journal article·2020-03Open access

Formulation of corrosion rate of magnesium alloys using microstructural parameters

Ahmad Bahmani, Srinivasan Arthanari, Kwang Seon Shin

Journal of Magnesium and Alloys· Volume 8· Issue 1

Abstract

Up to the date of writing this article, a quantitative analysis between corrosion rate and combined microstructural parameters including composition, grain size, and precipitations has not been reported. Hence, a literature review was carried out on these parameters to understand the quantitative effect of each one on the corrosion rate of Mg and Mg alloys. Moreover, using the available data in the literature and several experimental results, a new model was developed to predict the corrosion rate, through microstructural parameters. This model suggests that by using ultra-fined grains, alloying compounds with low Volta-potential difference relative to the matrix and a low fraction of secondary phase, a very low corrosion rates of materials are achievable.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. Fundamentals and advances in magnesium alloy corrosion10.1016/j.pmatsci.2017.04.011 ↗
2. The relation between severe plastic deformation microstructure and corrosion behavior of AZ31 magnesium alloy10.1016/j.jallcom.2008.01.084 ↗
3. Volta potentials measured by scanning kelvin probe force microscopy as relevant to corrosion of magnesium alloys10.5006/1432 ↗
4. Biodegradability engineering of biodegradable Mg alloys: tailoring the electrochemical properties and microstructure of constituent phases10.1038/srep02367 ↗
5. Texture effect on corrosion behavior of AZ31 Mg alloy in simulated physiological environment10.1016/j.matlet.2011.11.032 ↗
6. Effects of crystallographic orientation on corrosion behavior of magnesium single crystals10.1007/s11837-012-0334-0 ↗
7. The effect of texture on the corrosion behavior of AZ31 Mg alloy10.1007/s11837-012-0341-1 ↗
8. Crystal-orientation-dependent corrosion behaviour of single crystals of a pure Mg and Mg-Al and Mg-Cu solid solutions10.1016/j.corsci.2016.03.019 ↗
9. The control of crystallographic texture in the use of magnesium as a resorbable biomaterial10.1039/C4RA08484E ↗
10. Anisotropy of the crystallographic orientation and corrosion performance of high-strength AZ80 Mg alloy10.1016/j.jma.2015.11.002 ↗
11. Crystallographic effects on the corrosion of twin roll cast AZ31 Mg alloy sheet10.1016/j.actamat.2017.05.027 ↗
12. Influence of grain orientation on the corrosion behavior of rolled AZ31 magnesium alloy10.1007/s40195-015-0337-2 ↗
13. Grain refined and basal textured surface produced by burnishing for improved corrosion performance of AZ31B Mg alloy10.1016/j.corsci.2011.12.018 ↗
14. Corrosion and passivation of magnesium alloys10.1016/j.corsci.2016.05.041 ↗
15. First-principles studies on alloying and simplified thermodynamic aqueous chemical stability of calcium-, zinc-, aluminum-, yttrium- and iron-doped magnesium alloys10.1016/j.actbio.2009.08.016 ↗
16. Exploring the possibility of protective surface oxides upon Mg alloy AZ31 via lutetium additions10.1016/j.corsci.2014.08.015 ↗
17. Corrosion behaviour in salt spray and in 3.5% nacl solution saturated with Mg(Oh)2 of as-cast and solution heat-treated binary Mg–x alloys: x=Mn, Sn, Ca, Zn, Al, Zr, Si, Sr10.1016/j.corsci.2013.06.030 ↗
18. Corrosion of ultra-high-purity Mg in 3.5% NaCl solution saturated with Mg(OH)210.1016/j.corsci.2013.05.018 ↗
19. Bahmani · 2018
20. Grain character influences on corrosion of ECAPed pure magnesium, corrosion engineering
21. Revealing the relationship between grain size and corrosion rate of metals10.1016/j.scriptamat.2010.08.035 ↗
22. Effect of grain size on corrosion: a review10.5006/1.3462912 ↗
23. Effects of grain size on the corrosion resistance of pure magnesium by cooling rate-controlled solidification10.1007/s11706-015-0299-3 ↗
24. Preferred crystallographic pitting corrosion of pure magnesium in hanks’ solution10.1016/j.corsci.2012.06.011 ↗
25. Effect of grain size on the electrochemical behavior of pure magnesium anode10.1016/j.jma.2017.09.003 ↗
26. How useful is sbf in predicting in vivo bone bioactivity?10.1016/j.biomaterials.2006.01.017 ↗
27. Microstructural modification of pure mg for improving mechanical and biocorrosion properties10.1016/j.jmbbm.2016.04.015 ↗
28. Corrosion behavior of severely plastic deformed magnesium based alloys: a review10.3103/S1068375517050039 ↗
29. Corrosion behavior of equal-channel-angular-pressed pure magnesium in NaCl aqueous solution10.1016/j.corsci.2009.10.004 ↗
30. Effects of ecae processing temperature on the microstructure, mechanical properties, and corrosion behavior of pure Mg10.1007/s12613-015-1117-8 ↗
31. Anodic oxidation of aluminum, chromium, hafnium, niobium, tantalum, titanium, vanadium, and zirconium at very low current densities10.1149/1.2428577 ↗
32. Corrosion resistance of ultra fine-grained ti10.1016/j.scriptamat.2004.04.011 ↗
33. The electrochemical corrosion of bulk nanocrystalline ingot iron in acidic sulfate solution10.1021/jp0538971 ↗
34. Annealing effects on the corrosion resistance of ultrafine-grained pure titanium10.1016/j.corsci.2014.08.017 ↗
35. Corrosion behavior of ultra-fine grained industrial pure al fabricated by ECAP10.1016/S1003-6326(08)60407-0 ↗
36. Effect of grain size and twins on corrosion behaviour of AZ31B magnesium alloy10.1016/j.corsci.2009.10.018 ↗
37. Effects of grain size on the corrosion resistance of wrought magnesium alloys containing neodymium10.1016/j.corsci.2012.01.021 ↗
38. Corrosion behavior of fine-grained AZ31B magnesium alloy10.1016/j.corsci.2012.04.039 ↗
39. Corrosion behaviour of bulk ultra-fine grained AZ91D magnesium alloy fabricated by equal-channel angular pressing10.1016/j.corsci.2010.09.044 ↗
40. The relation between microstructure and corrosion behavior of AZ80 Mg alloy following different extrusion temperatures10.1016/j.corsci.2008.03.003 ↗
41. Effect of the number of ECAP pass time on the electrochemical properties of 1050 al alloys10.1016/j.msea.2003.08.056 ↗
42. Grain size distribution effects on the corrosion behaviour of materials10.1016/j.corsci.2012.04.040 ↗
43. Enhanced corrosion resistance of high strength Mg-3Al-1 Zn alloy sheets with ultrafine grains in a phosphate-buffered saline solution10.1016/j.corsci.2013.04.035 ↗
44. Enhanced corrosion resistance of ultrafine-grained AZ61 alloy containing very fine particles of Mg17Al12 phase10.1016/j.corsci.2013.05.032 ↗
45. Effect of severe plastic deformation on mechanical properties and corrosion behavior of magnesium alloys
46. Influence of ECAP process on mechanical and corrosion properties of pure Mg and ZK60 magnesium alloy for biodegradable stent applications10.4161/biom.28283 ↗
47. Microstructure, texture evolution, mechanical properties and corrosion behavior of ecap processed ZK60 magnesium alloy for biodegradable applications10.1016/j.jmbbm.2014.05.024 ↗
48. Determination of mechanical anisotropy of magnesium processed by ECAP10.1016/j.jmrt.2014.09.002 ↗
49. Effect of heat treatment and deformation temperature on the mechanical properties of ECAP processed ZK60 magnesium alloy10.1016/j.msea.2016.09.037 ↗
50. Exceptional mechanical properties of ultra-fine grain mg-4y-3re alloy processed by ECAP10.1016/j.msea.2017.09.106 ↗
51. Effect of cold rolling on the structure and hydrogen properties of AZ91 and AM60D magnesium alloys processed by ECAP10.1016/j.ijhydene.2017.07.118 ↗
52. Characterization of the microstructures and the shape memory properties of the Fe-Mn-Si-Cr-Ni-c shape memory alloy after severe plastic deformation by differential speed rolling and subsequent annealing10.1016/j.matchar.2017.11.055 ↗
53. Effect of post-annealing and strong deformation process on the mechanical and corrosion properties of a Mg-Mn alloy for biomedical application10.3938/jkps.72.692 ↗
54. Microstructure and mechanical properties of Mg–Al–Zn alloy sheets severely deformed by asymmetrical rolling10.1016/j.scriptamat.2006.09.034 ↗
55. Effect of grain size changes on corrosion behavior of copper produced by accumulative roll bonding process10.1590/S1516-14392013005000135 ↗
56. Nanostructure formation during accumulative roll bonding of commercial purity titanium10.1016/j.matchar.2016.10.024 ↗
57. Mechanical and microstructural investigation of Zn/Sn multilayered composites fabricated by accumulative roll bonding (ARB) process10.1016/j.jallcom.2017.08.241 ↗
58. The effect of annealing on the formability of aluminum 1200 after accumulative roll bonding10.1016/j.jmapro.2017.09.013 ↗
59. Processing of AZ31 magnesium alloy by a new noble severe plastic deformation method10.1016/j.msea.2010.10.033 ↗
60. Enhancing the strength and ductility in accumulative back extruded WE43 magnesium alloy through achieving bimodal grain size distribution and texture weakening10.1016/j.msea.2017.04.098 ↗
61. Accumulative back extrusion (ABE) processing as a novel bulk deformation method10.1016/j.msea.2008.10.027 ↗
62. Characterization of ultra-fine grained aluminum produced by accumulative back extrusion (ABE)10.1016/j.matchar.2012.03.004 ↗
63. Evolution of microstructure and mechanical properties in a hypoeutectic Al-Si-Mg alloy processed by accumulative back extrusion10.1016/j.msea.2015.10.066 ↗
64. Improving the mechanical properties of pure magnesium by three-roll planetary milling10.1016/j.msea.2014.06.061 ↗
65. Analytical and experimental study on the spiral marks of the rolled product during three-roll planetary rolling processes10.1016/j.ijmachtools.2005.09.013 ↗
66. Gradient structure produced by three roll planetary milling: numerical simulation and microstructural observations10.1016/j.msea.2015.04.078 ↗
67. Effect of friction stir processing on electrical conductivity and corrosion resistance of AA6063-T6 al alloy, proceedings of the institution of mechanical engineers
68. Corrosion behaviour of friction stir welded AZ31B Mg in 3·5%NaCl solution, corrosion engineering
69. Optimization of friction stir welding parameters for improved corrosion resistance of AA2219 aluminum alloy joints10.1016/j.dt.2015.05.003 ↗
70. Corrosion behavior of friction stir welded AZ31B Mg alloy - Al6063 alloy joint10.1080/23311916.2016.1145565 ↗
71. Homogeneous corrosion of high pressure torsion treated Mg–Zn–Ca alloy in simulated body fluid10.1016/j.matlet.2010.11.015 ↗
72. High pressure torsion extrusion as a new severe plastic deformation process10.1016/j.msea.2016.04.008 ↗
73. Microhardness and corrosion properties of hypoeutectic Al-7Si alloy processed by high-pressure torsion10.1016/j.matdes.2015.06.018 ↗
74. Incremental high pressure torsion as a novel severe plastic deformation process: processing features and application to copper10.1016/j.msea.2014.12.041 ↗
75. Structural development at severely high strain in AZ31 magnesium alloy processed by cold forging and subsequent annealing10.1016/j.matdes.2012.08.025 ↗
76. Multi-directional forging of AZ61Mg alloy under decreasing temperature conditions and improvement of its mechanical properties10.1016/j.msea.2011.05.050 ↗
77. Microstructures and mechanical properties of AZ61 magnesium alloy after isothermal multidirectional forging with increasing strain rate10.1016/j.msea.2015.07.028 ↗
78. On the effect of non-isothermal annealing and multi-directional forging on the microstructural evolutions and correlated mechanical and electrical characteristics of hot-deformed Al-Mg alloy10.1016/j.msea.2016.01.056 ↗
79. Enhanced mechanical property of AZ31B magnesium alloy processed by multi-directional forging method10.1016/j.matchar.2017.05.010 ↗
80. Microstructure evolution and mechanical properties of Mg-Gd-Y-Ag-Zr alloy fabricated by multidirectional forging and ageing treatment10.1016/j.msea.2017.06.038 ↗
81. Effect of ageing on microstructure and mechanical properties of a multi-directionally forged Mg-6al-1 Zn alloy10.1016/j.msea.2012.11.021 ↗
82. Effect of grain size on fatigue behavior in AZ61 Mg alloys fabricated by MDFing10.2320/matertrans.MH201508 ↗
83. Effect of multi-directional forging and annealing on abrasive wear behavior in a medium carbon low alloy steel10.1016/j.triboint.2017.11.043 ↗
84. Effect of multi-directional forging on the microstructure and mechanical properties of Tibw/ta15 composite with network architecture10.1016/j.matdes.2017.08.055 ↗
85. Review of recent developments in the field of magnesium corrosion10.1002/adem.201400434 ↗
86. Influence of hot rolling on the corrosion behavior of several Mg-x alloys10.1016/j.corsci.2014.10.012 ↗
87. Corrosion behaviour in salt spray and in 3.5% nacl solution saturated with Mg(oh)2 of as-cast and solution heat-treated binary Mg-Re alloys: rE=Ce, la, Nd, Y, Gd10.1016/j.corsci.2013.06.032 ↗
88. Corrosion mechanism applicable to biodegradable magnesium implants10.1016/j.mseb.2010.12.017 ↗
89. Effect of galvanic corrosion between precipitate and matrix on corrosion behaviour of As-cast Mg-Al alloys10.1007/BF03028082 ↗
90. Kelvin probe force microscopy and its application10.1016/j.surfrep.2010.10.001 ↗
91. Corrosion behaviour of AZ31 magnesium alloy containing various levels of strontium10.1016/j.corsci.2018.06.018 ↗
92. Improved corrosion resistant and strength of a magnesium alloy using multi-directional forging (MDF)10.1007/s00170-019-04176-1 ↗
93. Microgalvanic activity of an Mg-Al-Ca-based alloy studied by scanning kelvin probe force microscopy10.1016/j.scriptamat.2007.08.002 ↗
94. Susceptibility of rare-earth-magnesium alloys to micro-galvanic corrosion10.1016/j.corsci.2010.08.006 ↗
95. Effect of nd on the corrosion behaviour of AM50 and AZ91D magnesium alloys in 3.5 wt.% Nacl solution10.1016/j.corsci.2011.10.033 ↗
96. The relation between microstructure and corrosion behavior of GTA welded AZ31B magnesium sheet10.1016/j.msea.2006.12.122 ↗
97. Influence of chloride ion concentration and temperature on the corrosion of Mg-Al alloys in salt fog10.1016/j.corsci.2010.01.020 ↗
98. Influence of Gd on the corrosion behavior of AM50 and AZ91D magnesium alloys10.5006/0010-9312-68.5.398 ↗
99. A compilation of corrosion potentials for magnesium alloys10.5006/1257 ↗
100. Salt spray corrosion behaviour of new Mg-Al alloys containing nd or gd, corrosion engineering