Abstract
Additive Friction Stir Deposition (AFSD) is an emerging solid-state advanced manufacturing process with significant promise for aluminum alloys due to its ability to avoid solidification defects and enable sustainable fabrication, repair, and recycling. Despite rapid progress over the past decade, a comprehensive understanding of how AFSD process parameters govern the microstructure and properties remains fragmented, particularly in relation to precipitation behavior and mechanical performance. This review highlights a decade of research progress in AFSD of aluminum alloys since its invention in 2014, bridging experimental findings with modeling efforts and highlighting process–microstructure–property relationships. It also systematically reviews how variations in process parameters influence the material’s microstructure and hence determine the final properties. By critically evaluating progress and challenges, this review provides a roadmap for researchers and industry practitioners to guide future innovations, ensuring AFSD’s broader adoption across diverse applications.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties · Additive Manufacturing Materials and Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. J. Shao et al., Additive Friction Stir Deposition of Metallic Materials: Process, Structure and Properties, Mater. Des., 2023, 234, 112356. https://doi.org/10.1016/j.matdes.2023.11235610.1016/j.matdes.2023.112356 ↗
2. H.Z. Yu and R.S. Mishra, Additive Friction Stir Deposition: A Deformation Processing Route to Metal Additive Manufacturing, Mater. Res. Lett., 2021, 9(2), p 71–83. https://doi.org/10.1080/21663831.2020.184721110.1080/21663831.2020.1847211 ↗
3. Y.G.Y. Elshaghoul et al., Additive Friction Stir Deposition of AA7075-T6 Alloy: Impact of Process Parameters on the Microstructures and Properties of the Continuously Deposited Multilayered Parts, Appl. Sci., 2023, 13(18), 10255. https://doi.org/10.3390/app13181025510.3390/app131810255 ↗
4. R.J. Griffiths et al., Solid-State Additive Manufacturing of Aluminum and Copper using Additive Friction Stir Deposition: Process-Microstructure Linkages, Materialia, 2021, 15, 100967. https://doi.org/10.1016/j.mtla.2020.10096710.1016/j.mtla.2020.100967 ↗
5. C.J.T. Mason et al., Process-Structure-Property Relations for as-Deposited Solid-State Additively manufactured High-Strength Aluminum Alloy, Addit. Manuf., 2021, 40, 101879. https://doi.org/10.1016/j.addma.2021.10187910.1016/j.addma.2021.101879 ↗
6. J.B. Jordon et al., Direct Recycling of Machine Chips through a Novel Solid-State Additive Manufacturing Process, Mater. Des., 2020, 193, 108850. https://doi.org/10.1016/j.matdes.2020.10885010.1016/j.matdes.2020.108850 ↗
7. N.I. Palya et al., Multi-Physics Approach to Predict Fatigue Behavior of High Strength Aluminum Alloy Repaired via Additive Friction Stir Deposition, Integr. Mater. Manuf. Innov., 2023, 12(4), p 441–455. https://doi.org/10.1007/s40192-023-00309-310.1007/s40192-023-00309-3 ↗
8. Y. Jin, T. Yang, T. Wang, S. Dowden, A. Neogi, and N.B. Dahotre, Behavioral Simulations and Experimental Evaluations of Stress Induced Spatial Nonuniformity of Dynamic Bulk Modulus in Additive Friction Stir Deposited AA 6061, J. Manuf. Process., 2023, 94, p 454–465. https://doi.org/10.1016/j.jmapro.2023.03.08010.1016/j.jmapro.2023.03.080 ↗
9. X. Dong et al., Recent Advances in Additive Friction Stir Deposition: A Critical Review, Materials, 2024, 17(21), p 5205. https://doi.org/10.3390/ma1721520510.3390/ma17215205 ↗
10. I. Liu, T.C. Bor, P.G. Allison, and J.B. Jordon, Additive Friction Stir Deposition of Aluminum Alloys: A Critical Review, Mater. Des., 2025, 258, 114543. https://doi.org/10.1016/j.matdes.2025.11454310.1016/j.matdes.2025.114543 ↗
11. S.C. Beck et al., Examination of Microstructure and Mechanical Properties of Direct Additive Recycling for Al-Mg-Mn Alloy Machine Chip Waste, Mater. Des., 2023, 228, 111733. https://doi.org/10.1016/j.matdes.2023.11173310.1016/j.matdes.2023.111733 ↗
12. S. Babaniaris et al., Precipitation in AA6063 Produced from Swarf Using Additive Friction Stir Deposition, Addit. Manuf. Lett., 2022, 3, 100096. https://doi.org/10.1016/j.addlet.2022.10009610.1016/j.addlet.2022.100096 ↗
13. X. Li, X. Li, S. Hu, Y. Liu, and D. Ma, Additive Friction Stir Deposition: A Review on Processes, Parameters, Characteristics, and Applications, Int. J. Adv. Manuf. Technol., 2024, 133(3–4), p 1111–1128. https://doi.org/10.1007/s00170-024-13890-410.1007/s00170-024-13890-4 ↗
14. B.J. Phillips, C.J. Williamson, R.P. Kinser, J.B. Jordon, K.J. Doherty, and P.G. Allison, Microstructural and Mechanical Characterization of Additive Friction Stir-Deposition of Aluminum Alloy 5083 Effect of Lubrication on Material Anisotropy, Materials, 2021, 14(21), 6732. https://doi.org/10.3390/ma1421673210.3390/ma14216732 ↗
15. I. Liu et al., Influence of Aging Time to Achieve Tensile Build Direction Heat Treated T74 Forging Properties in Lubricant Free AFSD AA7050, Addit. Manuf. Lett., 2025, 14, 100296. https://doi.org/10.1016/j.addlet.2025.10029610.1016/j.addlet.2025.100296 ↗
16. N. Zhu et al., Neutron Diffraction Analysis of Residual Stress Distribution in the Lubricant-Free TR-AFSD AA7075 Repair Coupled with SPH Simulations, J. Adv. Join. Process., 2025, 11, 100283. https://doi.org/10.1016/j.jajp.2025.10028310.1016/j.jajp.2025.100283 ↗
17. F. Khodabakhshi and A.P. Gerlich, Potentials and Strategies of Solid-State Additive Friction-Stir Manufacturing Technology: A Critical Review, J. Manuf. Process., 2018, 36, p 77–92. https://doi.org/10.1016/j.jmapro.2018.09.03010.1016/j.jmapro.2018.09.030 ↗
18. M.B. Williams et al., Elucidating the Effect of Additive Friction Stir Deposition on the Resulting Microstructure and Mechanical Properties of Magnesium Alloy WE43, Metals, 2021, 11(11), 1739. https://doi.org/10.3390/met1111173910.3390/met11111739 ↗
19. N.I. Palya et al., Microstructure Prediction from Smooth Particle Hydrodynamics Process Simulations of Additive Friction Stir Deposition, Metall. Mater. Trans. A, 2024, 55(9), p 3601–3616. https://doi.org/10.1007/s11661-024-07499-110.1007/s11661-024-07499-1 ↗
20. Q. Qiao et al., In Situ Monitoring of Temperature, Force and Torque in Additive Friction Stir Deposition of AA6061: Effect of Rotational Driving Mode, Mater Charact, 2025, 227, 115326. https://doi.org/10.1016/j.matchar.2025.11532610.1016/j.matchar.2025.115326 ↗
21. H. Wang et al., Repairing the 7075 Al Alloy Plate by Additive Friction Stir Deposition with Different Feedstock Rods, Int. J. Adv. Manuf. Technol., 2024, 134(1–2), p 921–933. https://doi.org/10.1007/s00170-024-14186-310.1007/s00170-024-14186-3 ↗
22. C. Zeng et al., Microstructure Evolution of Al6061 Alloy Made by Additive Friction Stir Deposition, Materials, 2022, 15(10), 3676. https://doi.org/10.3390/ma1510367610.3390/ma15103676 ↗
23. J.-O. Andersson, T. Helander, L. Höglund, P. Shi, and B. Sundman, Thermo-Calc & DICTRA, Computational Tools for Materials Science, Calphad, 2002, 26(2), p 273–312. https://doi.org/10.1016/S0364-5916(02)00037-810.1016/S0364-5916(02)00037-8 ↗
24. J.K. Yoder, G.D. Hahn, N. Zhao, R.E. Brennan, K. Cho, and H.Z. Yu, Additive Friction Stir Deposition-Enabled Upcycling of Automotive cast Aluminum Chips, Addit. Manuf. Lett., 2023, 4, 100108. https://doi.org/10.1016/j.addlet.2022.10010810.1016/j.addlet.2022.100108 ↗
25. D.Z. Avery et al., Evaluation of Microstructure and Mechanical Properties of Al-Zn-Mg-Cu Alloy Repaired via Additive Friction Stir Deposition, J. Eng. Mater. Technol., 2022, 144(3), 031003. https://doi.org/10.1115/1.405281610.1115/1.4052816 ↗
26. L.P. Cahalan et al., Parametric Investigation of Parallel Deposition Passes on the Microstructure and Mechanical Properties of 7075 Aluminum Alloy Processed with Additive Friction Stir Deposition, Appl. Sci., 2024, 14(1), 457. https://doi.org/10.3390/app1401045710.3390/app14010457 ↗
27. W.D. Hartley et al., Solid-State Cladding on Thin Automotive Sheet Metals Enabled by Additive Friction Stir Deposition, J. Mater. Process. Technol., 2021, 291, 117045. https://doi.org/10.1016/j.jmatprotec.2021.11704510.1016/j.jmatprotec.2021.117045 ↗
28. N. Fernando, R. Sarvesha, J. Caudill, and I.S. Jawahir, Effect of Tool Face Geometry on Additive Friction Stir Deposition of Al-Mg-Si alloy: Process Modeling and Validation in Correlation with Mechanical Properties, J. Mater. Process. Technol., 2025, 344, 119007. https://doi.org/10.1016/j.jmatprotec.2025.11900710.1016/j.jmatprotec.2025.119007 ↗
29. G.G. Stubblefield, K. Fraser, B.J. Phillips, J.B. Jordon, and P.G. Allison, A meshfree Computational Framework for the Numerical Simulation of the Solid-State Additive Manufacturing Process, Additive Friction Stir-Deposition (AFS-D), Mater. Des., 2021, 202, 109514. https://doi.org/10.1016/j.matdes.2021.10951410.1016/j.matdes.2021.109514 ↗
30. G.R. Merritt, M.B. Williams, P.G. Allison, J.B. Jordon, T.W. Rushing, and C.A. Cousin, Closed-Loop Temperature and Force Control of Additive Friction Stir Deposition, J. Manuf. Mater. Process., 2022, 6(5), 92. https://doi.org/10.3390/jmmp605009210.3390/jmmp6050092 ↗
31. E. Yasa, O. Poyraz, K. Do, A. Molyneux, J. McManus, and J. Hughes, In-Situ Monitoring and Control of Additive Friction Stir Deposition, Materials, 2025, 18(7), 1509. https://doi.org/10.3390/ma1807150910.3390/ma18071509 ↗
32. L.P. Martin, A. Luccitti, and M. Walluk, Evaluation of Additive Friction Stir Deposition for the Repair of Cast Al-1.4Si-1.1Cu-1.5Mg-2.1Zn, J. Manuf. Sci. Eng., 2022, 144(6), 061006. https://doi.org/10.1115/1.405275910.1115/1.4052759 ↗
33. R.J. Griffiths, D.T. Petersen, D. Garcia, and H.Z. Yu, Additive Friction Stir-Enabled Solid-State Additive Manufacturing for the Repair of 7075 Aluminum Alloy, Appl. Sci., 2019, 9(17), 3486. https://doi.org/10.3390/app917348610.3390/app9173486 ↗
34. M.E.J. Perry, R.J. Griffiths, D. Garcia, J.M. Sietins, Y. Zhu, and H.Z. Yu, Morphological and microstructural investigation of the non-planar interface formed in solid-state metal additive manufacturing by additive friction stir deposition, Additive Manuf., 2020, 35, 101293. https://doi.org/10.1016/j.addma.2020.10129310.1016/j.addma.2020.101293 ↗
35. U. Suhuddin, S. Mironov, H. Krohn, M. Beyer, and J.F. Dos Santos, Microstructural Evolution during Friction Surfacing of Dissimilar Aluminum Alloys, Metall. Mater. Trans. A, 2012, 43(13), p 5224–5231. https://doi.org/10.1007/s11661-012-1345-810.1007/s11661-012-1345-8 ↗
36. A. Raj et al., Prediction of Temperature Distribution Using Coupled Eulerian-Lagrangian (CEL) Finite Element Modelling of Plunging Stage During Additive Friction Stir Deposition, Advanced Manufacturing, (Portland, Oregon, USA: American Society of Mechanical Engineers, 2024), p V002T03A052. https://doi.org/10.1115/IMECE2024-144626.10.1115/IMECE2024-144626 ↗
37. R. Mathews, J. Karandikar, C. Tyler, S. Smith, and T. Schmitz, “Coupled Eulerian-Lagrangian Thermomechanical Model to Predict Residual Stress During Additive Friction Stir Deposition of Aluminum 6061,”Additive Manufacturing; Advanced Materials Manufacturing; Biomanufacturing; Life Cycle Engineering, (Knoxville, Tennessee, USA: American Society of Mechanical Engineers, 2024) p V001T01A058. https://doi.org/10.1115/MSEC2024-131311.10.1115/MSEC2024-131311 ↗
38. C.S. Alam, V. Karami, S. Guo, and M.S. Rahman, Thermo-Mechanical Response of Aluminum Alloy in the Additive Friction-Stir Deposition Process, Additive Manuf. Lett., 2025, 12, 100263. https://doi.org/10.1016/j.addlet.2024.10026310.1016/j.addlet.2024.100263 ↗
39. K.C. Kincaid, D.W. MacPhee, G.G. Stubblefield, J.B. Jordon, T.W. Rushing, and P.G. Allison, A Finite Volume Framework for the Simulation of Additive Friction Stir Deposition, J. Eng. Mater. Technol., 2023, 145(3), 031002. https://doi.org/10.1115/1.405664210.1115/1.4056642 ↗
40. H. Jasak, OpenFOAM: Open Source CFD in Research and Industry, Int. J. Nav. Archit. Ocean Eng., 2009, 1(2), p 89–94. https://doi.org/10.2478/IJNAOE-2013-001110.2478/IJNAOE-2013-0011 ↗
41. U.F. Kocks, and H. Mecking. Physics and phenomenology of strain hardening: the FCC case, Prog. Mater. Sci., 2003, 48(3), p 171–27310.1016/S0079-6425(02)00003-8 ↗
42. T. Takaki, Y. Hisakuni, T. Hirouchi, A. Yamanaka, and Y. Tomita, Multi-Phase-Field Simulations for Dynamic Recrystallization, Comput. Mater. Sci., 2009, 45(4), p 881–888. https://doi.org/10.1016/j.commatsci.2008.12.00910.1016/j.commatsci.2008.12.009 ↗
43. C. Zener and J.H. Hollomon, Effect of Strain Rate Upon Plastic Flow of Steel, J. Appl. Phys., 1944, 15(1), p 22–32. https://doi.org/10.1063/1.170736310.1063/1.1707363 ↗
44. F. Hu, G. Chen, Y. Lin, H. Wang, and Z. Zhu, Numerical and Experimental Study on the Thermal Process during Additive Friction Stir Deposition, CIRP J. Manuf. Sci. Technol., 2024, 48, p 55–66. https://doi.org/10.1016/j.cirpj.2023.12.00210.1016/j.cirpj.2023.12.002 ↗
45. B. Feng et al., Multi-Stage Precipitation Modeling for AA 7050 Hole Repairs in Additive Friction Stir Deposition, J. Appl. Phys., 2024, 136(16), 165102. https://doi.org/10.1063/5.022189010.1063/5.0221890 ↗
46. E.L. Huskins, B. Cao, and K.T. Ramesh, Strengthening Mechanisms in an Al-Mg Alloy, Mater. Sci. Eng. A, 2010, 527(6), p 1292–1298. https://doi.org/10.1016/j.msea.2009.11.05610.1016/j.msea.2009.11.056 ↗
47. D.L. McDowell, Simulation-Based Strategies for Microstructure-Sensitive Fatigue Modeling, Mater. Sci. Eng. A, 2007, 468–470, p 4–14. https://doi.org/10.1016/j.msea.2006.08.12910.1016/j.msea.2006.08.129 ↗
48. Y. Jin et al., Gradient Process Parameter Optimization in Additive Friction Stir Deposition of Aluminum Alloys, Int. J. Mach. Tools Manuf, 2024, 195, 104113. https://doi.org/10.1016/j.ijmachtools.2023.10411310.1016/j.ijmachtools.2023.104113 ↗
49. Y. Jin, T. Yang, T. Wang, S. Dowden, N.B. Dahotre, and A. Neogi, Additive Friction Stir Deposition Induced Stress Ripples in Aluminum Alloy, Int. J. Adv. Manuf. Technol., 2024, 133(5–6), p 2435–2443. https://doi.org/10.1007/s00170-024-13900-510.1007/s00170-024-13900-5 ↗
50. W. Tang, X. Yang, T. Luo, R. Wang, and C. Gu, Precipitation Behavior and Strengthening-Toughening Mechanism of Additive Friction Stir-Deposited Al-Mg-Si-Cu alloy, Addit. Manuf., 2023, 76, 103785. https://doi.org/10.1016/j.addma.2023.10378510.1016/j.addma.2023.103785 ↗
51. P.M. Kelly, The Effect of Particle Shape on Dispersion Hardening, Scr. Metall., 1972, 6(8), p 647–656. https://doi.org/10.1016/0036-9748(72)90120-210.1016/0036-9748(72)90120-2 ↗
52. M. Dixit, R.S. Mishra, and K.K. Sankaran, Structure-Property Correlations in Al 7050 and Al 7055 High-Strength Aluminum Alloys, Mater. Sci. Eng. A, 2008, 478(1–2), p 163–172. https://doi.org/10.1016/j.msea.2007.05.11610.1016/j.msea.2007.05.116 ↗
53. H.R. Shercliff and M.F. Ashby, A process Model for Age Hardening of Aluminium Alloys-I. The Model, Acta Metall. Mater., 1990, 38(10), p 1789–1802. https://doi.org/10.1016/0956-7151(90)90291-N10.1016/0956-7151(90)90291-N ↗
54. D. G. E., Mechanical Metallurgy, 3rd edn in Crystal Research Technology, no. 23(2):194-194. New York: Mc Graw-Hill Book Co., 1986. [Online]. Available: https://doi.org/10.1002/crat.217023021110.1002/crat.2170230211 ↗
55. R.J. Griffiths, D. Garcia, G.D. Hahn, J. Lua, N. Phan, and H.Z. Yu, A Non-Melting Additive Approach to Structural Repair of Aluminum Aircraft Fastener Holes, Addit. Manuf. Lett., 2024, 11, 100249. https://doi.org/10.1016/j.addlet.2024.10024910.1016/j.addlet.2024.100249 ↗
56. T. Shi, J. Wu, M. Ma, E. Charles, and T. Schmitz, AFSD-Nets: A Physics-Informed Machine Learning Model for Predicting the Temperature Evolution during Additive Friction Stir Deposition, J. Manuf. Sci. Eng., 2024, 146(8), 081003. https://doi.org/10.1115/1.406517810.1115/1.4065178 ↗
57. Y. Zhu, X. Wu, N. Gotawala, D.M. Higdon, and H.Z. Yu, Thermal Prediction of Additive Friction Stir Deposition Through Bayesian Learning-Enabled Explainable Artificial Intelligence, J. Manuf. Syst., 2024, 72, p 1–15. https://doi.org/10.1016/j.jmsy.2023.10.01510.1016/j.jmsy.2023.10.015 ↗
58. G.R. Merritt, C.A. Cousin, and H.-S. Yoon, Nonlinear Temperature Control of Additive Friction Stir Deposition Evaluated on an Echo State Network, J. Dyn. Syst. Meas. Control., 2024, 146(2), 021004. https://doi.org/10.1115/1.406400010.1115/1.4064000 ↗
59. Q. Qiao et al., A comparative Study of Machine Learning in Predicting the Mechanical Properties of the Deposited AA6061 Alloys via Additive Friction Stir Deposition, Mater. Genome Eng. Adv., 2024, 2(1), e31. https://doi.org/10.1002/mgea.3110.1002/mgea.31 ↗
60. G. Chen, K. Wu, Y. Wang, Z. Zhu, P. Nie, and F. Hu, Effect of Rotational Speed and Feed Rate on Microstructure and Mechanical Properties of 6061 Aluminum Alloy Manufactured by Additive Friction Stir Deposition, Int. J. Adv. Manuf. Technol., 2023, 127(3–4), p 1165–1176. https://doi.org/10.1007/s00170-023-11527-610.1007/s00170-023-11527-6 ↗
61. Q. Qiao et al., Effect of Heat Input on Microstructure and Mechanical Properties of AA6061 Alloys Fabricated by Additive Friction Stir Deposition, J. Mater. Res. Technol., 2024, 33, p 6182–6195. https://doi.org/10.1016/j.jmrt.2024.10.25610.1016/j.jmrt.2024.10.256 ↗
62. M.B. Williams et al., Dynamic Behavior Characterization of Aluminum alloy 7020 Manufactured Using the Additive Friction Stir Deposition Process, JOM, 2023, 75(11), p 4868–4880. https://doi.org/10.1007/s11837-023-06126-510.1007/s11837-023-06126-5 ↗
63. G.G. Stubblefield et al., Ballistic Evaluation of Aluminum Alloy (AA) 7075 Plate Repaired by Additive Friction Stir Deposition Using AA7075 Feedstock, J. Dyn. Behav. Mater., 2023, 9(1), p 79–89. https://doi.org/10.1007/s40870-022-00363-610.1007/s40870-022-00363-6 ↗
64. W. Lyu et al., Relationship Between Grain Structure Evolution and Tensile Anisotropy in Al-Zn-Mg-Cu Cylindrical Part Formed by Additive Friction Stir Deposition, Mater. Sci. Eng. A, 2024, 918, 147423. https://doi.org/10.1016/j.msea.2024.14742310.1016/j.msea.2024.147423 ↗
65. X. Feng, M. Zhang, T. Jiang, Y. Xie, Z. Sun, and W. Li, Additive Friction Stir Deposition of an Al-Cu-Mg alloy: Microstructure Evolution and Mechanical Properties, Mater Charact, 2024, 218, 114562. https://doi.org/10.1016/j.matchar.2024.11456210.1016/j.matchar.2024.114562 ↗
66. G.D. Hahn, K.P. Knight, N. Gotawala, and H.Z. Yu, Additive Friction Stir Deposition of AA7050 Achieving Forging-Like Tensile Properties, Mater. Sci. Eng. A, 2024, 896, 146268. https://doi.org/10.1016/j.msea.2024.14626810.1016/j.msea.2024.146268 ↗
67. W. Tang, X. Yang, R. Wang, and T. Luo, Tailoring Microstructure of Additive Friction Stir-Deposited Al-Mg Alloy Through Post-Processing Deformation Treatment for Enhancing Mechanical Performance, Mater. Sci. Eng. A, 2023, 885, 145632. https://doi.org/10.1016/j.msea.2023.14563210.1016/j.msea.2023.145632 ↗
68. A. Pariyar et al., Understanding Process Parameter-Induced Variability for Tailoring Precipitation Behavior, Grain Structure, and Mechanical Properties of Al-Mg-Si-Mn Alloy During Solid-State Additive Manufacturing, Mater. Des., 2024, 245, 113238. https://doi.org/10.1016/j.matdes.2024.11323810.1016/j.matdes.2024.113238 ↗
69. L. Chen, Y. Li, L. Lu, Z. Yang, X. Ren, and X. Zhang, The Effect of Heat Treatment on the Microstructure and Mechanical Properties of Multilayer AA6061 Alloy Fabricated by Additive Friction Stir Deposition, Mater. Today Commun., 2024, 38, 108078. https://doi.org/10.1016/j.mtcomm.2024.10807810.1016/j.mtcomm.2024.108078 ↗
70. L. Chen, L. Zhu, L. Lu, Z. Yang, X. Ren, and X. Zhang, The Effect of Heat Treatment on the Microstructure and Electrochemical Corrosion Behavior of Multilayer AA6061 Alloy Fabricated by Additive Friction Stir Deposition, Appl. Surf. Sci., 2024, 650, 159167. https://doi.org/10.1016/j.apsusc.2023.15916710.1016/j.apsusc.2023.159167 ↗
71. E. Bagheri, S. Zavari, N. Adibi, H. Ding, H. Ghadimi, and S. Guo, Additive Friction Stir Deposition of al 7075 Parts and the Effect of Heat Treatment on Microstructure, Electroconductivity, and Mechanical Properties, Int. J. Adv. Manuf. Technol., 2024, 135(1–2), p 763–774. https://doi.org/10.1007/s00170-024-14582-910.1007/s00170-024-14582-9 ↗
72. F. Guo, S. Duan, K. Matsuda, X. Liu, and Y. Zou, The Microstructure and Corrosion Behavior Analysis of Different Aging Al-Zn-Mg-Cu Alloys Manufactured by Additive Friction Stir Deposition, Mater Charact, 2025, 225, 115187. https://doi.org/10.1016/j.matchar.2025.11518710.1016/j.matchar.2025.115187 ↗
73. H. Wang, D. Li, R. Lai, Y. Li, Z. Wang, and Y. Li, Effect of Different Cooling Conditions on Microstructure and Mechanical Properties of Al-Zn-Mg-Cu Alloys Repaired by Additive Friction Stir Deposition, Mater Charact, 2025, 219, 114636. https://doi.org/10.1016/j.matchar.2024.11463610.1016/j.matchar.2024.114636 ↗
74. M. P. E. E Silva, H. Lalvani, A. Reimer, and S. Fitzpatrick, “Understanding the Impact of Additive Friction Stir Deposition on the Production of 7XXX Aluminum Alloy Parts,” in Progress in Additive Manufacturing 2021, N. Shamsaei, N. Hrabe, and M. Seifi, Eds., ASTM International100 (Barr Harbor Drive, West Conshohocken, PA 19428-2959, 2022) p 213–224. https://doi.org/10.1520/STP164420210118.10.1520/STP164420210118 ↗
75. M. Zhang, X. Ye, Y. Li, H. Wang, R. Lai, and Y. Li, Effect of Heat Treatment States of Feedstock on the Microstructure and Mechanical Properties of AA2219 Layers Deposited by Additive Friction Stir Deposition, Materials, 2023, 16(24), 7591. https://doi.org/10.3390/ma1624759110.3390/ma16247591 ↗
76. H. Ghadimi, M. Talachian, H. Ding, S. Emanet, and S. Guo, The Effects of Layer Thickness on the Mechanical Properties of Additive Friction Stir Deposition-Fabricated Aluminum Alloy 6061 Parts, Metals, 2024, 14(1), 101. https://doi.org/10.3390/met1401010110.3390/met14010101 ↗
77. L.P. Martin, A. Luccitti, and M. Walluk, Repair of Aluminum 6061 Plate by Additive Friction Stir Deposition, Int. J. Adv. Manuf. Technol., 2022, 118(3–4), p 759–773. https://doi.org/10.1007/s00170-021-07953-z10.1007/s00170-021-07953-z ↗
78. P. Allison et al., Understanding the Influence of Heat Input and Deposition Pitch on Achieving Isotropic Tensile Behavior in Large-Scale Am of Aa7075 Additive Friction Stir Depositions, SSRN 4965160, 2024 https://doi.org/10.2139/ssrn.496516010.2139/ssrn.4965160 ↗
79. X. Zhu, R. Wang, L. Wang, M. Liu, and S. Li, Effect of Rotational Shear and Heat Input on the Microstructure and Mechanical Properties of Large-Diameter 6061 Aluminium Alloy Additive Friction Stir Deposition, Crystals, 2024, 14(7), 581. https://doi.org/10.3390/cryst1407058110.3390/cryst14070581 ↗
80. J. Hu et al., Effect of Teardrop-Shaped Protrusions and Sc Micro-Additions on Resulting Microstructure and Tensile Behavior of Al-Ce-Sc Alloy Fabricated by Additive Friction Stir Deposition, J. Manuf. Process., 2025, 141, p 1752–1765. https://doi.org/10.1016/j.jmapro.2025.03.07510.1016/j.jmapro.2025.03.075 ↗
81. M. Zhang, T. Jiang, Y. Su, Z. Sun, Y. Xu, and W. Li, Study on the Interfacial Bonding Behavior of Dissimilar Aluminum Alloys via Additive Friction Stir Deposition, Prog. Nat. Sci. Mater. Int., 2025, 35(2), p 433–439. https://doi.org/10.1016/j.pnsc.2025.02.00810.1016/j.pnsc.2025.02.008 ↗
82. G. Chen et al., Quantitative Study on the Correlation Between Microstructure and Mechanical Properties of Additive Friction Stir Deposited 6061-T6 Al-Mg-Si Alloy, J. Mater. Res. Technol., 2023, 25, p 6725–6736. https://doi.org/10.1016/j.jmrt.2023.07.09710.1016/j.jmrt.2023.07.097 ↗
83. R.P. Kinser et al., Effects on Microstructure and Mechanical Properties of Aluminum alloy 6061 Processed via Underwater Additive Friction Stir Deposition, J. Manuf. Process., 2025, 134, p 932–942. https://doi.org/10.1016/j.jmapro.2025.01.00610.1016/j.jmapro.2025.01.006 ↗
84. Q. Qiao et al., Hybrid Heat-Source Solid-State Additive Manufacturing: A Method to Fabricate High Performance AA6061 Deposition, J. Mater. Sci. Technol., 2025, 228, p 107–124. https://doi.org/10.1016/j.jmst.2024.11.07910.1016/j.jmst.2024.11.079 ↗
85. Q. Qiao et al., In-Situ Monitoring of Additive Friction Stir Deposition of AA6061: Effect of Layer Thickness on the Microstructure and Mechanical Properties, Additive Manuf., 2024, 84, 104141. https://doi.org/10.1016/j.addma.2024.10414110.1016/j.addma.2024.104141 ↗
86. W. Tang, X. Yang, C. Tian, and C. Gu, Effect of Rotation Speed on Microstructure and Mechanical Anisotropy of Al-5083 Alloy Builds Fabricated by Friction Extrusion Additive Manufacturing, Mater. Sci. Eng. A, 2022, 860, 144237. https://doi.org/10.1016/j.msea.2022.14423710.1016/j.msea.2022.144237 ↗
87. M.B. Williams et al., Towards Understanding the Relationships Between Processing Conditions and Mechanical Performance of the Additive Friction Stir Deposition Process, Metals, 2023, 13(10), 1663. https://doi.org/10.3390/met1310166310.3390/met13101663 ↗
88. D.Z. Avery et al., Influence of Grain Refinement and Microstructure on Fatigue Behavior for Solid-State Additively Manufactured Al-Zn-Mg-Cu Alloy, Metall. Mater. Trans. A, 2020, 51(6), p 2778–2795. https://doi.org/10.1007/s11661-020-05746-910.1007/s11661-020-05746-9 ↗
89. S. Li et al., Microstructure Evolution and Mechanical Properties of High-Strength Aluminum Alloy Prepared by Additive Friction Stir Deposition, J. Mater. Res. Technol., 2025, 36, p 1774–1788. https://doi.org/10.1016/j.jmrt.2025.03.17810.1016/j.jmrt.2025.03.178 ↗
90. F. Girault, L. Toualbi, Q. Barres, and E. Charkaluk, Investigating Multi-Scale Heterogeneity in Multi-Layer Additive Friction Stir Deposition of High-Strength Aluminum Alloys, Mater. Sci. Eng. A, 2025, 927, 147979. https://doi.org/10.1016/j.msea.2025.14797910.1016/j.msea.2025.147979 ↗
91. E. Acquah, S. Bhowmik, A.F.M.M. Hossain, and N. Kumar, Stress Corrosion Cracking of AA7075 Aluminum Alloy Processed via Additive Friction Stir Deposition, J. Mater. Eng. Perform., 2025, 34(10), p 8963–8977. https://doi.org/10.1007/s11665-025-10738-010.1007/s11665-025-10738-0 ↗
92. H. Gao, P. Dong, and Z. Wei, Microstructure and Properties of 6061 Aluminum Alloy by Additive Friction Stir Deposition, Metals, 2025, 15(5), 539. https://doi.org/10.3390/met1505053910.3390/met15050539 ↗
93. P.C. Metz et al., Heterogeneous Microstructure Development in Additive Friction-Stir Deposited Al-Mg-Si Alloy, Addit. Manuf., 2024, 81, 103989. https://doi.org/10.1016/j.addma.2024.10398910.1016/j.addma.2024.103989 ↗
94. T. Yang, Y. Jin, T. Wang, S. Dowden, A. Neogi, and N.B. Dahotre, Stress Interference in Multilayer Additive Friction Stir Deposition of AA6061 Aluminum, Int. J. Adv. Manuf. Technol., 2024, 132(11–12), p 5385–5393. https://doi.org/10.1007/s00170-024-13688-410.1007/s00170-024-13688-4 ↗
95. L. Chen et al., Microstructure Evolution and Mechanical Properties of Multilayer AA6061 Alloy Fabricated by Additive Friction Stir Deposition, Metall. Mater. Trans. A, 2024, 55(4), p 1049–1064. https://doi.org/10.1007/s11661-024-07303-010.1007/s11661-024-07303-0 ↗
96. V. Yakubov et al., Hardness Distribution and Defect Formation in Aluminium Alloys Fabricated via Additive Friction Stir Deposition (AFSD).
97. V. Yakubov et al., Evolution of Material Properties and Residual Stress with Increasing Number of Passes in Aluminium Structure Printed via Additive Friction Stir Deposition, Materials, 2024, 17(14), 3457. https://doi.org/10.3390/ma1714345710.3390/ma17143457 ↗
98. H. Ghadimi et al., Hardness Distribution of Al2050 Parts Fabricated Using Additive Friction Stir Deposition, Materials, 2023, 16(3), 1278. https://doi.org/10.3390/ma1603127810.3390/ma16031278 ↗
99. R.B. Gottwald, R.J. Griffiths, D.T. Petersen, M.E.J. Perry, and H.Z. Yu, Solid-State Metal Additive Manufacturing for Structural Repair, Acc. Mater. Res., 2021, 2(9), p 780–792. https://doi.org/10.1021/accountsmr.1c0009810.1021/accountsmr.1c00098 ↗
100. H. Livatyali and O. Keles, Additive Friction Stir Deposition for Aluminum Alloys in Aerospace Applications, Alum. Technol. Aerosp. Appl., 2025, 1, p 149–188.