journal article·2023-08

The Cytotoxic and Genotoxic Assays of Mg-Ag Alloy Doped with Zn, Ca, and Nd Elements

Levent Elen, Yunus Turen, Bunyamin Cicek, Busra Moren Bozer, A. Najah Saud, Erkan Koc

Publisher page

Abstract

Magnesium alloys are being studied for their potential as biodegradable metals, and there is a growing need for multipurpose materials, such as those with more than one use. Binary Mg-Ag alloys were developed as implant materials, combining the beneficial qualities of magnesium with silver's well-known compatibility feature. The result shows that as the amount of the added Ag in the cast alloys increased, the secondary phases (Mg4Ag and Mg54Ag17) that appeared in the structure became more pronounced, and the grains became finer. The best percentage of Ag was found to be 3%, so Ca, Zn and Nd were added, and a study of the biocompatible Mg-3Ag alloy's cytotoxicity and genotoxicity showed that the alloy is safe for cells. In conclusion, 1/1 (total material concentration) cell viability for QE-30, QZ-30, QX-30, and QZEX3000 was 79.39 +/- 1.85, 106.46 +/- 1.99, 93.55 +/- 2.4, and 141.76 +/- 2.71%, respectively. Reducing material concentration by 50% (application at 1/2 concentration) raised viability to 96.83 +/- 1.35, 108.40 +/- 1.92, 124.71 +/- 2.76, and 129.05 +/- 3.5%, indicating the as-cast Mg + 3%Ag + 0.5% Nd-Ca-Zn alloy was extremely biocompatible.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Hydrogen Storage and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. V. Tsakiris, C. Tardei, and F.M. Clicinschi, Biodegradable Mg Alloys for Orthopedic Implants—A Review, J. Magnes. Alloys, 2021, 9(6), p 1884–1904.10.1016/j.jma.2021.06.024 ↗
2. F. Witte, N. Hort, and C. Vogt et al., Degradable Biomaterials Based on Magnesium Corrosion, Curr. Opin. Solid State Mater. Sci., 2008, 12(5–6), p 63–72.10.1016/j.cossms.2009.04.001 ↗
3. G.E.J. Poinern, S. Brundavanam, and D. Fawcett, Biomedical Magnesium Alloys: A Review of Material Properties, Surface Modifications and Potential as a Biodegradable Orthopaedic Implant, Am. J. Biomed. Eng., 2012, 2(6), p 218–240.10.5923/j.ajbe.20120206.02 ↗
4. Y.F. Zheng, X.N. Gu, and F. Witte, Biodegradable Metals, Mater. Sci. Eng. R. Rep., 2014, 77, p 1–34.10.1016/j.mser.2014.01.001 ↗
5. A. Atrens, M. Liu, and N.I.Z. Abidin, Corrosion Mechanism Applicable to Biodegradable Magnesium Implants, Mater. Sci. Eng. B, 2011, 176(20), p 1609–1636.10.1016/j.mseb.2010.12.017 ↗
6. S.F. Hassan, M. Islam, N. Saheb, and M. Baig, Magnesium for Implants: A Review on the Effect of Alloying Elements on Biocompatibility and Properties, Material, 2022, 15(16), p 5669.10.3390/ma15165669 ↗
7. S. Zhang, X. Zhang, C. Zhao et al., Research on an Mg-Zn alloy as a Degradable Biomaterial, Acta Biomater., 2010, 6(2), p 626–640.10.1016/j.actbio.2009.06.028 ↗
8. L. Elen, Y. Turen, H. Ahlatci, M. Unal, and D. Ergin, Microstructural, Mechanical, and In vitro Corrosion Properties of Biodegradable Mg-Ag Alloys, Biointerphases, 2022, 17(4), p 041001.10.1116/6.0001858 ↗
9. Elen L. Investigation of the Effect of Additional Elements on the Mechanical and Biodegradability Properties of Mg-AG Alloys, Doctoral Dissertation, Karabük Üniversitesi, Türkiye, 2021
10. H. Yang, B. Jia, Z. Zhang et al., Alloying Design of Biodegradable Zinc as Promising Bone Implants for Load-Bearing Applications, Nat. Commun., 2020, 11(1), p 1–16.10.1038/s41467-019-13993-7 ↗
11. F. Rosalbino, S. De Negri, A. Saccone, E. Angelini, and S. Delfino, Bio-Corrosion Characterization of Mg-Zn-X (X= Ca, Mn, Si) Alloys for Biomedical Applications, J. Mater. Scie. Mater. Med., 2010, 21(4), p 1091–1098.10.1007/s10856-009-3956-1 ↗
12. T. Zhang, G. Meng, Y. Shao, Z. Cui, and F. Wang, Corrosion of Hot Extrusion AZ91 Magnesium Alloy. Part II: Effect of Rare Earth Element Neodymium (Nd) on the Corrosion Behavior of Extruded Alloy, Corros. Sci., 2011, 53(9), p 2934–2942.10.1016/j.corsci.2011.05.035 ↗
13. R. Arrabal, E. Matykina, A. Pardo et al., Corrosion Behaviour of AZ91D and AM50 Magnesium Alloys with Nd and Gd Additions in Humid Environments, Corros. Sci., 2012, 55, p 351–362.10.1016/j.corsci.2011.10.038 ↗
14. Q. Wang, W. Jin, G. Wu et al., Rare-Earth-Incorporated Polymeric Vector for Enhanced Gene Delivery, Biomaterials, 2014, 35(1), p 479–488.10.1016/j.biomaterials.2013.09.069 ↗
15. W. Jin, G. Wu, H. Feng, W. Wang, X. Zhang, and P.K. Chu, Improvement of Corrosion Resistance and Biocompatibility of Rare-Earth WE43 Magnesium Alloy by Neodymium Self-Ion Implantation, Corros. Sci., 2015, 94, p 142–155.10.1016/j.corsci.2015.01.049 ↗
16. E. Willbold, X. Gu, D. Albert et al., Effect of the Addition of Low Rare Earth Elements (Lanthanum, Neodymium, Cerium) on the Biodegradation and Biocompatibility of Magnesium, J Acta Biomater., 2015, 11, p 554–562.10.1016/j.actbio.2014.09.041 ↗
17. Y. Li, P.D. Hodgson, and C.E. Wen, The Effects of Calcium and Yttrium Additions on the Microstructure, Mechanical Properties and Biocompatibility of Biodegradable Magnesium Alloys, J. Mater. Sci., 2011, 46(2), p 365–371.10.1007/s10853-010-4843-3 ↗
18. E. Dabah, G. Ben-Hamu, V. Lisitsyn, D. Eliezer, and K. Shin, The Influence of Ca on the Corrosion Behavior of New Die Cast Mg-Al-Based Alloys for Elevated Temperature Applications, J. Mater. Sci., 2010, 45(11), p 3007–3015.10.1007/s10853-010-4302-1 ↗
19. Y. Sun, Y. Huang, H. Fan et al., In vitro and In vivo Biocompatibility of an Ag-Bearing Zr-Based Bulk Metallic Glass for Potential Medical use, J. Non Cryst. Solids., 2015, 419, p 82–91.10.1016/j.jnoncrysol.2015.03.039 ↗
20. Y. Dai, Y. Tang, X. Xu et al., Evaluation of the Mechanisms and Effects of Mg-Ag-Y alloy on the Tumor Growth and Metastasis of the MG63 Osteosarcoma Cell Line, J. Biomed. Mater. Res. Part B Appl. Biomater., 2019, 107(8), p 2537–2548.10.1002/jbm.b.34344 ↗
21. U. Erdem, B.M. Bozer, M.B. Turkoz et al., Spectral Analysis and Biological Activity Assessment of Silver Doped Hydroxyapatite, J. Asian Ceram. Soc., 2021, 9(4), p 1524–1545.10.1080/21870764.2021.1989749 ↗
22. P. Pérez, S. Cabeza, G. Garcés, and P. Adeva, Influence of Long Period Stacking Ordered Phase Arrangements on the Corrosion Behaviour of Extruded Mg97Y2Zn1 Alloy, Corros. Sci., 2016, 107, p 107–112.10.1016/j.corsci.2016.02.024 ↗
23. Iso IS, Biological Evaluation of Medical Devices. Part 5: Tests for In Vitro Cytotoxicity, ISO, Switzerland, 2009
24. S.G. Iz, S.İ Gürhan, B.H. Şen, T. Endoğan, and N. Hasirci, Comparison of in vitro Cytotoxicity and Genotoxicity of MMA-Based Polymeric Materials and Various Metallic Materials, Turkish J. Med. Sci., 2010, 40(6), p 905–916.
25. G.P. Ellis and G.B. West, Progress in Medicinal Chemistry, Elsevier, Amsterdam, 2011.
26. Catacchio I, Berardi S, Reale A, et al. Evidence for Bone Marrow Adult Stem Cell Plasticity: Properties, Molecular Mechanisms, Negative Aspects, and Clinical Applications of Hematopoietic and Mesenchymal Stem Cells Transdifferentiation. Stem Cells Int. 2013;2013.10.1155/2013/589139 ↗
27. K. Mortelmans and E. Zeiger, The Ames Salmonella/Microsome Mutagenicity Assay, Mutat. Res Fundam. Mol. Mech. Mutagen., 2000, 455(1–2), p 29–60.10.1016/S0027-5107(00)00064-6 ↗
28. R.T. Przygoda, Safety Assessment and Global Regulatory Requirements for Genetic Toxicity Evaluations of Medical Devices, Environ. Mol. Mutagen., 2017, 58(5), p 375–379.10.1002/em.22102 ↗
29. J. Wu, L. Wang, J. He, and C. Zhu, In vitro Cytotoxicity of Cu2+, Zn2+, Ag+ and their Mixtures on Primary Human Endometrial Epithelial Cells, Contraception, 2012, 85(5), p 509–518.10.1016/j.contraception.2011.09.016 ↗
30. M.H. Yoo, J.-Y. Lee, S.E. Lee, J.-Y. Koh, and Y.H. Yoon, Protection by Pyruvate of Rat Retinal Cells Against Zinc Toxicity In vitro, and Pressure-Induced Ischemia In vivo, Invest. Ophthalmol. Vis. Sci., 2004, 45(5), p 1523–1530.10.1167/iovs.03-1315 ↗
31. V. Rodilla, A.T. Miles, W. Jenner, and G.M. Hawksworth, Exposure of Cultured Human Proximal Tubular Cells to Cadmium, Mercury, Zinc and Bismuth: Toxicity and Metallothionein Induction, Chemic Biol. Interact., 1998, 115(1), p 71–83.10.1016/S0009-2797(98)00059-3 ↗
32. J. Cheng, B. Liu, Y. Wu, and Y. Zheng, Comparative In vitro Study on Pure Metals (Fe, Mn, Mg, Zn and W) as Biodegradable Metals, J. Mater. Sci. Technol., 2013, 29(7), p 619–627.10.1016/j.jmst.2013.03.019 ↗
33. H. Li, X. Xie, Y. Zheng et al., Development of biodegradable Zn-1X Binary Alloys with Nutrient Alloying Elements Mg Ca and Sr, Sci. Rep., 2015, 5(1), p 1–14.
34. H. Gong, K. Wang, R. Strich, and J.G. Zhou, In vitro Biodegradation Behavior, Mechanical Properties, and Cytotoxicity Of Biodegradable Zn-Mg alloy, J. Biomed. Mater. Res. Part B Appl. Biomater., 2015, 103(8), p 1632–1640.10.1002/jbm.b.33341 ↗
35. N. Murni, M. Dambatta, S. Yeap, G. Froemming, and H. Hermawan, Cytotoxicity Evaluation of Biodegradable Zn-3Mg Alloy Toward Normal Human Osteoblast Cells, Mater. Sci. Eng. C., 2015, 49, p 560–566.10.1016/j.msec.2015.01.056 ↗
36. M. Dambatta, N. Murni, S. Izman, D. Kurniawan, G. Froemming, and H. Hermawan, In vitro Degradation and Cell Viability Assessment of Zn-3Mg Alloy for Biodegradable Bone Implants, Proc. Inst. Mech. Eng. Part H J. Eng. Med., 2015, 229(5), p 335–342.10.1177/0954411915584962 ↗
37. L. Elen, Y. Turen, H. Ahlatci, Y. Sun, and M. Unal, Investigation of Microstructure, Mechanical and Corrosion Properties of Biodegradable Mg-Ag Alloys, Arch. Metall. Mater., 2022, 67(3), p 041001.
38. 10993-3 I-aID. Biological Evaluation of Medical Devices—Part 3: Tests for Genotoxicity, Carcinogenicity and Reproductive Toxicity. Geneva, Switzerland. (2000)
39. P.L. Olive and J.P. Banáth, The Comet Assay: a Method to Measure DNA Damage in Individual Cells, Nat. protoc., 2006, 1(1), p 23–29.10.1038/nprot.2006.5 ↗
40. A. Comba, B. Cicek, B. Comba et al., Investigation of in-vitro Biocompatibility and in-vivo Biodegradability of AM Series Mg Alloys, Mater. Technol., 2022, 37, p 1–13.10.1080/10667857.2022.2081115 ↗
41. M. Can, S. Demirci, Y. Yildrim, C.Ç. Çoban, M. Turk, and N. Sahiner, Modification of Halloysite Clay Nanotubes with Various Alkyl Halides, and their Characterization, Blood Compatibility, Biocompatibility, and Genotoxicity, Mater. Chem. Phys., 2021, 259, p 124013.10.1016/j.matchemphys.2020.124013 ↗
42. R. Rajendran and S. Dondapati, Insights of Microstructural Features and their Effect on Degradation and the In vitro Bioactivity Response of as-Cast Mg-Sn Alloys for Orthopedic Implant Applications, Materials., 2022, 15(18), p 6327.10.3390/ma15186327 ↗
43. D. Tie, F. Feyerabend, W.-D. Mueller et al., Antibacterial Biodegradable Mg-Ag alloys, Eur. cells Mater., 2013, 25, p 284–298. (Discussion 298)10.22203/eCM.v025a20 ↗
44. H.M. Wong, Y. Zhao, V. Tam et al., In vivo Stimulation of Bone Formation by Aluminum and Oxygen Plasma Surface-Modified Magnesium Implants, Biomaterials, 2013, 34(38), p 9863–9876.10.1016/j.biomaterials.2013.08.052 ↗
45. K. Bryła, J. Horky, M. Krystian, L. Lityńska-Dobrzyńska, and B. Mingler, Microstructure, Mechanical Properties, and Degradation of Mg-Ag Alloy after Equal-Channel Angular Pressing, Mater. Sci. Eng. C., 2020, 109, p 110543.10.1016/j.msec.2019.110543 ↗
46. J. Wang, Z. Zhang, Y. Zhang, L. Jin, and L. Sheng, Experimental Measurement on the Phase Equilibria of the Mg-Ag-Cu Ternary System at 350 and 400 °C, J. Magnes. Alloys., 2022, 10(2), p 449–457.10.1016/j.jma.2020.12.019 ↗
47. A. Rakowska, M. Podosek, and R. Ciach, Some Aspects of Solidification and Homogenisation of Mg-Ag Alloys, Mater. Des., 1997, 18(4–6), p 279–283.10.1016/S0261-3069(97)00064-2 ↗
48. L. Sheng, X. Zhang, H. Zhao, B. Du, Y. Zheng, and T. Xi, Influence of Multi-Pass Hot Extrusion on Microstructure and Mechanical Properties of the Mg-4Zn-1.2 Y-0.8 Nd Alloy, Crystals, 2021, 11(4), p 425.10.3390/cryst11040425 ↗
49. S. Gorsse, C.R. Hutchinson, B. Chevalier, and J.-F. Nie, A Thermodynamic Assessment of the Mg-Nd Binary System Using Random Solution and Associate Models for the Liquid Phase, J. Alloys Compd., 2005, 392(1–2), p 253–262.10.1016/j.jallcom.2004.09.040 ↗
50. Wang J, Meng L, Zhang Z, et al. Investigation on the Crystal Structure and Mechanical Properties of the Ternary Compound Mg11-xZnxSr Combined with Experimental Measurements and First-Principles Calculations. J. Magnes. Alloys (2021). https://doi.org/10.1016/j.jma.2021.07.01110.1016/j.jma.2021.07.011 ↗
51. G. Ben-Hamu, D. Eliezer, A. Kaya, Y. Na, and K. Shin, Microstructure and Corrosion Behavior of Mg-Zn-Ag Alloys, Mater. Sci. Eng. A., 2006, 435, p 579–587.10.1016/j.msea.2006.07.109 ↗
52. C.M. Santoro, N.L. Duchsherer, and D.W. Grainger, Minimal In vitro Antimicrobial Efficacy and Ocular Cell Toxicity from Silver Nanoparticles, NanoBiotechnology, 2007, 3(2), p 55–65.10.1007/s12030-008-9007-z ↗
53. Drewa T, Szmytkowska K, Chaberski M. The short term exposition of AgNO3 on 3T3 mouse fibroblasts cell line. Acta Pol Pharm. 64(4), (2007)
54. J. Fischer, D. Pröfrock, N. Hort, R. Willumeit, and F. Feyerabend, Reprint of: Improved Cytotoxicity Testing of Magnesium Materials, Mater. Sci. Eng. B, 2011, 176(20), p 1773–1777.10.1016/j.mseb.2011.06.002 ↗
55. V. PeŠŠková, D. Kubies, H. Hulejova, and L. Himmlova, The Influence of Implant Surface Properties on Cell Adhesion and Proliferation, J. Mater. Sci. Mater. Med., 2007, 18(3), p 465–473.10.1007/s10856-007-2006-0 ↗
56. Y. Yun, Z. Dong, N. Lee et al., Revolutionizing Biodegradable Metals, Mater. Today., 2009, 12(10), p 22–32.10.1016/S1369-7021(09)70273-1 ↗
57. D. Tie, F. Feyerabend, N. Hort, R. Willumeit, and D. Hoeche, XPS Studies of Magnesium Surfaces After Exposure to Dulbecco’s Modified Eagle Medium, Hank’s Buffered Salt Solution, and Simulated Body Fluid, Adv. Eng. Mater., 2010, 12(12), p B699–B704.10.1002/adem.201080070 ↗
58. C L. Liu, J. Jiang, M. Wang, Y.J. Wang , P.K. Chu\, and W.J. Huang, In vitro Degradation and Biocompatibility of WE43, ZK60, and AZ91 Biodegradable Magnesium Alloys. Paper presented at: Advanced Materials Research 2011.10.4028/www.scientific.net/AMR.287-290.2008 ↗
59. K.K. Khanna and S.P. Jackson, DNA Double-Strand Breaks: Signaling, Repair and the Cancer Connection, Nat. Genet., 2001, 27(3), p 247–254.10.1038/85798 ↗
60. J. Jiang, K. Huo, Z. Wu et al., Silicon-induced DNA Damage Pathway and Its Modulation by Titanium Plasma Immersion Ion Implantation, Biomaterials, 2008, 29(5), p 544–550.10.1016/j.biomaterials.2007.10.013 ↗