Assessment of Coating Adhesion
Source abstract
Abstract
The main factor which has hitherto prevented the more widespread use of many coating processes has been poor adhesion. There is a real need for a standard test for adhesion to improve user confidence and avoid failure in service. We discuss the available adhesion test methods and recommend the scratch test as offering the best solution at this time, and a new laser photothermal technique as having good potential.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Surface Roughness and Optical Measurements · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Metals Laboratory, Technical Research Centre of Finland, Espoo, Finland.
Department of Engineering Design and Manufacture, University of Hull.
References (35)
Show source-provided references
1. MATTHEWS A. Surf Eng., 1985, 1, 93.10.1179/sur.1985.1.2.93 ↗
2. 10.1016/0040-6090(85)90322-010.1016/0040-6090(85)90322-0 ↗
3. KUWAHARA K., HIROTA H., and UMEMETO N.: in ‘Adhesion measurement of thin films, thick films and bulk coatings’, STP 640, (ed. Mittal K. L.), 198; 1978, Philadelphia, Pa, ASTM.10.1520/STP38633S ↗
4. Sales literature, Megatech Ltd, Havant, Hants P09 1BH.
5. El SHABASY M. · Period. Polytech., Electr. Eng · 1981 · 25 · 283
6. CAMPBELL D. S.: in ‘Handbook of thin film technology’, (eds Maissel L. I., and Glang R.), 12.3; 1970, New York, McGraw-Hill.
7. KRONGELB S.: in ‘Adhesion measurement of thin films, thick films and bulk coatings’, STP 640, (ed. Mittal K. L.), 107; 1978, Philadelphia, Pa, ASTM.10.1520/STP38628S ↗
8. 10.1051/jphysrad:0195000110703550010.1051/jphysrad:01950001107035500 ↗
9. 10.1051/jphysrad:01952001301206580010.1051/jphysrad:019520013012065800 ↗
10. BENJAMIN P. · Proc. R. Soc. (London), A · 1959 · 254 · 177
11. BENJAMIN P. · Proc. R. Soc. (London), A · 1959 · 254 · 163
12. BENJAMIN P. · Proc. R. Soc. (London), A · 1961 · 261 · 516
13. BENJAMIN P. · Proc. R. Soc. (London), A · 1963 · 274 · 267
14. MATTHEWS A. · 1974
15. PERRY A. J., LAENG P., and HINTERMANN H. E.: in Proc. 8th Int. Conf. on Chemical Vapour Deposition, 1981, Paris, 475; 1981, Princeton, Electrochemical Society.
16. 10.1016/0040-6090(81)90520-410.1016/0040-6090(81)90520-4 ↗
17. 10.1016/0040-6090(82)90211-510.1016/0040-6090(82)90211-5 ↗
18. 10.1016/0040-6090(83)90019-610.1016/0040-6090(83)90019-6 ↗
19. VOSSEN J. L.: in ‘Adhesion measurement of thin films, thick films and bulk coatings’, STP 640, (ed. Mittal K. L.), 122; 1978, Philadelphia, Pa, ASTM.10.1520/STP38629S ↗
20. AINDOW A. M., DEWHURST R. J., PALMER S. B., and SCRUBY C. B. NDT Int., 1984, 17, 329.10.1016/0308-9126(84)90141-X ↗
21. COOPER J. A., DEWHURST R. J., and PALMER S. B.: in Proc. ‘Ultrasonics international’, Brighton; 1985, London, Butterworths.
22. DEWHURST R. J.: unpublished work, University of Hull.
23. BEAMS J. W. · Tech. Proc. Am. Electroplaters Soc. · 1956 · 43 · 211
24. 10.1021/ie50478a05910.1021/ie50478a059 ↗
25. 10.1016/0040-6090(72)90123-X10.1016/0040-6090(72)90123-X ↗
26. 10.1016/0040-6090(80)90093-010.1016/0040-6090(80)90093-0 ↗
27. 10.1155/APEC.3.2110.1155/APEC.3.21 ↗
28. 10.1016/0040-6090(84)90204-910.1016/0040-6090(84)90204-9 ↗
29. 10.1149/1.242677210.1149/1.2426772 ↗
30. BROOK G. B. · J. Inst. Met. · 1929 · 41 · 73
31. 10.1038/physci229155a010.1038/physci229155a0 ↗
32. HINTERMANN H. E., and LAENG P.: in Proc. Int. Conf. on ‘Recent developments in speciality steels and hard materials’, (Materials Development 82), (eds Comins N. R., and Clark J. B.); 1982, Pretoria.
33. 10.1088/0022-3727/3/6/30710.1088/0022-3727/3/6/307 ↗
34. 10.1116/1.57284810.1116/1.572848 ↗
35. 10.1063/1.168672710.1063/1.1686727 ↗