Abstract
The microstructure of Ti-Fe polycrystals has been studied between 595 and 815 °C in the concentration interval between 1 and 9 wt.% Fe. In these conditions, two phases, namely hexagonal α(Ti, Fe) and cubic β(Ti, Fe), are in equilibrium. The α(Ti, Fe) phase forms either continuous or discontinuous layers in the β(Ti, Fe)/β(Ti, Fe) grain boundaries (GBs). Continuous layers correspond to the complete wetting of β(Ti, Fe)/β(Ti, Fe) GBs by a second solid phase α(Ti, Fe). Discontinuous layers correspond to the incomplete (or partial) GB wetting by a second solid phase. The temperature dependences of the portion of completely wetted GBs as well as that of the thickness of continuous GB layer of α(Ti, Fe) phase have been measured. Both values monotonously increase with increasing temperature.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. R. Boyer, E.W. Collings, and G. Welsch, Materials Properties Handbook: Titanium Alloys, ASM International, Materials Park, 1994
2. T.B. Massalski, Ed., Binary Alloy Phase Diagrams, 2nd ed., ASM International, Materials Park, 1990
3. O.A. Kaibyshev and F.Z. Utjashev, Superplasticity, Structure Refinement and Processing of Difficult Deformable Alloys, Nauka, Moscow, 2002
4. O.A. Kaibyshev, Superplasticity of Industrial Alloys, Metallurgy, Moscow, 1984
5. M.J. Donachie, Jr., Titanium: A Technical Guide, 2nd ed., ASM International, Materials Park, 200010.31399/asm.tb.ttg2.9781627082693 ↗
6. B.B. Straumal, O.A. Kogtenkova, A.S. Gornakova, V.G. Sursaeva, and B. Baretzky, Review: Grain Boundary Faceting-Roughening Phenomena, J. Mater. Sci., 2016, 51, p 382–40410.1007/s10853-015-9341-1 ↗
7. B.B. Straumal, A.A. Mazilkin, and B. Baretzky, Grain Boundary Complexions and Pseudopartial Wetting, Curr. Opin. Solid State Mater. Sci., 2016, 20, p 247–25610.1016/j.cossms.2016.05.006 ↗
8. G.A. López, E.J. Mittemeijer, and B.B. Straumal, Grain Boundary Wetting by a Solid Phase; Microstructural Development in a Zn-5 wt% Al Alloy, Acta. Mater., 2004, 52, p 4537–454510.1016/j.actamat.2004.06.011 ↗
9. A.S. Gornakova, B.B. Straumal, A.L. Petelin, and A.B. Straumal, Solid-Phase Wetting at Grain Boundaries in the Zr-Nb System, Bull. Russ. Acad. Sci. Phys., 2012, 76, p 102–10510.3103/S106287381201008X ↗
10. O.A. Kogtenkova, B.B. Straumal, S.G. Protasova, A.S. Gornakova, P. Zięba, and T. Czeppe, Effect of the Wetting of Grain Boundaries on the Formation of a Solid Solution in the Al-Zn System, JETP Lett., 2012, 96, p 380–38410.1134/S0021364012180063 ↗
11. B.B. Straumal, A.S. Gornakova, Y.O. Kucheev, B. Baretzky, and A.N. Nekrasov, Grain Boundary Wetting by a Second Solid Phase in the Zr-Nb Alloys, J. Mater. Eng. Perform., 2012, 21, p 721–72410.1007/s11665-012-0158-7 ↗
12. R. Ray, B.C. Giessen, and N.J. Grant, The Constitution of Metastable Titanium-rich Ti-Fe Alloys: An Order-Disorder Transition, Metall. Trans., 1972, 3, p 627–62910.1007/BF02642743 ↗
13. B.W. Levinger, Lattice Parameter of Beta Titanium at Room Temperature, Trans. Am. Inst. Min. Met. Eng., 1953, 197, p 195–200
14. S.G. Fedotov, N.F. Kvasova, and M.I. Ermolova, Decomposition of the Metastable Solid Solution of Titanium with Iron, Dokl. Akad. Nauk SSSR, 1974, 216(2), p 363–366
15. L.N. Guseva and L.K. Dolinskaya, Metastable Phases in Titanium Alloys with Group VIII, Elements Quenched from the β-Region, Izv. Akad. Nauk SSSR Met., 1974, 6, p 195–202
16. A.B. Straumal, B.S. Bokstein, A.L. Petelin, B.B. Straumal, B. Baretzky, A.O. Rodin, and A.N. Nekrasov, Apparently Complete Grain Boundary Wetting in Cu-In Alloys, J. Mater. Sci., 2012, 47, p 8336–834310.1007/s10853-012-6773-8 ↗
17. R.F. Peart, Effect of Pressure on the Diffusion of Fe in Ti and Ti + 10% Fe, Phys. Stat. Sol., 1967, 20, p 545–55010.1002/pssb.19670200214 ↗
18. B.A. Kolachev and V.S. Lyasotskaya, Correlation Between Diagrams of Isothermal and Anisothermal Transformations and Phase Composition Diagram of Hardened Titanium Alloys, Metal Sci. Heat Treat., 2003, 45, p 119–12610.1023/A:1024571622294 ↗
19. Y.B. Egorova, A.A. Il’in, B.A. Kolachev, V.K. Nosov, and A.M. Mamonov, Effect of the Structure on the Cutability of Titanium Alloys, Metal Sci. Heat Treat., 2003, 45, p 134–13910.1023/A:1024527807272 ↗
20. B.A. Kolachev, M.G. Veitsman, and L.N. Gus’kova, Structure and Mechanical Properties of Annealed α + β Titanium Alloys, Metal Sci. Heat Treat., 1983, 25, p 626–63110.1007/BF00741929 ↗
21. A.V. Fishgoit, V.M. Maistrov, and M.A. Rozanov, Interaction of Short Cracks with the Structure of Metals, Sov. Mater. Sci., 1988, 24, p 247–25110.1007/BF00724331 ↗
22. V.N. Bobovnikov, V.V. Luk’yanenko, and A.V. Fishgoit, Effect of Particles of the Insoluble Phase Al9FeNi on the Kinetics of Fatigue Crack Propagation in Alloy AK4-1, Metal Sci. Heat Treat., 1982, 24, p 191–19410.1007/BF01166851 ↗