journal article·2022-02-01Open access

Feasibility study of dissimilar metal joining by laser riveting of Ti-6Al-4V to AA6061

Bowei Li, Ali Khan, Bin Wang, Paola De Bono

Journal of Laser Applications· Volume 34· Issue 1

Abstract

Aluminum of cylindrical profile (of diameter 1–4 mm) was trailed by laser metal wire deposition for potential riveting applications. The rivet was built onto a Ti6Al4V substrate through a hole in an AA6061 sheet. The built feature was postprocessed by a high-frequency laser washing technique to obtain the desired finish. Parameter optimization has allowed increased productivity by almost seven times while achieving required wetting conditions and metallurgical properties. It is found that the quality (both morphology and metallurgy) of the laser rivet joint is highly dependent on the laser wash parameters. The rivet crown and welding areas improved by the postwash process were directly reflected in the microhardness and shear tests and increased by 90% and 62%, respectively, compared with those in an unwashed rivet.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

National Structural Integrity Research Centre 1 , Granta Park, Cambridge CB2 16AL, United Kingdom

College of Engineering, Design and Physical Sciences, Brunel University London 2 , Kingston Lane, Uxbridge, Middlesex UB8 3PH, United Kingdom

TWI Ltd. 3 , Granta Park, Cambridge CB21 6AL, United Kingdom

References (34)

Show source-provided references
1. Enhanced wetting behavior using femtosecond laser-textured surface in laser welding-brazing of Ti/Al butt joint10.1016/j.optlastec.2021.107212 ↗
2. The optimization of friction spot welding process parameters in AA6181-T4 and Ti6Al4V dissimilar joints10.1016/j.matdes.2015.05.082 ↗
3. Interfacial microstructure and mechanical properties of Al/Ti dissimilar joints fabricated via friction stir welding10.1016/j.jallcom.2019.03.043 ↗
4. Joining mechanism of Ti/Al dissimilar alloys during laser welding-brazing process10.1016/j.jallcom.2010.09.125 ↗
5. Self-riveting friction stir lap welding of aluminum alloy to steel10.1016/j.matlet.2016.08.102 ↗
6. TIG welding-brazing of Ti6Al4V and Al5052 in overlap configuration with assistance of zinc foil10.1016/j.jmatprotec.2017.08.015 ↗
7. Investigations on the material flow and the role of the resulting hooks on the mechanical behaviour of dissimilar friction stir welded Al2024-T3 to Ti-6Al-4V overlap joints10.1016/j.jmatprotec.2021.117057 ↗
8. The failure mechanics analysis of the solid self-piercing riveting joints10.1016/j.engfailanal.2014.10.008 ↗
9. Multi-material adhesively bonded structures: Characterisation and modelling of their rate-dependent performance10.1016/j.compositesb.2020.108077 ↗
10. Joining of carbon fibre reinforced polymer (CFRP) composites and aluminium alloys—A review10.1016/j.compositesa.2017.06.007 ↗
11. 2013 · 87050M
12. Real-time monitoring of laser hot-wire cladding of Inconel 62510.1016/j.optlastec.2014.03.007 ↗
13. Metal additive manufacturing: A review10.1007/s11665-014-0958-z ↗
14. Additive manufacturing of Ti–6Al–4V components by shaped metal deposition: Microstructure and mechanical properties10.1016/j.matdes.2009.11.032 ↗
15. Deposition of Ti–6Al–4V using laser and wire, part I: Microstructural properties of single beads10.1016/j.surfcoat.2011.07.095 ↗
16. Deposition of Ti–6Al–4V using laser and wire, part II: Hardness and dimensions of single beads10.1016/j.surfcoat.2011.07.094 ↗
17. Micro laser metal wire deposition for additive manufacturing of thin-walled structures10.1016/j.optlaseng.2017.07.003 ↗
18. Wire-feed additive manufacturing of metal components: Technologies, developments and future interests10.1007/s00170-015-7077-3 ↗
19. Dissimilar metals deposition by directed energy based on powder-fed laser additive manufacturing10.1016/j.jmapro.2019.05.018 ↗
20. Fabrication of highly dissimilar TC4/steel joint with V/Cu composite transition layer by laser melting deposition10.1016/j.jallcom.2020.158319 ↗
21. Transfer mode effects on Ti6Al4V wall building in wire laser additive manufacturing10.1016/j.mfglet.2021.03.001 ↗
22. Numerical analysis of heat transfer and fluid flow in multilayer deposition of PAW-based wire and arc additive manufacturing10.1016/j.ijheatmasstransfer.2018.03.085 ↗
23. Wire based additive layer manufacturing: Comparison of microstructure and mechanical properties of Ti–6Al–4V components fabricated by laser-beam deposition and shaped metal deposition10.1016/j.jmatprotec.2011.01.018 ↗
24. On the origin of microstructural banding in Ti-6Al4V wire-arc based high deposition rate additive manufacturing10.1016/j.actamat.2018.12.038 ↗
25. 2003
26. 2010
27. Effects of fusion zone size and failure mode on peak load and energy absorption of advanced high strength steel spot welds under lap shear loading conditions10.1016/j.engfailanal.2007.01.018 ↗
28. Critical review of automotive steels spot welding: Process, structure and properties10.1179/1362171813Y.0000000120 ↗
29. Failure loads of spot welds under combined opening and shear static loading conditions10.1016/S0020-7683(01)00187-1 ↗
30. Failure characterization of spot welds under combined axial–shear loading conditions10.1016/j.ijmecsci.2011.04.008 ↗
31. Additive manufacturing of strong and ductile Ti–6Al–4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
32. Effect of hot working on flow behavior of Ti–6Al–4V alloy in single phase and two phase regions10.1016/j.matdes.2010.01.060 ↗
33. Effect of heat treatment temperature on microstructure characteristic and hardness properties of casted Ti-6Al-4V ELI10.14203/widyariset.4.2.2018.153-162 ↗
34. Assessing the riveting process and the quality of riveted lap joints in aerospace and other applications10.1016/B978-0-12-819140-8.00013-4 ↗