Comparative Study of Induction Quenching and Laser Surface Texturing on Anti-wear Performance of 40Cr Steel

Hui Li, Hong Zhou, Deping Zhang, Peng Zhang, Ti Zhou, Wei Su

Publisher page

Abstract

Wear is the main cause of the eventual failure for machinery products composed of 40Cr steel during severe working environment. Induction quenching (IQ) is extensively used to improve the anti-wear performance of 40Cr steel. Nevertheless, the IQ technique has significant drawbacks related to easy deformation and more power consumption. To enhance the performance of 40Cr steel during wear, the laser processing technique was implemented to manufacture various surface texturing shapes (gridding and striation patterns). First, the distinct microstructure, phase components, and microhardness of surface texturing sample were observed and compared with those of IQ and untreated samples. Then, the anti-wear performance of 40Cr steel was experimentally evaluated. The results indicate that surface texturing is beneficial in improving the anti-wear performance of 40Cr steel. The anti-wear performance of surface texturing specimen with gridding pattern was the best, resulting in significant improvement of 73.83% than the untreated sample; the surface texturing sample with striation pattern had the second-best anti-wear performance, improvement of 70.22%, and the IQ sample had the third-best anti-wear performance, improvement of 62.47%.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Tribology and Lubrication Engineering · Metal Alloys Wear and Properties · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. C.Y. Wang, X.D. Li, Y. Chang, S. Han and H. Dong, Comparison of Three Body Impact Abrasive Anti-Wear Performances for Quenching–Partitioning Tempering and Quenching–Tempering 20Si2Ni3 Steels, Wear, 2016, 362–363, p 121–128.10.1016/j.wear.2016.05.026 ↗
2. M. Shah and S.D. Bakshi, Three-Body Abrasive Wear of Carbide-Free Bainite, Martensite and Bainite-Martensite Structure of Similar Hardness, Wear, 2018, 402–403, p 207–215.10.1016/j.wear.2018.02.020 ↗
3. R. Thornton, T. Slatter, A.H. Jones and R. Lewis, Effects of Cryogenic Processing on the Anti-Wear Performance of Grey Cast Iron Brake Discs, Wear, 2011, 271, p 2386–2395.10.1016/j.wear.2010.12.014 ↗
4. S.T. Ahn, D.S. Kim and W.J. Nam, Microstructural Evolution and Mechanical Properties of Low Alloy Steel Tempered by Induction Heating, J. Mater. Process. Technol., 2005, 160, p 54–58.10.1016/j.jmatprotec.2004.03.019 ↗
5. M.H. Kim, K.Y. Rhee, Y.N. Paik, J.S. Hong and Y.S. Ham, Experimental Investigation on the Mechanical Behavior of High-Frequency Induction-Hardened Mild Carbon, SPS5 Steel, Mater. Sci. Eng. A, 2008, 485, p 31–38.10.1016/j.msea.2007.07.088 ↗
6. J.L. Cunningham, D.J. Medlin and G. Krauss, Effects of Induction Hardening and Prior Cold Work on a Micro-alloyed Medium Carbon Steel, J. Mater. Eng. Perform., 1999, 8, p 401–408.10.1361/105994999770346684 ↗
7. C.R.F. Azevedo and J. Belotti Neto, Failure Analysis of Forged and Induction Hardened Steel Cold Work Rolls, Eng. Fail. Anal., 2004, 11, p 951–966.10.1016/j.engfailanal.2003.11.005 ↗
8. H. Kristoffersen and P. Vomacka, Influence of Process Parameters for Induction Hardening on Residual Stresses, Mater. Des., 2001, 22, p 637–644.10.1016/S0261-3069(01)00033-4 ↗
9. W.B. Kim and S.J. Na, A Study on Residual Stresses in Surface Hardening by High Frequency Induction Heating, Surf. Coat. Techol., 1992, 52, p 281–288.10.1016/0257-8972(92)90027-8 ↗
10. E. Abbasi, Q.S. Luo and D. Owens, A Comparison of Microstructure and Mechanical Properties of Low-Alloy Medium-Carbon Steels After Quench-Hardening, Mater. Sci. Eng. A, 2018, 725, p 65–75.10.1016/j.msea.2018.04.012 ↗
11. H. Sert, A. Can, H. Arikan, B. Selcuk and H. Toprak, Anti-Wear Performance of Different Surface Treated Cam Spindles, Wear, 2006, 260, p 1013–1019.10.1016/j.wear.2005.06.012 ↗
12. N.Y. Sari and M. Yilmaz, Investigation of Abrasive + erosive Anti-wear Performance of Surface Hardening Methods Applied to AISI 1050 steel, Mater. Design, 2006, 27, p 470–478.10.1016/j.matdes.2004.11.020 ↗
13. S. Skvarenina and Y. Shin, Predictive Modeling and Experimental Results for Laser Hardening of AISI 1536 Steel with Complex Geometric Features by a High Power Diode Laser, Surf. Coat. Technol., 2006, 201(6), p 2256–2269.10.1016/j.surfcoat.2006.03.039 ↗
14. A. Yánez, J. Álvarez, A. López, G. Nicolás, J. Pérez, A. Ramil and E. Saavedra, Modelling of Temperature Evolution on Metals During Laser Hardening Process, Appl. Surf. Sci., 2002, 186(1–4), p 611–616.10.1016/S0169-4332(01)00696-1 ↗
15. E. Liverani, A.H.A. Lutey, A. Ascari, A. Fortunato and L. Tomesani, A Complete Residual Stress Model for Laser Surface Hardening of Complex Medium Carbon Steel Components, Surf. Coat. Technol., 2016, 302, p 100–106.10.1016/j.surfcoat.2016.05.066 ↗
16. W.S. Yang, H. Zhou, L. Sun, C.W. Wang and Z.K. Chen, Effect of Biomimetic Coupling Units’ Morphologies on Rolling Contact Fatigue Anti-Wear Performance of Steel from Machine Tool Rolling Tracks, Opt. Laser Technol., 2014, 57, p 175–180.10.1016/j.optlastec.2013.10.013 ↗
17. C.L. Zang, T. Zhou, H. Zhou, Y.H. Yuan, P. Zhang, C. Meng and Z.H. Zhang, Effects of Substrate Microstructure on Biomimetic Unit Properties and Anti-Wear Performance of H13 Steel Processed by Laser Remelting, Opt. Laser Technol., 2018, 106, p 299–310.10.1016/j.optlastec.2018.04.022 ↗
18. R. Cui, Y.H. Cheng, X.L. Meng, S.Z. Feng and Z.T. Han, Microstructure and Properties of Heat Treated 1Cr17Ni4MoB Steel Fabricated by Laser Melting Deposition, Opt. Laser Technol., 2018, 108, p 59–68.10.1016/j.optlastec.2018.06.045 ↗
19. X.W. Qiu, Effect of Incident Angle on Laser Transformation Hardening Layer Microstructure and Properties, Adv. Mater. Res., 2011, 148–149, p 606–610.10.4028/www.scientific.net/AMR.194-196.606 ↗
20. A.Q. Wu, Q.B. Liu and S.J. Qin, Influence of Yttrium on Laser Surface Alloying Organization of 40Cr Steel, J. Rare Earths, 2011, 29, p 1004.10.1016/S1002-0721(10)60586-8 ↗
21. F.X. Fu, Y.L. Zhang, G.R. Chang and J. Dai, Analysis on the Physical Mechanism of Laser Cladding Crack and Its Influence Factors, Optik, 2016, 127, p 200–202.10.1016/j.ijleo.2015.10.043 ↗
22. D.A. Starostin, V.P. Biryukov, D.V. Klevetov and V.F. Yudkin, Effect of Laser Hardening Modes on the Hardening Zone Geometric Parameters and Tribological Properties of 40Cr Steel, IOP Conf. Series: Mater. Sci. Eng., 2019, 489, p 012032.10.1088/1757-899X/489/1/012032 ↗
23. X.H. Zhao, H.C. Zhang and Y. Liu, Effect of Laser Surface Remelting on the Fatigue Crack Propagation Rate of 40Cr Steel, Results in Physics., 2019, 12, p 424–431.10.1016/j.rinp.2018.11.097 ↗
24. Y.Q. Xing, J.X. Deng, X.S. Wang and R. Meng, Effect of Laser Surface Textures Combined with Multi-solid Lubricant Coatings on the Tribological Properties of Al2O3/TiC Ceramic, Wear, 2015, 342–343, p 1–12.10.1016/j.wear.2015.08.002 ↗
25. W. Su, T. Zhou, Q. Sui, P. Zhang, H. Zhou, H. Li and Z.H. Zhang, Study on the Relationship between Intervals Among Laser Stripes and the Abrasion Resistance of Biomimetic Laser Textured Surfaces, Opt. Laser Technol., 2018, 104, p 216–224.10.1016/j.optlastec.2018.02.025 ↗
26. I. Etsion, State of the Art in Laser Surface Texturing, J. Tribol., 2005, 127, p 248–253.10.1115/1.1828070 ↗
27. V.G. Efremenko, K. Shimizu, T. Noguchi, A.V. Efremenko and Y.G. Chabak, Impact–Abrasive–Corrosion Wear of Fe-Based Alloys: Influence of Microstructure and Chemical Composition Upon Anti-Wear Performance, Wear, 2013, 305, p 155–165.10.1016/j.wear.2013.06.006 ↗
28. H. Li, H. Zhou, P. Zhang, T. Zhou, W. Su, S.Y. Wang and H.F. Zhang, Influence of Laser Energy Density on Acquisition and Wear Rresistance of Surface Semisolid Unit of 40Cr Steel, J. Mater. Eng. Perform., 2020, 29, p 2283–2295.10.1007/s11665-020-04735-8 ↗