Biswas, and B. Raj, Internal Nitride Formation During Gas-Phase Thermal nitridation of Titanium, Scr. Mater., 2009, 61, p 403–40610.1016/j.scriptamat.2009.04.029 ↗
2. V.L. Sordi, M. Ferrante, M. Kawasaki, and T.G. Langdon, Microstructure and Tensile Strength of Grade 2 Titanium Processed by Equal-Channel Angular Pressing and by Rolling, J. Mater. Sci., 2012, 47, p 7870–787610.1007/s10853-012-6593-x ↗
3. H.J. Rack and J.I. Qazi, Titanium Alloys for Biomedical Applications, Mater. Sci. Eng. C., 2006, 26, p 1269–127710.1016/j.msec.2005.08.032 ↗
4. Z.B. Wang, H.X. Hu, Y.G. Zheng, W. Ke, and Y.X. Qiao, Comparison of the Corrosion Behavior of Pure Titanium and Its Alloys in Fluoride-Containing Sulfuric Acid, Corros. Sci., 2016, 103, p 50–6510.1016/j.corsci.2015.11.003 ↗
5. K.G. Budinski, Tribological Properties of Titanium Alloys, Wear, 1991, 151, p 203–21710.1016/0043-1648(91)90249-T ↗
6. W. Sha, H. Ali, and X. Wu, Gas Nitriding of Titanium Alloy Ti Metal 205, Surf. Coat. Technol., 2008, 202, p 5832–583710.1016/j.surfcoat.2008.06.155 ↗
7. M. Long and H.J. Rack, Friction and Surface Behavior of Selected Titanium Alloys During Reciprocating-Sliding Motion, Wear, 2001, 249, p 157–16710.1016/S0043-1648(01)00517-8 ↗
8. L. Lu, G. Feng, M. Ren, H. Zhang, and S. Lyu, Effect of Al Content on Structure and Properties Ti1-xAlxN Hard Film Prepared by Multi-arc Ion Plating, Int. J. Precis. Eng. Manuf., 2013, 141, p 161–16410.1007/s12541-013-0022-1 ↗
9. M. Yoshi, R. Ichiki, and N. Utsumi, Surface Hardening of Titanium Using Gas Nitriding, Int. J. Precis. Eng. Manuf., 2013, 14, p 971–97610.1007/s12541-013-0128-5 ↗
10. D.A. Zhecheva, S. Malinov, and W. Shac, Surf. Coat. Technol., 2006, 201, p 2467–247410.1016/j.surfcoat.2006.04.019 ↗
11. P.K. Ajikumar, M. Kamruddin, R. Nithya, P. Shankar, S. Dash, A.K. Tyagi, and R. Baldev, Surface Nitridation of Ti and Cr in Ammonia Atmosphere, Scr. Mater., 2004, 51, p 361–36610.1016/j.scriptamat.2004.05.024 ↗
12. D. She, W. Yue, Z. Fu, C. Wang, X. Yang, and J. Liu, Effects of Nitriding Temperature on Microstructures and Vacuum Tribological Properties of Plasma-Nitrided Titanium, Surf. Coat. Technol., 2015, 264, p 32–4010.1016/j.surfcoat.2015.01.029 ↗
13. H.J. Spies, Surface Engineering of Aluminium and Titanium Alloys: An Overview, Surf. Eng., 2010, 26, p 126–13410.1179/174329409X451146 ↗
14. W.H. Kao, Y.L. Su, J.H. Horng, H.C. Huang, and S.E. Yang, Improved Tribological, Electrochemical and Biocompatibility Properties of Ti6Al4V Alloy by Gas-Nitriding and Ti-C: H Coating, Surf. Coat. Technol., 2015, 283, p 70–7910.1016/j.surfcoat.2015.10.035 ↗
15. A. Zhecheva, S. Malinov, and W. Sha, Surface Gas Nitriding of Ti-6Al-4V and Ti-6Al-2Sn-4Zr-2Mo-0.08Si Alloys, Z. Metallkd., 2003, 94, p 19–2410.3139/146.030019 ↗
16. A.M. Gatey, S.S. Hosmani, C.A. Figueroa, S.B. Arya, and R.P. Singh, Role of Surface Mechanical Attrition Treatment and Chemical Etching on Plasma Nitriding Behavior of AISI, 304L Steel, Surf. Coat. Technol., 2016, 304, p 413–42410.1016/j.surfcoat.2016.07.020 ↗
17. S.S. Akhtar, A.F.M. Arif, B.S. Yilbas, and A.K. Sheikh, Influence of Surface Preparation on the Kinetics of Controlled Gas-Nitrided AISI, H13 Steels Used in Extrusion Dies, J. Mater. Eng. Perform., 2010, 10, p 347–35510.1007/s11665-009-9496-5 ↗
18. A. Zhecheva, W. Sha, S. Malinov, and A. Long, Enhancing the Microstructure and Properties of Titanium Alloys Through Nitriding and Other Surface Engineering Methods, Surf. Coat. Technol., 2005, 200, p 2192–220710.1016/j.surfcoat.2004.07.115 ↗
19. A. daS Rocha, T. Strohaecker, and T. Hirsch, Effect of Different Surface States Before Plasma Nitriding on Properties and Machining Behavior of M2 High-Speed Steel, Surf. Coat. Technol., 2003, 165, p 176–18510.1016/S0257-8972(02)00768-5 ↗
20. G.P. Singh, J. Alphonsa, P.K. Barhai, P.A. Rayjada, P.M. Raole, and S. Mukherjee, Effect of Surface Roughness on the Properties of the Layer Formed on AISI, 304 Stainless Steel After Plasma Nitriding, Surf. Coat. Technol., 2006, 200, p 5807–581110.1016/j.surfcoat.2005.08.149 ↗
21. S.R. Bradbury, D.B. Lewis, and M. Sarwar, The Effect of Product Quality on the Integrity of Advanced Surface Engineering Treatments Applied to High Speed Steel Circular Saw Blades, Surf. Coat. Technol., 1996, 85, p 215–22010.1016/0257-8972(95)02756-4 ↗
22. G. Abrasonis, J.P. Riviere, C. Templier, S. Muzard, and L. Pranevicius, Influence of Surface Preparation and Ion Flux on the Nitriding Efficiency of Austenitic Stainless Steel, Surf. Coat. Technol., 2005, 196, p 279–28310.1016/j.surfcoat.2004.08.109 ↗
23. E. Arslan, Y. Totik, E. Demirci, and A. Alsaran, Influence of Surface Roughness on Corrosion and Tribological Behavior of CP-Ti After Thermal Oxidation Treatment, J. Mater. Eng. Perform., 2010, 19, p 428–43310.1007/s11665-009-9504-9 ↗
24. S.S. Akhtar, A.F.M. Arif, B.S. Yilbas, and A.K. Sheikh, Influence of Surface Preparation on the Kinetics of Controlled Gas-Nitrided AISI, H13 Steels Used in Extrusion Dies, J. Mater. Eng. Perform., 2010, 19, p 347–35510.1007/s11665-009-9496-5 ↗
25. J.S. Kim, E.S. Lim, and Y.G. Jung, Determination of Efficient Super Finishing Conditions for Mirror Surface Finishing of Titanium, J. Cent. South Univ. Technol., 2012, 19, p 155–16210.1007/s11771-012-0985-6 ↗
26. Ya.S. Matychak, I.M. Pohrelyuk, and V.M. Fedirko, Thermodiffusion Saturation of α-Titanium with Nitrogen from a Rarefied Atmosphere, Mater. Sci., 2009, 45, p 66–7510.1007/s11003-009-9156-9 ↗
27. R. Onodera and Y. Ishii, Two-Wavelength Phase-Shifting Interferometry Insensitive to the Intensity Modulation of Dual Laser Diodes, Appl. Opt., 1994, 33, p 5052–506110.1364/AO.33.005052 ↗
28. L.I. Muravsky, O.P. Ostash, A.B. Kmet, T.I. Voronyak, and I.M. Andreiko, Two-Frame Phase Shifting Interferometry for Retrieval of Smooth Surface and Its Displacements, Opt. Lasers Eng., 2011, 49, p 305–31210.1016/j.optlaseng.2010.11.021 ↗
29. I.M. Pohrelyuk, Ways of Intensification of Thermodiffusive Saturation of Titanium Alloys in Molecular Nitrogen, Mater. Sci., 1999, 35, p 66–7510.1007/BF02355603 ↗
30. X. Xhang, C. Krewet, and B. Kuhlenko, Automatic Classification of Defects on th Product Surface in Grinding and Polishing, Tools Manuf., 2006, 46, p 59–6910.1016/j.ijmachtools.2005.03.013 ↗
31. S.H. Chen, S.C. Ho, C.H. Chang, C.C. Chen, and W.C. Say, Influence of Roughness on Invivo Properties of Titanium Implant Surface and Their Electrochemical Behavior, Surf. Coat. Technol., 2016, 302, p 215–22610.1016/j.surfcoat.2016.06.007 ↗
32. H.I. Dawood, K.S. Mohammed, A. Rahmat, and M.B. Uday, The Influence of the Surface Roughness on the Microstructures and Mechanical Properties of 6061 Aluminium Alloy Using Friction Stir Welding, Surf. Coat. Technol., 2015, 270, p 272–28310.1016/j.surfcoat.2015.02.045 ↗
33. W. Grzesik and S. Brol, Hybrid Approach to Surface Roughness Evaluation in Multistage Machining Processes, J. Mater. Process. Technol., 2003, 134, p 265–27210.1016/S0924-0136(02)01105-6 ↗
34. W. Grzesik and T. Wanat, Comparative Assessment of Surface Roughness Produced b Hard Machining with Mixed Ceramic Tools Including 2D and 3D Analysis, J. Mater. Process. Technol., 2005, 169, p 364–37110.1016/j.jmatprotec.2005.04.080 ↗