Role of raw material morphology on microstructures and magnetic properties of bulk SmCo/Fe(Co) nanocomposite magnets

Li Lou, Jingchao Yan, Hongyangsu Zhang, Yingxin Hua, Wenpeng Song, Qian Zhang, Xiaohong Li

Publisher page

Abstract

Abstract The role of the morphology of raw Fe materials on microstructures and magnetic properties of bulk SmCo/Fe(Co) nanocomposite magnets prepared by ball milling combined with annealing and high pressure thermal compression (HPTC) was investigated. We found that the branch-like coarse-grained Fe (BLCG-Fe) promoted SmCo amorphization and reduced grain sizes of the formed Fe(Co) nanocrystals during ball milling process compared with spherical nanocrystalline Fe (SN-Fe). The BLCG-Fe resulted in a three-phased nanocomposite consisting of SmCo7, SmCo3 and Fe(Co) phases and the SN-Fe led to a two-phased magnet composed of SmCo7 and Fe(Co) phases after annealing at 580 °C. And the BLCG-Fe nanocomposite had a smaller Fe(Co) grain size d = 12 nm compared with d = 18 nm for the SN-Fe nanocomposite. For the nanocomposites prepared by HPTC, the BLCG-Fe enhanced obviously the (0 0 2) texture of the SmCo7 phase and improved the magnetic anisotropy compared with the SN-Fe, which resulted in a much higher energy product 25.5 MGOe (203 kJ/m3) than that 15.5 MGOe (123 kJ/m3). The detailed mechanism was discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic Properties of Alloys · Magnetic and transport properties of perovskites and related materials · Magnetic properties of thin films

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Materials science: the pull of stronger magnets10.1038/472022a ↗
2. Applied physics: strong magnets by self-assembly10.1038/420374a ↗
3. Meltspun permanent magnet materials containing Fe3B as the main phase10.1016/0304-8853(89)90333-8 ↗
4. The exchange-spring magnet: a new material principle for permanent magnets10.1109/20.102931 ↗
5. Development of crystal texture in Nd-lean amorphous Nd9Fe85B6 under hot deformation
6. Nanocrystallization and magnetic properties of amorphous Nd9Fe85B6 subjected to high-pressure torsion deformation upon annealing
7. Structure, magnetic properties, and coercivity mechanism of nanocomposite SmCo5/α-Fe magnets prepared by mechanical milling10.1063/1.1365430 ↗
8. Effect of milling time on magnetic properties and structures of bulk Sm-Co/α-(Fe, Co) nanocomposite magnets10.1063/1.3673413 ↗
9. Influence of milled α-Fe powders on structure and magnetic properties of Sm(Co, Zr)7/α-(Fe, Co) nanocomposite magnets made by mechanical alloying10.1063/1.3565997 ↗
10. Morphology and magnetic properties of SmCo3/α-Fe nanocomposite magnets prepared via severe plastic deformation10.1063/1.4862937 ↗
11. Spark plasma sintered Sm2Co17-FeCo nanocomposite permanent magnets synthesized by high energy ball milling10.1088/0957-4484/19/33/335701 ↗
12. Influence of mechanical milling on the physical properties of SmCo5/Fe65Co35 type hard/soft magnetic nanocomposite10.1016/j.jallcom.2013.01.140 ↗
13. Bulk SmCo5/α-Fe nanocomposite permanent magnets fabricated by mould-free Joule-heating compaction10.1063/1.3563098 ↗
14. Structure and magnetic properties of bulk anisotropic SmCo5/α-Fe nanocomposite permanent magnets with different α-Fe content10.1063/1.3564967 ↗
15. Effects of Zr, Nb and Cu substitutions on magnetic properties of melt-spun and hot deformed bulk anisotropic nanocomposite SmCo type magnets10.1063/1.2831334 ↗
16. Structure and magnetic properties of bulk anisotropic SmCo5/α-Fe nanocomposite permanent magnets prepared via a bottom up approach10.1016/j.jallcom.2012.05.079 ↗
17. Fabrication of bulk nanocomposite magnets via severe plastic deformation and warm compaction10.1063/1.3358390 ↗
18. Novel bimorphological anisotropic bulk nanocomposite materials with high energy products10.1002/adma.201606430 ↗
19. Engineering bulk, layered, multicomponent nanostructures with high energy density10.1002/smll.201800619 ↗
20. Controllably manipulating three-dimensional hybrid nanostructures for bulk nanocomposites with large energy products10.1021/acs.nanolett.7b00264 ↗
21. Development of crystallography texture in SmCo7/α-Fe nanocomposite magnets prepared by high-pressure thermal compression10.1016/j.jallcom.2018.03.363 ↗
22. Study of Interface Structure of α-Fe/Nd2Fe14B Nanocomposite Magnets10.1063/1.1456950 ↗
23. Effect of soft phase on magnetic properties of bulk Sm-Co/α-Fe nanocomposite magnets10.1109/TMAG.2013.2246781 ↗
24. Structural and magnetic studies on spark plasma sintered SmCo5/Fe bulk nanocomposite magnets10.1016/j.jmmm.2006.10.057 ↗
25. Self-nanoscaling of the soft magnetic phase in bulk SmCo/Fe nanocomposite magnets10.1007/s10853-011-5568-7 ↗
26. Crystal structure and magnetic properties of ultrafine nanocrystalline SmCo3 compound10.1088/0957-4484/21/11/115708 ↗
27. Mechanical alloying and milling10.1016/S0079-6425(99)00010-9 ↗