Joining Alumina to Inconel 600 and UMCo-50 Superalloys Using an Sn10Ag4Ti Active Filler Metal

Sui‐Yuan Chang, Yu-Ting Hung, T. H. Chuang

Publisher page

Abstract

Alumina ceramics were brazed to Inconel 600 and UMCo-50 superalloys at 900 °C for 10 min using an Sn10Ag4Ti active filler metal. The brazing filler showed good wettability on alumina and superalloys. The flexural strengths were 69 and 57 MPa for alumina/Inconel 600 and alumina/UMCo-50 joints, respectively. In both cases, the brazed specimens fractured along the Sn10Ag4Ti/superalloy interfaces after four-point bending tests. Electron probe microanalysis (EPMA) elemental mapping revealed that the Ni of Inconel 600 and the Co of UMCo-50 dissolved into Sn10Ag4Ti filler metal, which serves to reinforce the weak Sn10Ag4Ti matrix.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · High-Temperature Coating Behaviors · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.