Abstract
Two WC-10Co-4Cr coatings were deposited by high-velocity oxygen fuel (HVOF) and high-velocity air fuel (HVAF) spray processes, respectively, and their basic mechanical properties, cavitation and sand slurry erosion resistances were investigated. The results show that the HVAF-sprayed WC-10Co-4Cr coating exhibited a lower degree of decarburization and better properties in terms of hardness, fracture toughness, porosity, cavitation and sand slurry erosion resistances than those of the HVOF-sprayed WC-10Co-4Cr coatings, respectively. Therefore, HVAF-sprayed WC-10Co-4Cr coatings may be better employed for the protection of hydro-turbine component surfaces against cavitation and sand slurry erosion.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Erosion and Abrasive Machining · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. R. Singh, S.K. Tiwari, and S.K. Mishra, Cavitation Erosion in Hydraulic Turbine Components and Mitigation by Coatings: Current Status and Future Needs, J. Mater. Eng. Perform., 2012, 21, p 1539–155110.1007/s11665-011-0051-9 ↗
2. F.T. Cheng, P. Shi, and H.C. Man, Correlation of Cavitation Erosion Resistance with Indentation-Derived Properties for a NiTi Alloy, Scripta Mater., 2001, 45, p 1083–108910.1016/S1359-6462(01)01143-5 ↗
3. S.K. Singhal and S. Ratnendra, Proceedings of the Himalayan Small Hydropower Summit, Held During October 12-13, Dehradun, 2006, p 200-207
4. B.S. Mann and V. Arya, Abrasive and Erosive Wear Characteristics of Plasma Nitriding and HVOF Coatings: Their Application in Hydro Turbines, Wear, 2001, 249, p 354–36010.1016/S0043-1648(01)00537-3 ↗
5. Q. Wang, J. Xiang, G.Y. Chen, Y.L. Cheng, X.Q. Zhao, and S.Y. Zhang, Propylene Flow, Microstructure and Performance of WC-12Co Coatings Using a Gas-Fuel HVOF Spray Process, J. Mater. Process. Technol., 2013, 213, p 1653–166010.1016/j.jmatprotec.2013.04.007 ↗
6. L. Jacobs, M.M. Hyland, and M.D. Bonte, Study of the Influence of Microstructural Properties on the Sliding-Wear Behavior of HVOF and HVAF Sprayed WC-Cermet Coatings, J. Therm. Spray Technol., 1999, 8, p 125–13210.1361/105996399770350656 ↗
7. A. Verstak and V. Baranovski, in: B.R. Marple, M.M. Hyland, Y.-C. Lan, R.S. Lima, J. Voger (Eds.), AC-HVAF Sprayed Tungsten Carbide: Properties and Applications, Thermal Spray 2006: Building on 100 Years of Success, ASM International, Seattle, A, May 15-18, 2006, (Paper 11827)
8. A. Verstak and V. Baranovski, Deposition of Carbides by Activated Combustion HVAF Spraying, Thermal Spray Solutions: Advances in Technology and Application, May 10-14, 2004 (Osaka, Japan), DVS, German Welding Society, 2004, p 55110.31399/asm.cp.itsc2004p0551 ↗
9. S.L. Liu, X.P. Zheng, and G.Q. Geng, Influence of Nano-WC-12Co Powder Addition in WC-10Co-4Cr AC-HVAF Sprayed Coatings on Wear and Erosion Behavior, Wear, 2010, 269, p 362–36710.1016/j.wear.2010.04.019 ↗
10. S. Matthews, M. Hyland, and B. James, Long-Term Carbide Development in High-Velocity Oxygen Fuel/High-Velocity Air Fuel Cr3C2-NiCr Coatings Heat Treated at 900 °C, J. Therm. Spray Technol., 2004, 13, p 526–53610.1361/10599630421442 ↗
11. Q. Wang, S.Y. Zhang, Y.L. Cheng, J. Xiang, X.Q. Zhao, and G.B. Yang, Wear and Corrosion Performance of WC-10Co-4Cr Coatings Deposited by Different HVOF and HVAF Spraying Processes, Surf. Coat. Technol., 2013, 218, p 127–13610.1016/j.surfcoat.2012.12.041 ↗
12. I. Hulka, V.A. Şerban, I. Secoşan, P. Vuoristo, and K. Niemi, Wear Properties of CrC-37WC-18 M Coatings Deposited by HVOF and HVAF Spraying Processes, Surf. Coat. Technol., 2012, 210, p 15–2010.1016/j.surfcoat.2012.07.077 ↗
13. A.G. Evans and T.R. Wilshaw, Quasi-Static Solid Particle Damage in Brittle Solids—I. Observations Analysis and Implications, Acta Metall., 1976, 24(10), p 939–95610.1016/0001-6160(76)90042-0 ↗
14. O. Eso, Z.Z. Fang, and A. Griffo, Kinetics of Cobalt Gradient Formation During the Liquid Phase Sintering of Functionally Graded WC-Co, Int. J. Refract. Met. Hard Mater., 2007, 25, p 286–29210.1016/j.ijrmhm.2006.07.002 ↗
15. X.B. Zhang, C.S. Liu, X.D. Liu, J. Dong, and B. Yu, Cavitation Erosion Behavior of WC Coatings on CrNiMo Stainless Steel by Laser Alloying, Int. J. Miner. Metall. Mater., 2009, 16, p 203–20710.1016/S1674-4799(09)60034-0 ↗
16. S.K. Wu, H.C. Lin, and C.H. Yeh, A Comparison of the Cavitation Erosion Resistance of TiNi Alloys, SUS304 Stainless Steel and Ni-Based Self-Fluxing Alloy, Wear, 2000, 244, p 85–9310.1016/S0043-1648(00)00443-9 ↗
17. I. Hussainova, J. Kübarsepp, and I. Shcheglov, Investigation of Impact of Solid Particles Against Hard Metal and Cermet Targets, Tribol. Int., 1999, 32, p 337–34410.1016/S0301-679X(99)00073-0 ↗
18. L. Thakur, N. Aroraa, R. Jayaganthan, and R. Soodc, An Investigation on Erosion Behavior of HVOF Sprayed WC-CoCr Coatings, Appl. Surf. Sci., 2011, 258, p 1225–123410.1016/j.apsusc.2011.09.079 ↗
19. G.W. Stachowiak and A.W. Batchelor, Engineering Tribology, Butterworth-Heinemann, Oxford, 2005