Coercivity enhancement and grain refinement in Nd-Fe-B sintered magnets with pyrite doping by jet milling

Fang Yang, Li You, Zhimeng Guo, Vladislay Paley, Alex A. Volinsky

Publisher page

Abstract

Abstract In this paper, the methods to solve the uniformity problem of sulfur (S) element were studied in pyrite-doped Nd-Fe-B sintered magnets. With pyrite addition, the coercivity was enhanced, except for the magnets with pyrite doped by arc melting. Sulphur loss existed during the arc melting process. When pyrite doped by ball milling, the coercivity increased from 1236.3 kA/m to 1327.0 kA/m. The average grain size decreased from 9.10 µm to 7.9 µm. As a drawback, obvious sulfur clusters were formed. Jet milling was an effective way to achieve uniform distribution of S element. In the magnets with pyrite doped by jet milling, clear and continuous grain boundary phases were formed with smaller grain size. Correspondingly, the average grain size further decreased to 6.7 µm. A coercivity enhancement of 13.4% (1401.8 kA/m) was obtained with slightly decreasing in remanence and maximum magnetic energy product.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic Properties of Alloys · Magnetic Properties and Applications · Superconducting Materials and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Strategy for high-coercivity Nd-Fe-B magnets10.1016/j.scriptamat.2012.06.038 ↗
2. Temperature-dependent Dy diffusion processes in Nd-Fe-B permanent magnets10.1016/j.actamat.2014.09.039 ↗
3. Effect of Nd content on the microstructure and coercivity of hot-deformed Nd-Fe-B permanent magnets10.1016/j.actamat.2014.09.021 ↗
4. The effect of nano-TiC addition on sintered Nd-Fe-B permanent magnets10.1016/j.jmmm.2016.12.115 ↗
5. Normal and abnormal grain growth in fine-grained Nd-Fe-B sintered magnets prepared from He jet milled powders10.1016/j.jmmm.2016.10.139 ↗
6. Thermally activated coercivity in core-shell permanent magnets10.1063/1.4916542 ↗
7. Structure and chemical compositions of the grain boundary phase in Nd-Fe-B sintered magnets10.1016/j.actamat.2016.05.035 ↗
8. Effect of post-sinter annealing on the coercivity and microstructure of Nd-Fe-B permanent magnets10.1016/j.actamat.2008.11.019 ↗
9. Understanding the microstructure and coercivity of high performance NdFeB-based magnets10.1016/j.scriptamat.2012.05.038 ↗
10. Grain refinement in heavy rare earth element-free sintered Nd-Fe-B magnets by addition of a small amount of molybdenum10.1063/1.4916496 ↗
11. The role of Nb addition in Nd-Fe-B sintered magnets with high performance10.1016/S0925-8388(01)00900-8 ↗
12. Evidence of domin-wall pining in W-doped (NdDy)(FeCo)B sintered magnets10.1063/1.358146 ↗
13. Effeet of Al, Cu, Ga, and Nb additions on the magnetic properties and microstructural features of sintered NdFeB10.1063/1.1513879 ↗
14. Microstructure and magnetic effects of small Cu additions to (Nd, Dy)FeB magnets10.1016/S1359-6462(96)00312-0 ↗
15. Microstructure of sintered ND-Fe-Ga-B magnets with Mo and MoS2 addition10.1016/j.jmmm.2011.11.049 ↗
16. Effect of WS2/Al co-doping on microstructural and magnetic properties of Nd-Fe-B sintered magnets10.1016/j.jallcom.2016.03.023 ↗
17. Dysprosium-saving improvement of coercivity in Nd-Fe-B sintered magnets by Dy2S3 additions10.1063/1.3574444 ↗
18. Boundary structure modification and magnetic properties of Nd-Fe-B sintered magnets by co-doping with Dy2O3/S powders10.1016/j.jmmm.2017.01.029 ↗
19. Thermodynamics and phase relationships of transition metal-sulfur systems: thermodynamic properties of the Fe-S liquid phase and the calculation of the Fe-S phase diagram10.1007/BF02653979 ↗
20. Multi-phase EBSD mapping and local texture analysis in Nd-Fe-B sintered magnets10.1016/j.actamat.2010.10.033 ↗
21. Dependence of magnetic, phase-transformation and microstructural characteristics on the Cu content of Nd-Fe-B sintered magnets10.1016/j.actamat.2013.11.063 ↗