journal article·2012-06

Effect of Thermal Oxidation on Corrosion Resistance of Commercially Pure Titanium in Acid Medium

M. Jamesh, Satendra Kumar, T. S. N. Sankara Narayanan

Publisher page

Abstract

This article addresses the characteristics of commercially pure titanium (CP-Ti) subjected to thermal oxidation in air at 650 °C for 48 h and its corrosion behavior in 0.1 and 4 M HCl and HNO3 mediums. Thermal oxidation of CP-Ti leads to the formation of thick oxide scales (~20 μm) throughout its surface without any spallation. The oxide layer consists of rutile- and oxygen-diffused titanium as predominant phases with a hardness of 679 ± 43 HV1.96. Electrochemical studies reveal that the thermally oxidized CP-Ti offers a better corrosion resistance than its untreated counterpart in both HCl and HNO3 mediums. The uniform surface coverage and compactness of the oxide layer provide an effective barrier toward corrosion of CP-Ti. The study concludes that thermal oxidation is an effective approach to engineer the surface of CP-Ti so as to increase its corrosion resistance in HCl and HNO3 mediums.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Metal and Thin Film Mechanics · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. B.D. Craig and D.S. Anderson, Handbook of Corrosion Data, ASM International, Materials Park, OH, 1995
2. A. Robin, J.L. Rosa, and H.R.Z. Sandim, Corrosion Behavior of Ti-4Al-4V Alloy in Nitric, Phosphoric and Sulphuric Acid Solutions at Room Temperature, J. Appl. Electrochem., 2001, 31, p 455–46010.1023/A:1017584120460 ↗
3. D.J. Blackwood and S.K.M. Chooi, Stability of Protective Oxide Films Formed on a Porous Titanium, Corros. Sci., 2002, 44, p 395–40510.1016/S0010-938X(01)00080-4 ↗
4. A.S. Mogoda, Y.H. Ahmad, and W.A. Badawy, Corrosion Behaviour of Ti-6Al-4V Alloy in Concentrated Hydrochloric and Sulphuric Acids, J. Appl. Electrochem., 2004, 34, p 873–87810.1023/B:JACH.0000040447.26482.bd ↗
5. A.S. Mogoda, Y.H. Ahmad, and W.A. Badawy, Corrosion Inhibition of Ti-6Al-4V Alloy in Sulfuric and Hydrochloric Acid Solutions Using Inorganic Passivators, Mater. Corros., 2004, 55, p 449–45610.1002/maco.200303751 ↗
6. M.V. Popa, E. Vasilescu, P. Drob, C. Vasilescu, J. Mirza-Rosca, and A. Santana Lopez, Corrosion Behavior of Some Titanium Base Alloys in Acid Solutions, Mater. Manuf. Process., 2005, 20, p 35–4510.1081/AMP-200041602 ↗
7. J. Vaughan and A. Alfantazi, Corrosion of Titanium and Its Alloys in Sulfuric Acid in the Presence of Chlorides, J. Electrochem. Soc., 2006, 153, p B6–B1210.1149/1.2126580 ↗
8. K. Azumi, M. Nakajima, K. Okamoto, and M. Seo, Dissolution of Ti Wires in Sulphuric Acid and Hydrochloric Acid Solutions, Corros. Sci., 2007, 49, p 469–48010.1016/j.corsci.2006.04.017 ↗
9. R.Sh. Razavi, M. Salehi, M. Ramazani, and H.C. Man, Corrosion Behaviour of Laser Gas Nitrided Ti-6Al-4V in HCl Solution, Corros. Sci., 2009, 51, p 2324–232910.1016/j.corsci.2009.06.016 ↗
10. N.D. Tomashov, R.M. Altovsky, and G.P. Chernova, Passivity and Corrosion Resistance of Titanium and its Alloys, J. Electrochem. Soc., 1961, 108, p 113–11910.1149/1.2428023 ↗
11. N.D. Tomashov, G.P. Chernova, Yu.S. Ruscol, and G.A. Ayuyan, The Passivation of Alloys on Titanium Bases, Electrochim. Acta, 1974, 19, p 159–17210.1016/0013-4686(74)85012-7 ↗
12. S. Piazza, G. Lo Biundo, N.C. Romano, C. Sunseri, and F. di Quatro, In Situ Characterization of Passive Films on Al-Ti Alloy by Photocurrent and Impedance Spectroscopy, Corros. Sci., 1998, 40, p 1087–110810.1016/S0010-938X(98)00009-2 ↗
13. C.M. Chen, F.H. Beck, and M.G. Fontana, Stress Corrosion Cracking of Ti-8Al-1Mo-1V Alloy, Corrosion, 1970, 26, p 135–13910.5006/0010-9312-26.4.135 ↗
14. K. Azumi, S. Watanabe, M. Seo, I. Saecki, Y. Inokuchi, P. James, and W.N. Smyrl, Characterization of Anodic Oxide Film Formed on Tin Coating in Neutral Borate Buffer Solution, Corros. Sci., 1998, 40, p 1363–137710.1016/S0010-938X(98)00031-6 ↗
15. C. Sittig, M. Textor, N.D. Spencer, M. Wieland, and P.H. Vallotton, Surface Characterization of Implant Materials CP-Ti, Ti-6Al-7Nb and Ti-6Al-4V with Different Pretreatments, J. Mater. Sci. Mater. Med., 1999, 10, p 35–4610.1023/A:1008840026907 ↗
16. H.B. Wen, J.G. Wolke, J.R. Wijn, Q. Liu, F.Z. Cui, and K. de Groot, Fast Precipitation of Calcium Phosphate Layers on Titanium Induced by Simple Chemical Treatments, Biomaterials, 1997, 18, p 1471–147810.1016/S0142-9612(97)82297-1 ↗
17. X. Nie, E.I. Meletis, J.C. Jiang, A. Leyland, A.L. Yerokhin, and A. Matthews, Abrasive Wear/Corrosion Properties and TEM Analysis of Al2O3 Coatings Fabricated Using Plasma Electrolysis, Surf. Coat. Technol., 2002, 149, p 245–25110.1016/S0257-8972(01)01453-0 ↗
18. P. Andreazza, M.I. De Barros, C. Andreazza-Vignolle, D. Rats, and L. Vandenbulcke, In-Depth Structural X-ray Investigation of PECVD Grown Diamond Films on Titanium Alloys, Thin Solid Films, 1998, 319, p 62–6610.1016/S0040-6090(97)01086-9 ↗
19. M. Uchida, N. Nihira, A. Mitsuo, K. Toyoda, K. Kubota, and T. Aizawa, Friction and Wear Properties of CrAlN and CrVN Films Deposited by Cathodic Arc Ion Plating Method, Surf. Coat. Technol., 2004, 177–178, p 627–63010.1016/S0257-8972(03)00937-X ↗
20. T. Brendel, A. Engel, and C. Russel, Hydroxyapatite Coatings by a Polymeric Route, J. Mater. Sci. Mater. Med., 1992, 3, p 175–17910.1007/BF00713445 ↗
21. S.W.K. Kweh, K.A. Khor, and P. Cheang, An In Vitro Investigation of Plasma Sprayed Hydroxyapatite (HA) Coatings Produced with Flame-Spheroidized Feedstock, Biomaterials, 2002, 23, p 775–78510.1016/S0142-9612(01)00183-1 ↗
22. T. Hanawa, Y. Kamiura, S. Yamamoto, T. Kohgo, A. Amemiya, H. Ukai et al., Early Bone Formation Around Calcium-Ion-Implanted Titanium Inserted into Rat Tibia, J. Biomed. Mater. Res., 1997, 36, p 131–13610.1002/(SICI)1097-4636(199707)36:1<131::AID-JBM16>3.0.CO;2-L ↗
23. H. Guleryuz and H. Cimenoglu, Effect of Thermal Oxidation on Corrosion and Corrosion-Wear Behaviour of a Ti-6Al-4V Alloy, Biomaterials, 2004, 25, p 3325–333310.1016/j.biomaterials.2003.10.009 ↗
24. M.F. Lopez, J.A. Jimenez, and A. Gutierrez, Corrosion Study of Surface-Modified Vanadium-Free Titanium Alloys, Electrochim. Acta, 2003, 48, p 1395–140110.1016/S0013-4686(03)00006-9 ↗
25. D. Velten, V. Biehl, F. Aubertin, B. Valeske, W. Possart, and J. Breme, Preparation of TiO(2) Layers on CP-Ti and Ti6Al4V by Thermal and Anodic Oxidation and by Sol-Gel Coating Techniques and Their Characterization, J. Biomed. Mater. Res., 2002, 59, p 18–2810.1002/jbm.1212 ↗
26. M.L. Escudero, J.L. Gonzalez-Carrasco, C. Garcia-Alonso, and E. Ramirez, Electrochemical Impedance Spectroscopy of Preoxidized MA 956 Superalloy During In Vitro Experiments, Biomaterials, 1995, 16, p 735–74010.1016/0142-9612(95)99703-O ↗
27. D. Siva Rama Krishna, Y.L. Brama, and Y. Sun, Thick Rutile Layer on Titanium for Tribological Applications, Tribol. Int., 2007, 40, p 329–33410.1016/j.triboint.2005.08.004 ↗
28. A. Bloyce, P.Y. Qi, H. Dong, and T. Bell, Surface Modification of Titanium Alloys for Combined Improvements in Corrosion and Wear Resistance, Surf. Coat. Technol., 1998, 107, p 125–13210.1016/S0257-8972(98)00580-5 ↗
29. S. Kumar, T.S.N. Sankara Narayanan, S. Ganesh Sundara Raman, and S.K. Seshadri, Thermal Oxidation of CP-Ti: Evaluation of Characteristics and Corrosion Resistance as a Function of Treatment Time, Mater. Sci. Eng. C, 2009, 29, p 1942–194910.1016/j.msec.2009.03.007 ↗
30. S. Kumar, T.S.N. Sankara Narayanan, S. Ganesh Sundara Raman, and S.K. Seshadri, Thermal Oxidation of Ti6Al4V Alloy: Microstructural and Electrochemical Characterization, Mater. Chem. Phys., 2010, 119, p 337–34610.1016/j.matchemphys.2009.09.007 ↗
31. S. Kumar, T.S.N. Sankara Narayanan, S. Ganesh Sundara Raman, and S.K. Seshadri, Thermal Oxidation of CP Ti—An Electrochemical and Structural Characterization, Mater. Charact., 2010, 61, p 589–59710.1016/j.matchar.2010.03.002 ↗
32. S. Kumar, T.S.N. Sankara Narayanan, S. Ganesh Sundara Raman, and S.K. Seshadri, Fretting Corrosion Behaviour of Thermally Oxidized CP-Ti in Ringer’s Solution, Corros. Sci., 2010, 52, p 711–72110.1016/j.corsci.2009.10.029 ↗
33. S. Kumar, T.S.N. Sankara Narayanan, S. Ganesh Sundara Raman, and S.K. Seshadri, Surface Modification of CP-Ti to Improve the Fretting Corrosion Resistance: Thermal Oxidation vs. Anodizing, Mater. Sci. Eng. C, 2010, 30, p 921–92710.1016/j.msec.2010.03.024 ↗
34. D.C. Silverman, ‘‘Tutorial on Polexperttm and the Cyclic Potentiodynamic Polarization Technique,” http://www.argentumsolutions.com/tutorials/polexpert_tutorialpg1.html
35. M. Jamesh, S. Kumar, and T.S.N. Sankara Narayanan, Corrosion Behavior of Commercially Pure Mg and ZM21 Mg Alloy in Ringer’s Solution—Long Term Evaluation by EIS, Corros. Sci., 2011, 53, p 645–65410.1016/j.corsci.2010.10.011 ↗
36. L. Peguet, B. Malki, and B. Baroux, Influence of Cold Working on the Pitting Corrosion Resistance of Stainless Steels, Corros. Sci., 2007, 49, p 1933–194810.1016/j.corsci.2006.08.021 ↗
37. F.M. Bayoumi, W.A. Ghanem, and B.G. Ateya, Electrochemical Behavior of Cr-Mo Steel Alloy in High Temperature Aqueous Sodium Chloride Solution, Int. J. Electrochem. Sci., 2006, 1, p 258–26710.1016/S1452-3981(23)17155-0 ↗
38. H. Guleryuz and H. Cimenoglu, Surface Modification of a Ti-6Al-4V Alloy by Thermal Oxidation, Surf. Coat. Technol., 2005, 192, p 164–17010.1016/j.surfcoat.2004.05.018 ↗
39. A.R. Ebrahimi, F. Zarei, and R.A. Khosroshahi, Effect of Thermal Oxidation Process on Fatigue Behavior of Ti-4Al-2V Alloy, Surf. Coat. Technol., 2008, 203, p 199–20310.1016/j.surfcoat.2008.08.038 ↗
40. K. Nakajima, K. Terao, and T. Miata, The Effect of Microstructure on Fatigue Crack Propagation of α + β Titanium Alloys: In-Situ Observation of Short Fatigue Crack Growth, Mater. Sci. Eng. A, 1998, 243, p 176–18110.1016/S0921-5093(97)00797-1 ↗
41. J.A. Hall, Fatigue Crack Initiation in Alpha-Beta Titanium Alloys, Int. J. Fatigue, 1997, 19, p 23–3710.1016/S0142-1123(97)00047-9 ↗
42. C. Leinenbach and D. Eifler, Influence of Oxidation Treatment on Fatigue and Fatigue-Induced Damage of Commercially Pure Titanium, Acta Biomater., 2009, 5, p 2810–281910.1016/j.actbio.2009.03.029 ↗
43. S.Y. Yu, C.W. Brodrick, M.P. Ryan, and J.R. Scully, Effects of Nb and Zr Alloying Additions on the Activation Behavior of Ti in Hydrochloric Acid, J. Electrochem. Soc., 1999, 146, p 4429–443810.1149/1.1392655 ↗
44. M. Pourbaix, Atlas of Electrochemical Equilibria in Aqueous Solutions, Vol 1, Pergamon Press, New York, 1966, p 213
45. E. Mccafferty, Introduction to Corrosion Science, Springer, New York, 2010, p 21210.1007/978-1-4419-0455-3 ↗
46. E. Klar and P.K. Samal, Powder Metallurgy Stainless Steels: Processing, Microstructures, and Properties, ASM International, Materials Park, OH, 2007, p 15510.31399/asm.tb.pmsspmp.9781627083126 ↗
47. D. Marecil, D. Sutiman, A. Cailean, and I. Creţescu, Effect of Vanadium Replacement by Zirconium on the Electrochemical Behavior of Ti6Al4V Alloy in Ringer’s Solution, Environ. Eng. Manage. J., 2008, 7, p 701–70610.30638/eemj.2008.093 ↗
48. I.C. Lavos-Valereto, S. Wolynec, I. Ramires, A.C. Guastaldi, and I. Costa, Electrochemical Impedance Spectroscopy Characterization of Passive Film Formed on Implant Ti-6Al-7Nb Alloy in Hank’s Solution, J. Mater. Sci. Mater. Med., 2004, 15, p 55–5910.1023/B:JMSM.0000010097.86245.74 ↗
49. S.L. Assis, S. Wolynec, and I. Costa, Corrosion Characterization of Titanium Alloys by Electrochemical Techniques, Electrochim. Acta, 2006, 51, p 1815–181910.1016/j.electacta.2005.02.121 ↗
50. A. Cremasco, W.R. Osorio, C.M.A. Freire, A. Garcia, and R. Caram, Electrochemical Corrosion Behavior of a Ti-35Nb Alloy for Medical Prostheses, Electrochim. Acta, 2008, 53, p 4867–487410.1016/j.electacta.2008.02.011 ↗
51. G.S. Firstov, R.G. Vitchev, H. Kumar, B. Blanpain, and J. Van Humbeeck, Surface Oxidation of NiTi Shape Memory Alloy, Biomaterials, 2002, 23, p 4863–487110.1016/S0142-9612(02)00244-2 ↗
52. S. Barisona, S. Cattarina, S. Daolioa, M. Musiania, and A. Tuissib, Characterization of Surface Oxidation of Nickel-Titanium Alloy by Ion-Beam and Electrochemical Techniques, Electrochim. Acta, 2004, 50, p 11–1810.1016/j.electacta.2004.07.007 ↗