Abstract

In this work, a post treatment of laser surface melting (LSM) has been employed on Stellite 6 and 10 wt.% Mo-alloyed Stellite 6 hardfacings deposited by plasma transferred arc (PTA) process. LSM process refined the microstructures of both hardfacings, while favoring a network-like complex carbide dominated microstructure in the Mo-alloyed version. With reference to the PTA Stellite 6 hardfacing, LSM process led to an increment in surface hardness albeit a subsequent reduction of wear loss at room temperature, where abrasive wear mechanism was dominant. At 500 °C, oxidative wear contributed to the progress of wear by favoring CoO and Co3O4 type tribo-oxides on the contact surfaces of the PTA and LSM’ed hardfacings, respectively. However, Co3O4 type tribo-oxides exhibited poor mechanical stability, than CoO, which led to easier removal from the contact surface and aggravated the wear loss by abrasive wear mechanism. In this respect, LSM’ed hardfacings exhibited higher wear loss than PTA Stellite 6 hardfacing at 500 °C, unlike room temperature.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High Entropy Alloys Studies · Metal and Thin Film Mechanics · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. M. Riddihough, Stellite as a Wear-Resistant Material, Tribology, 1970, 4(3), p 211–215. https://doi.org/10.1016/0041-2678(70)90058-810.1016/0041-2678(70)90058-8 ↗
2. R. Davis, ASM Specialty Handbook: Nickel, Cobalt, and Their Alloys, ASM International, Materials Park, 2000, https://doi.org/10.1007/s11665-018-3796-610.1007/s11665-018-3796-6 ↗
3. B. Venkatesh, K. Sriker, and V.S.V. Prabhakar, Wear Characteristics of Hardfacing Alloys: State-of-the-Art, Procedia Mater. Sci., 2015, 10, p 527–532. https://doi.org/10.1016/j.mspro.2015.06.00210.1016/j.mspro.2015.06.002 ↗
4. M. Shahanur Hasan, M. Abdul Mazid, and R.E. Clegg, The Basics of Stellites in Machining Perspective, Int. J. Eng. Mater. Manuf., 2016, 1(2), p 35–50. https://doi.org/10.26776/ijemm.01.02.2016.0110.26776/ijemm.01.02.2016.01 ↗
5. D. Ahn, Hardfacing Technologies for Improvement of Wear Characteristics of Hot Working Tools: A Review, Int. J. Precis. Eng. Manuf., 2013, 14(7), p 1271–1283. https://doi.org/10.1007/s12541-013-0174-z10.1007/s12541-013-0174-z ↗
6. A. Motallebzadeh, E. Atar, and H. Cimenoglu, Microstructure and Tribological Properties of PTA Deposited Stellite 12 Coating on Steel Substrate, Manuf. Sci. Technol., 2015, 3(5), p 224–228. https://doi.org/10.13189/mst.2015.03050510.13189/mst.2015.030505 ↗
7. L. Wang and D.Y. Li, Effects of Yttrium on Microstructure, Mechanical Properties and High-Temperature Wear Behavior of Cast Stellite 6 Alloy, Wear, 2003, 255(1), p 535–544. https://doi.org/10.1016/S0043-1648(03)00057-710.1016/S0043-1648(03)00057-7 ↗
8. J. Shin, J. Doh, J. Yoon, D. Lee, and J. Kim, Effect of Molybdenum on the Microstructure and Wear Resistance of Cobalt-Base Stellite Hardfacing Alloys, Surf. Coat. Technol., 2003, 166(2–3), p 117–126. https://doi.org/10.1016/S0257-8972(02)00853-810.1016/S0257-8972(02)00853-8 ↗
9. I. Radu and D.Y. Li, The WEAR Performance of Yttrium-Modified Stellite 712 at Elevated Temperatures, Tribol. Int., 2007, 40(2), p 254–265. https://doi.org/10.1016/j.triboint.2005.09.02710.1016/j.triboint.2005.09.027 ↗
10. P. Huang, R. Liu, X. Wu, and M.X. Yao, Effects of Molybdenum Content and Heat Treatment on Mechanical and Tribological Properties of a Low-Carbon Stellite® Alloy, J. Eng. Mater. Technol., 2007, 129(4), p 523–529. https://doi.org/10.1115/1.274442910.1115/1.2744429 ↗
11. R. Liu, J.H. Yao, Q.L. Zhang, M.X. Yao, and R. Collier, Sliding Wear and Solid-Particle Erosion Resistance of a Novel High-Tungsten Stellite Alloy, Wear, 2015, 322–323, p 41–50. https://doi.org/10.1016/j.wear.2014.10.01210.1016/j.wear.2014.10.012 ↗
12. Y. Wu, Y. Liu, H. Chen, Y. Chen, H. Li, and X. Cao, Developing the Ductility and Thermal Fatigue Cracking Property of Laser-Deposited Stellite 6 Coatings by Adding Titanium and Nickel, Mater. Des., 2019, 162, p 271–284. https://doi.org/10.1016/j.matdes.2018.11.06310.1016/j.matdes.2018.11.063 ↗
13. H. Ningkang, W. Yi, Z.X. Zhong, and W.X. Pu, Electron Beam Treatment of Detonation-Sprayed Stellite Coatings, Surf. Coat. Technol., 1991, 46(3), p 255–263. https://doi.org/10.1016/0257-8972(91)90168-V10.1016/0257-8972(91)90168-V ↗
14. C. Ciubotariu, D. Frunzăverde, G. Mărginean, V. Serban, and A. Bîrdeanu, Optimization of the Laser Remelting Process for HVOF-Sprayed Stellite 6 Wear Resistant Coatings, Opt. Laser Technol., 2016, 77, p 98–103. https://doi.org/10.1016/j.optlastec.2015.09.00510.1016/j.optlastec.2015.09.005 ↗
15. R. Shoja-Razavi, Laser Surface Treatment of Stellite 6 Coating Deposited by HVOF on 316L Alloy, J. Mater. Eng. Perform., 2019, 25, p 2583–2595. https://doi.org/10.1007/s11665-016-2138-910.1007/s11665-016-2138-9 ↗
16. Š. Houdková, Z. Pala, E. Smazalová, M. Vostřák, and Z. Česánek, Microstructure and Sliding Wear Properties of HVOF sprayed, Laser Remelted and Laser Clad Stellite 6 Coatings, Surf. Coat. Technol., 2017, 318, p 129–141. https://doi.org/10.1016/j.surfcoat.2016.09.01210.1016/j.surfcoat.2016.09.012 ↗
17. A.A.M. Alhattab, S.A.A. Dilawary, A. Motallebzadeh, C.F. Arisoy, and H. Cimenoglu, Effect of Electron Beam Surface Melting on the Microstructure and Wear Behaviour of Stellite 12 Hardfacing, Ind. Lubr. Tribol., 2019, 71(5), p 636–641. https://doi.org/10.1108/ILT-05-2018-018210.1108/ILT-05-2018-0182 ↗
18. A.A.M. Alhattab, S.A.A. Dilawary, M. Altay, A. Motallebzadeh, C.F. Arisoy, and H. Cimenoglu, Effect of Electron Beam Surface Melting on the Structure and Wear Characteristics of Cobalt-Based Hardfacing and Its Mo-Alloyed Version, Tribol. Trans., 2019, 62(5), p 907–918. https://doi.org/10.1080/10402004.2019.164032810.1080/10402004.2019.1640328 ↗
19. M. Galati and L. Iuliano, A Literature Review of Powder-Based Electron Beam Melting Focusing on Numerical Simulations, Addit. Manuf., 2018, 19, p 1–20. https://doi.org/10.1016/j.addma.2017.11.00110.1016/j.addma.2017.11.001 ↗
20. A. Motallebzadeh, E. Atar, and H. Cimenoglu, Sliding Wear Characteristics of Molybdenum Containing Stellite 12 Coating at Elevated Temperatures, Tribiol. Int., 2015, 91, p 40–47. https://doi.org/10.1016/j.triboint.2015.06.00610.1016/j.triboint.2015.06.006 ↗
21. S.A.A. Dilawary, A. Motallebzadeh, H. Paksoy, M. Afzal, E. Atar, and H. Cimenoglu, Influence of Laser Surface Melting on the Characteristics of Stellite 12 Plasma Transferred Arc Hardfacing Deposit, Surf. Coat. Technol., 2017, 317, p 110–116. https://doi.org/10.1016/j.surfcoat.2017.03.05110.1016/j.surfcoat.2017.03.051 ↗
22. S.A.A. Dilawary, A. Motallebzadeh, R. Akhter, E. Atar, and H. Cimenoglu, Enhanced Wear Resistance of Stellite 12 by Mo Addition and LSM, Surf. Eng., 2017, 34(8), p 1–8. https://doi.org/10.1080/02670844.2017.139316410.1080/02670844.2017.1393164 ↗
23. S.A.A. Dilawary, A. Motallebzadeh, M. Afzal, E. Atar, and H. Cimenoglu, Laser Surface Melting of 10 wt% Mo Alloyed Hardfacing Stellite 12 Plasma Transferred Arc Deposits: Structural Evolution and High Temperature Wear Performance, Opt. Laser Technol., 2018, 101, p 404–412. https://doi.org/10.1016/j.optlastec.2017.11.03810.1016/j.optlastec.2017.11.038 ↗
24. B.A. Van Brussel and J. De Hosson, Residual Stresses in the Surface Layer of Laser-Treated Steels, Mater. Sci. Eng., 1993, 161(1), p 83–89. https://doi.org/10.1016/0921-5093(93)90478-W10.1016/0921-5093(93)90478-W ↗
25. B.J. Abdul Aleem, M.S.J. Hashmi, and B.S. Yilbas, Laser Controlled Melting of Pre-prepared Inconel 718 Alloy Surface, Opt. Lasers Eng., 2011, 49(11), p 1314–1319. https://doi.org/10.1016/j.optlaseng.2011.06.00210.1016/j.optlaseng.2011.06.002 ↗
26. L. Aucott, D. Huang, H.B. Dong, S.W. Wen, J.A. Marsden, A. Rack, and A.C.F. Cocks, Initiation and Growth Kinetics of Solidification Cracking During Welding of Steel, Sci. Rep., 2017, 7, p 1–10. https://doi.org/10.1038/srep4025510.1038/srep40255 ↗
27. V. Kuzucu, M. Ceylan, H. Çelik, and I. Aksoy, Microstructure and Phase Analyses of Stellite 6 Plus 6 wt% Mo Alloy, J. Mater. Process. Technol., 1997, 69(1–3), p 257–263. https://doi.org/10.1016/S0924-0136(97)00027-710.1016/S0924-0136(97)00027-7 ↗
28. U. Malayoglu and A. Neville, Mo and W as Alloying Elements in Co-Based Alloys: Their Effects on Erosion-Corrosion Resistance, Wear, 2005, 259(1–6), p 219–229. https://doi.org/10.1016/j.wear.2005.02.03810.1016/j.wear.2005.02.038 ↗
29. K. Prasad Rao, R. Damodaram, H. Khalid Rafi, G.D. Janaki Ram, G. Madhusudhan Reddy, and R. Nagalakshmi, Friction Surfaced Stellite 6 Coatings, Mater. Charact., 2012, 70, p 111–116. https://doi.org/10.1016/j.matchar.2012.05.00810.1016/j.matchar.2012.05.008 ↗
30. X.P. Tan, P. Wang, Y. Kok, W.Q. Toh, Z. Sun, S.M.L. Nai, M. Descoins, D. Mangelinck, E. Liu, and S.B. Tor, Carbide Precipitation Characteristics in Additive Manufacturing of Co-Cr-Mo Alloy via Selective Election Beam Melting, Scr. Mater., 2018, 143, p 117–121. https://doi.org/10.1016/j.scriptamat.2017.09.02210.1016/j.scriptamat.2017.09.022 ↗
31. I. Hutchings and P. Shipway, Tribology: Friction and Wear of Engineering Materials, 2nd ed., Butterworth-Heinemann, Oxford, 2017
32. C.S. Ramachandran, V. Balasubramanian, and R. Varahamoorthy, Comparative Evaluation of the Abrasive Slurry Wear Behavior of Alloy Surfaces Produced by a Plasma Transferred Arc Hardfacing Process, Met. Mater. Int., 2010, 16(2), p 235–246. https://doi.org/10.1007/s12540-010-0412-110.1007/s12540-010-0412-1 ↗
33. M.S. Sawant and N.K. Jain, Investigations on Wear Characteristics of Stellite Coating by Micro-plasma Transferred Arc Powder Deposition Process, Wear, 2017, 378–379, p 155–164. https://doi.org/10.1016/j.wear.2017.02.04110.1016/j.wear.2017.02.041 ↗
34. J. George, H. Smudde, and P.C. Stair, The Oxidation of Mo (100) Studied by XPS and Surface Raman Spectroscopy: The Onset of MoO2 Formation and the Formation of Surface polymolybdate, Surf. Sci., 1994, 317(1–2), p 65–72. https://doi.org/10.1016/0039-6028(94)90253-410.1016/0039-6028(94)90253-4 ↗
35. M. Dieterle, G. Mestl, J. Jäger, Y. Uchida, H. Hibst, and R. Schlögl, Mixed Molybdenum Oxide Based Partial Oxidation Catalyst 2. Combined X-ray Diffraction, Electron Microscopy and Raman Investigation of the Phase Stability of (MoVW)5O14-Type Oxides, J. Mol. Catal. A Chem., 2001, 174(1–2), p 169–185. https://doi.org/10.1016/S1381-1169(01)00074-710.1016/S1381-1169(01)00074-7 ↗
36. M. Dieterle and G. Mestl, Raman Spectroscopy of Molybdenum Oxides Part II. Resonance Raman Spectroscopic Characterization of the Molybdenum Oxides Mo4O11 and MoO2, Phys. Chem. Chem. Phys., 2002, 4(5), p 822–826. https://doi.org/10.1039/B107046K10.1039/B107046K ↗
37. B. Varghese, Y. Zhang, L. Dai, V.B.C. Tan, C.T. Lim, and C. Sow, Structure-Mechanical Property of Individual Cobalt Oxide Nanowires, Nano Lett., 2008, 8(10), p 3226–3232. https://doi.org/10.1021/nl801555d10.1021/nl801555d ↗
38. J. Robertson and M.I. Manning, Limits to Adherence of Oxide Scales, Mater. Sci. Technol., 1990, 6(1), p 81–92. https://doi.org/10.1179/mst.1990.6.1.8110.1179/mst.1990.6.1.81 ↗
39. P. Alnegren, M. Sattari, J. Froitzheim, and J. Svensson, Degradation of Ferritic Stainless Steels Under Conditions Used for Solid Oxide Fuel Cells and Electrolyzers at Varying Oxygen Pressures, Corros. Sci., 2016, 110, p 200–212. https://doi.org/10.1016/j.corsci.2016.04.03010.1016/j.corsci.2016.04.030 ↗
40. R. Ahmed, A. Ashraf, M. Elameen, N.H. Faisal, A.M. El-Sherik, Y.O. Elakwah, and M.F.A. Goosen, Single Asperity Nanoscratch Behaviour of HIPed and Cast Stellite 6 Alloys, Wear, 2014, 312(1–2), p 70–82. https://doi.org/10.1016/j.wear.2014.02.00610.1016/j.wear.2014.02.006 ↗
41. N. Andrews, L. Giourntas, A.M. Galloway, and A. Pearson, Effect of Impact Angle on the Slurry Erosion-Corrosion of Stellite 6 and SS316, Wear, 2014, 320, p 143–151. https://doi.org/10.1016/j.wear.2014.08.00610.1016/j.wear.2014.08.006 ↗
42. R. Liu, X.J. Wu, S. Kapoor, M.X. Yao, and R. Collier, Effects of Temperature on the Hardness and Wear Resistance of High-Tungsten Stellite Alloys, Metall. Mater. Trans. A, 2015, 46, p 587–599. https://doi.org/10.1007/s11661-014-2664-810.1007/s11661-014-2664-8 ↗
43. G.R. Mirshekari, S. Daee, S. Fatoureh Bonabi, M.R. Tavakoli, A. Shafyei, and M. Safaei, Effect of Interlayers on the Microstructure and Wear Resistance of Stellite 6 Coatings Deposited on AISI, 420 Stainless Steel by GTAW Technique, Surf. Interface, 2017, 9, p 79–92. https://doi.org/10.1016/j.surfin.2017.08.00510.1016/j.surfin.2017.08.005 ↗
44. A. Gholipour, M. Shamanian, and F. Ashrafizadeh, Microstructure and Wear Behavior of Stellite 6 Cladding on 17-4 PH Stainless Steel, J. Alloys Compd., 2011, 509(14), p 4905–4909. https://doi.org/10.1016/j.jallcom.2010.09.21610.1016/j.jallcom.2010.09.216 ↗
45. S.F. Gnyusov, A.A. Ignatov, V.G. Durakov, and SYu Tarasov, The Effect of Thermal Cycling by Electron-Beam Surfacing on Structure and Wear Resistance of Deposited M2 Steel, Appl. Surf. Sci., 2012, 263, p 215–222. https://doi.org/10.1016/j.apsusc.2012.09.03010.1016/j.apsusc.2012.09.030 ↗
46. L. Venkatesh, S.B. Pitchuka, G. Sivakumar, R.C. Gundakaram, S.V. Joshi, and I. Samajdar, Microstructural Response of Various Chromium Carbide Based Coatings to Erosion and Nano Impact Testing, Wear, 2017, 386–387, p 72–79. https://doi.org/10.1016/j.wear.2017.06.00210.1016/j.wear.2017.06.002 ↗
47. C. Hao and P. Chun-xu, Microstructure and Fractural Morphology of Cobalt-based Alloy Laser Cladding*, J. Wuhan Univ. Technol., 2003, 18(3), p 30–32. https://doi.org/10.1007/BF0283845210.1007/BF02838452 ↗
48. D.R. Askeland, P.P. Fulay, and W.J. Wright, The Science and Engineering of Materials, 6th ed., Cengage Learning Inc., Boston, 2010
49. M.X. Yao, J.B.C. Wu, and Y. Xie, Wear, Corrosion and Cracking Resistance of Some W- or Mo-Containing Stellite Hardfacing Alloys, Mater. Sci. Eng., 2005, 407(1–2), p 234–244. https://doi.org/10.1016/j.msea.2005.06.06210.1016/j.msea.2005.06.062 ↗
50. Y. Ding, R. Liu, J. Yao, Q. Zhang, and L. Wang, Stellite Alloy Mixture Hardfacing via Laser Cladding for Control Valve Seat Sealing Surfaces, Surf. Coat. Technol., 2017, 329, p 97–108. https://doi.org/10.1016/j.surfcoat.2017.09.01810.1016/j.surfcoat.2017.09.018 ↗
51. J. Castaing, M. Spendel, J. Philibert, A. Dominguez Rodriguez, and R. Marquez, Plastic Deformation of CoO Single Crystals, Revue Phys. Appl., 1980, 15(2), p 277–283. https://doi.org/10.1051/rphysap:0198000150202770010.1051/rphysap:01980001502027700 ↗
52. J. Kim, D. Kim, S. Suwas, E. Fleury, and K. Yi, Grain-Size Effects on the High-Temperature Oxidation of Modified 304 Austenitic Stainless Steel, Oxid. Met., 2013, 79(3–4), p 239–247. https://doi.org/10.1007/s11085-012-9347-x10.1007/s11085-012-9347-x ↗
53. M.W. Edwards and N.S. McIntyre, Gas Phase Initial Oxidation of Incoloy 800 Surfaces, Oxid. Met., 2013, 79, p 179–200. https://doi.org/10.1007/s11085-012-9316-410.1007/s11085-012-9316-4 ↗
54. S. Kapoor, R. Liu, X.J. Wu, and M.X. Yau, Temperature-Dependence of Hardness and Wear Resistance of Stellite Alloys, Int. J. Mater. Metall. Eng., 2012, 6(7), p 592–601. https://doi.org/10.5281/zenodo.106087210.5281/zenodo.1060872 ↗