Surface properties of metallic material significantly affect its fatigue, tribological and other functional properties. Titanium (Ti) alloys are hard to machine material, and therefore, wire electrical discharge machining (WEDM) is preferred over the conventional turning and milling process for machining of Ti-alloys. In the present work, surface integrity and wear behavior of Ti-6Al-7Nb have been evaluated under rough cut and trim cut modes of WEDM process. Rough cut mode resulted in high thermal damage with high surface roughness (Ra 2.34 μm), thick recast layer (Avg. 13.71 μm) and high crack density with large size micro-cracks. Significant improvement in surface properties of Ti-6Al-7Nb has obtained using trim cut mode with reduced surface roughness (0.94 μm), thin recast layer (3.51 μm), and the average crack length and average crack density reduced by 30% approximately. Energy-dispersive spectroscopy analysis showed that the trim cut mode yielded a high percentage of Ti and O elements in machined surface layers and reduced the contents of Al, Cu and C, thus favors the improved biocompatibility of Ti-alloy. Rough cut and trim cut modes of WEDM played the significant role in enhancing the surface hardness of Ti-6Al-7Nb, thus affected the coefficient of friction (c.o.f.) and wear rate. Trim cut mode resulted in lowest c.o.f. and wear rate as compared to rough cut machining and polishing. The results of the present work are highly motivated to promote the trim cut mode of WEDM as a promising manufacturing route for Ti-alloy.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Machining and Optimization Techniques · Advanced machining processes and optimization · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Y. Xu, E. Liu, and S. Wei, Investigation on Tensile Fracture Properties of TA15 Specimen Formed by Selective Electron Beam Melting, Mater. Sci. Eng. A, 2020, 773, p 13882610.1016/j.msea.2019.138826 ↗
2. P.S. Nnamchi, C.S. Obayi, I. Todd, and M.W. Rainforth, Mechanical and Electrochemical Characterisation of New Ti-Mo-Nb-Zr Alloys for Biomedical Applications, J. Mech. Behav. Biomed. Mater., 2016, 60, p 68–7710.1016/j.jmbbm.2015.12.023 ↗
3. D. Arulkirubakaran, V. Senthilkumar, and V. Kumawat, Effect of Micro-Textured Tools on Machining of Ti–6Al–4V Alloy: An Experimental and Numerical Approach, Int. J. Refract. Met. Hard Mater., 2016, 54, p 165–17710.1016/j.ijrmhm.2015.07.027 ↗
4. Z. Li, J. Tang, and J. Bai, A Novel Micro-EDM Method to Improve Microhole Machining Performances Using Ultrasonic Circular Vibration (UCV) Electrode, Int. J. Mech. Sci., 2020, 175, p 10557410.1016/j.ijmecsci.2020.105574 ↗
5. Y. Arima and H. Iwata, Effect of Wettability and Surface Functional Groups on Protein Adsorption and Cell Adhesion Using Well-Defined Mixed Self-Assembled Monolayers, Biomaterials, 2007, 28(20), p 3074–308210.1016/j.biomaterials.2007.03.013 ↗
6. A. Kumar, V. Kumar, and J. Kumar, Experimental Investigation on Material Transfer Mechanism in WEDM of Pure Titanium (Grade-2), Adv. Mater. Sci. Eng., 2013, 2013, p 1–2010.1155/2013/847876 ↗
7. C. Prakash, H.K. Kansal, B.S. Pabla, and S. Puri, Powder Mixed Electric Discharge Machining: An Innovative Surface Modification Technique to Enhance Fatigue Performance and Bioactivity of β -Ti Implant for Orthopedics Application, J. Comput. Inf. Sci. Eng., 2016, 16(4), p 04100610.1115/1.4033901 ↗
8. A. Li, J. Pang, J. Zhao, J. Zang, and F. Wang, FEM-Simulation of Machining Induced Surface Plastic Deformation and Microstructural Texture Evolution of Ti-6Al-4V Alloy, Int. J. Mech. Sci., 2017, 123, p 214–22310.1016/j.ijmecsci.2017.02.014 ↗
9. T. Renkawitz and S. Dendorfer, Orthopedic Navigation Technology and Biomechanical Evaluation for Total Hip Replacement, Proc. Inst. Mech. Eng. H, 2012, 226(12), p 897–89810.1177/0954411912458746 ↗
10. S.L. Soo, M.T. Antar, D.K. Aspinwall, C. Sage, M. Cuttell, R. Perez, and A.J. Winn, The Effect of Wire Electrical Discharge Machining on the Fatigue Life of Ti-6Al-2Sn-4Zr-6Mo Aerospace Alloy, Proc. CIRP, 2013, 6, p 215–21910.1016/j.procir.2013.03.043 ↗
11. S. Jithin, A. Raut, U.V. Bhandarkar, and S.S. Joshi, Finite Element Model for Topography Prediction of Electrical Discharge Textured Surfaces Considering Multi-Discharge Phenomenon, Int. J. Mech. Sci., 2020, 177, p 10560410.1016/j.ijmecsci.2020.105604 ↗
12. V. Kumar, V. Kumar, and K.K. Jangra, An Experimental Analysis and Optimization of Machining Rate and Surface Characteristics in WEDM of Monel-400 Using RSM and Desirability Approach, J. Ind. Eng. Int., 2015, 11(3), p 297–30710.1007/s40092-015-0103-0 ↗
13. S.S. Rahman, MdZI, Ashraf, M.S. Bashar, M. Kamruzzaman, A.K.M. Nurul Amin, and M.M. Hossain, Crystallinity, Surface Morphology, and Chemical Composition of the Recast Layer and Rutile-TiO2 Formation on Ti-6Al-4V ELI, by Wire-EDM to Enhance Biocompatibility, Int. J. Adv. Manuf. Technol., 2017, 93(9–12), p 3285–329610.1007/s00170-017-0772-5 ↗
14. K.K. Jangra, An Experimental Study for Multi-Pass Cutting Operation in Wire Electrical Discharge Machining of WC-5.3% Co Composite, Int. J. Adv. Manuf. Technol., 2015, 76(5–8), p 971–98210.1007/s00170-014-6218-4 ↗
15. N. Sharma, R. Khanna, Y.K. Sharma, and R.D. Gupta, Multi-quality Characteristics Optimisation on WEDM for Ti-6Al-4V using Taguchi-Grey Relational Theory, Int. J. Mach. Mach. Mater., 2019, 21, p 66–81
16. S.-L. Chen, M.-H. Lin, C.-C. Chen, and K.-L. Ou, Effect of Electro-Discharging on Formation of Biocompatible Layer on Implant Surface, J. Alloys Compd., 2008, 456(1–2), p 413–41810.1016/j.jallcom.2007.02.055 ↗
17. A. Mahajan and S.S. Sidhu, Surface Modification of Metallic Biomaterials for Enhanced Functionality: A Review, Mater. Technol., 2018, 33(2), p 93–10510.1080/10667857.2017.1377971 ↗
18. M. Ramulu, G. Paul, and J. Patel, EDM Surface Effects on the Fatigue Strength of a 15 Vol% SiCp/Al Metal Matrix Composite Material, Compos. Struct., 2001, 54, p 79–8610.1016/S0263-8223(01)00072-1 ↗
19. J.W. Murray, N. Ahmed, T. Yuzawa, T. Nakagawa, S. Sarugaku, D. Saito, and A.T. Clare, Dry-Sliding Wear and Hardness of Thick Electrical Discharge Coatings and Laser Clads, Tribol. Int. 106392 (2020).10.1016/j.triboint.2020.106392 ↗
20. M. Bazrafshan, M.B. de Rooij, and D.J. Schipper, The Effect of Adhesion and Roughness on Friction Hysteresis Loops, Int. J. Mech. Sci., 2019, 155, p 9–1810.1016/j.ijmecsci.2019.02.027 ↗
21. I. Cvijović-Alagić, Z. Cvijović, S. Mitrović, V. Panić, and M. Rakin, Wear and Corrosion Behaviour of Ti-13Nb-13Zr and Ti-6Al-4V Alloys in Simulated Physiological Solution, Corros. Sci., 2011, 53(2), p 796–80810.1016/j.corsci.2010.11.014 ↗
22. J.I. Onate, F. Alonso, and A. Garcıa, Improvement of Tribological Properties by Ion Implantation, p 6 (1998).
23. B. Evgeny, T. Hughes, and D. Eskin, Effect of Surface Roughness on Corrosion Behaviour of Low Carbon Steel in Inhibited 4M Hydrochloric Acid under Laminar and Turbulent Flow Conditions, Corros. Sci., 2016, 103, p 196–20510.1016/j.corsci.2015.11.019 ↗
24. R. Chalisgaonkar and J. Kumar, Multi-response Optimization and Modeling of Trim Cut WEDM Operation of Commercially Pure Titanium (CPTi) Considering Multiple User’s Preferences, Eng. Sci. Technol. Int. J., 2015, 18(2), p 125–134
25. “Sandvik Coromant Catalogues & Handbooks—Download as PDF!,” Sandvik Coromant, n.d., https://www.sandvik.coromant.com:443/en-gb/downloads/pages/default.aspx. Accessed 20 April 2020.
26. S. Das, S. Paul, and B. Doloi, Application of CFD and Vapor Bubble Dynamics for an Efficient Electro-Thermal Simulation of EDM: An Integrated Approach, Int. J. Adv. Manuf. Technol., 2019, 102(5–8), p 1787–180010.1007/s00170-018-3144-x ↗
27. B. Ekmekci, O. Elkoca, and A. Erden, A Comparative Study on the Surface Integrity of Plastic Mold Steel Due to Electric Discharge Machining, Metall. Mater. Trans. B, 2005, 36(1), p 117–12410.1007/s11663-005-0011-6 ↗
28. N. Sharma, G. Singh, M. Gupta, H. Hegab, and M. Mia, Investigations of Surface Integrity, Bio-Activity and Performance Characteristics during Wire-Electrical Discharge Machining of Ti-6Al-7Nb Biomedical Alloy, Mater. Res. Express, 2019, 6(9), p 09656810.1088/2053-1591/ab3094 ↗