journal article·2024-10

Impact of High Temperature and Water Vapor on the Oxidation Behavior of Chemical Vapor Infiltration-SiCf/SiC Composite

Anu Mohan, A. Udayakumar, M. Kamaraj, Ashutosh S. Gandhi

Publisher page

Abstract

SiCf/SiC composites are replacing superalloy components in hot sections of gas turbines. The high-velocity combustion gases in gas turbine hot sections contain water vapor. The mechanism of oxidative water vapor attack on SiC is vastly different from that of oxidation in static dry air. Therefore, it is of paramount importance to study the oxidation of these composites in high-velocity combustion environments. This study focuses on the high-temperature oxidation behavior of SiCf/SiC composites with a BN interfacial coating in both static air and combustion environments. The composite was prepared by the chemical vapor infiltration process (CVI). To elucidate the impact of water vapor in a combustion environment, an oxyacetylene flame apparatus was used. Oxidation of the SiCf/SiC composite was investigated at 1200, 1300 and 1400 °C, for up to 100 h in static dry air, and for up to 24 h in a combustion environment. The microstructure evolution and recession of the composite under combustion environment were investigated by scanning electron microscopy. The oxidation kinetics of the SiCf/SiC composite showed a parabolic nature in static air; however, in the combustion environment the composite showed accelerated mass loss owing to the concurrent effects of oxidation and recession.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. R.R. Naslain, SiC-Matrix Composites: Nonbrittle Ceramics for Thermo-Structural Application, Int. J. Appl. Ceram. Technol., 2005, 2(2), p 75–84.10.1111/j.1744-7402.2005.02009.x ↗
2. M. Steinbrueck, M. Grosse, U. Stegmaier, J. Braun, and C. Lorrette, Oxidation of Silicon Carbide Composites for Nuclear Applications at Very High Temperatures in Steam, Coatings, 2022, 12(7), p 875.10.3390/coatings12070875 ↗
3. Y. Arai, Y. Aoki, and Y. Kagawa, Effect of Cristobalite Formation on the Delamination Resistance of an Oxide/Si/(SiC/SiC) Environmental Barrier Coating System after Cyclic High Temperature Thermal Exposure, Scr. Mater., 2017, 139, p 58–62. https://doi.org/10.1016/j.scriptamat.2017.06.00610.1016/j.scriptamat.2017.06.006 ↗
4. F.W. Zok, P.T. Maxwell, K. Kawanishi, and E.B. Callaway, Degradation of a SiC-SiC Composite in Water Vapor Environments, J. Am. Ceram. Soc., 2020, 103(3), p 1927–1941.10.1111/jace.16838 ↗
5. Y. Katoh, L.L. Snead, C.H. Henager, T. Nozawa, T. Hinoki, A. Iveković, S. Novak, and S.M. Gonzalez De Vicente, Current Status and Recent Research Achievements in SiC/SiC Composites, J. Nucl. Mater., 2014, 455(1–3), p 387–397.10.1016/j.jnucmat.2014.06.003 ↗
6. N.S. Jacobson, Corrosion of Silicon-Based Ceramics in Combustion Environments, J. Am. Ceram. Soc., 1993, 76(1), p 3–28.10.1111/j.1151-2916.1993.tb03684.x ↗
7. T. Ogasawara, T. Aoki, M.S.A. Hassan, Y. Mizokami, and N. Watanabe, Ablation Behavior of SiC Fiber/Carbon Matrix Composites under Simulated Atmospheric Reentry Conditions, Compos. Part A Appl. Sci. Manuf, 2011, 42(3), p 221–228. https://doi.org/10.1016/j.compositesa.2010.10.01510.1016/j.compositesa.2010.10.015 ↗
8. E.J. Opila, Oxidation and Volatilization of Silica Formers in Water Vapor, J. Am. Ceram. Soc., 2003, 86(8), p 1238–1248.10.1111/j.1151-2916.2003.tb03459.x ↗
9. A. Udayakumar, P.M. Raole, and M. Balasubramanian, Synthesis of Tailored 2D SiCf/SiC Ceramic Matrix Composites with BN/C Interphase through ICVI, J. Nucl. Mater., 2011, 417(1–3), p 363–366. https://doi.org/10.1016/j.jnucmat.2010.12.25310.1016/j.jnucmat.2010.12.253 ↗
10. R.B. Reitz, F.W. Zok, and C.G. Levi, Reactive Alloy Melt Infiltration for SiC Composite Matrices: Mechanistic Insights, J. Am. Ceram. Soc., 2017, 100(12), p 5471–5481.10.1111/jace.15167 ↗
11. E.J. Opila, Oxidation Kinetics of Chemically Vapor-Deposited Silicon Carbide in Wet Oxygen, J. Am. Ceram. Soc., 1994, 77(3), p 730–736.10.1111/j.1151-2916.1994.tb05357.x ↗
12. E.J. Opila and M.K. Boyd, Oxidation of SiC Fiber-Reinforced SiC Matrix Composites with a BN Interphase, Mater. Sci. Forum, 2011, 696, p 342–347.10.4028/www.scientific.net/MSF.696.342 ↗
13. S. Wu, L. Cheng, and L. Zhang, Oxidation Behavior of 3D Hi-Nicalon/SiC Composite Exposed in Wet and Simulated Air Environments, Corros. Sci., 2013, 66, p 111–117. https://doi.org/10.1016/j.corsci.2012.09.00810.1016/j.corsci.2012.09.008 ↗
14. G. Sun, Y. Wu, X. Luan, X. Xu, X. Cao, J. Zhang, H. Zhao, Q. Zhang, and L. Cheng, Non-Destruction Evaluation Method for Long-Term Oxidation Behavior of SiC/SiC Composites with Different Preforms in Wet Oxygen, Materials (Basel), 2022, 15(11), p 3812.10.3390/ma15113812 ↗
15. Z. Peng, W. Sun, X. Xiong, H. Zhang, F. Guo, and J. Li, Novel Refractory High-Entropy Ceramics: Transition Metal Carbonitrides with Superior Ablation Resistance, Corros. Sci., 2021, 184, p 109359.10.1016/j.corsci.2021.109359 ↗
16. L. Silvestroni, A. Vinci, S. Failla, L. Zoli, V. Rubio, J. Binner, and D. Sciti, Ablation Behaviour of Ultra-High Temperature Ceramic Matrix Composites: Role of MeSi2 Addition, J. Eur. Ceram. Soc., 2019, 39(9), p 2771–2781. https://doi.org/10.1016/j.jeurceramsoc.2019.03.03110.1016/j.jeurceramsoc.2019.03.031 ↗
17. A. Mohan, A. Udayakumar, and A.S. Gandhi, High Temperature Oxidation Behaviour of CVD β-SiC Seal Coated SiCf/SiC Composites in Static Dry Air and Combustion Environment, Ceram. Int., 2017, 43(12), p 9472–9480. https://doi.org/10.1016/j.ceramint.2017.04.12510.1016/j.ceramint.2017.04.125 ↗
18. A. Udayakumar, A. Sri Ganesh, S. Raja, and M. Balasubramanian, Effect of Intermediate Heat Treatment on Mechanical Properties of SiCf/SiC Composites with BN Interphase Prepared by ICVI, J. Eur. Ceram. Soc., 2011, 31(6), p 1145–1153. https://doi.org/10.1016/j.jeurceramsoc.2010.12.01810.1016/j.jeurceramsoc.2010.12.018 ↗
19. A. Udayakumara, M. Stalin, M.B. Abhayalakshmi, and R. Hariharan, Effect of Thermal Cycling of SiCf/SiC Composites on Their Mechanical Properties, Mater. Sci. Eng. A, 2013, 586(1–3), p 330–337. https://doi.org/10.1016/j.msea.2013.07.01710.1016/j.msea.2013.07.017 ↗
20. ASTM, Standard Test Method for Oxyacetylene Ablation Testing of Thermal Insulation, Annu. B. ASTM Stand., 2002, 80(Reapproved), p 1–6.
21. E.J. Opila and R.E. Hann, Paralinear Oxidation of CVD SiC in Water Vapor, J. Am. Ceram. Soc., 1997, 80(1), p 197–205.10.1111/j.1151-2916.1997.tb02810.x ↗
22. J.A.C.R.E. Tressler, Oxygen Penetration into Silicon Carbide Ceramics during Oxidation, Ceram. Int., 1984, 2, p 39–44.
23. C.E. Ramberg and W.L. Worrell, Oxygen Transport in Silica at High Temperatures: Implications of Oxidation Kinetics, J. Am. Ceram. Soc., 2001, 84, p 2607.10.1111/j.1151-2916.2001.tb01061.x ↗
24. L.U.J.T. Ogbuji, Effect of Oxide Devitrification on Oxidation Kinetics of SiC, J. Am. Ceram. Soc., 1997, 50(191593), p 1544–1550.10.1111/j.1151-2916.1997.tb03014.x ↗
25. V. Presser and K.G. Nickel, Silica on Silicon Carbide, Crit. Rev. Solid State Mater. Sci., 2008, 33(1), p 1–99. https://doi.org/10.1080/1040843070171891410.1080/10408430701718914 ↗
26. X. Sun, X. Yin, X. Fan, X. Ma, X. Cao, L. Cheng, and L. Zhang, Oxidation Resistance of SiC/SiC Composites Containing SiBC Matrix Fabricated by Liquid Silicon Infiltration, J. Eur. Ceram. Soc., 2018, 38(2), p 479–485. https://doi.org/10.1016/j.jeurceramsoc.2017.09.00410.1016/j.jeurceramsoc.2017.09.004 ↗
27. W. Pabst and E. Gregorová, Elastic Properties of Silica Polymorphs—A Review, Ceramics-Silikáty, 2013, 57(3), p 167–184.
28. E.J. Opila, Variation of the Oxidation Rate of Silicon Carbide with Water-Vapor Pressure, J. Am. Ceram. Soc., 1999, 82, p 625–636.10.1111/j.1151-2916.1999.tb01810.x ↗
29. R. Naslain, A. Guette, F. Rebillat, S. Le Gallet, F. Lamouroux, L. Filipuzzi, and C. Louchet, Oxidation Mechanisms and Kinetics of SiC-Matrix Composites and Their Constituents, J. Mater. Sci., 2004, 39(24), p 7303–7316.10.1023/B:JMSC.0000048745.18938.d5 ↗
30. R. Naslain, Design, Preparation and Properties of Non-Oxide CMCs for Application in Engines and Nuclear Reactors: An Overview, Compos. Sci. Technol., 2004, 64(2), p 155–170. https://doi.org/10.1016/S0266-3538(03)00230-610.1016/S0266-3538(03)00230-6 ↗
31. N.S. Jacobson and D.L. Myers, Active Oxidation of SiC, Oxid. Met., 2010, 75(1–2), p 1–25. https://doi.org/10.1007/s11085-010-9216-410.1007/s11085-010-9216-4 ↗
32. B.E. Deal and A.S. Grove, General Relationship for the Thermal Oxidation of Silicon, J. Appl. Phys., 1965, 36(12), p 3770. https://doi.org/10.1063/1.171394510.1063/1.1713945 ↗
33. L.U.J.T. Ogbuji, A Pervasive Mode of Oxidative Degradation in a SiC-SiC Composite, J. Am. Ceram. Soc., 1998, 81(11), p 2777–2784.10.1111/j.1151-2916.1998.tb02696.x ↗
34. F.T. Wallenberger, R. Naslain, J.B. Macchesney, and H.D. Ackler, Advanced Inorganic Fibers: Processes, Structures, Properties, Applications, 2000, p 351.10.1007/978-1-4419-8722-8 ↗