Effects of process parameters on the fatigue strength of laser beam welds
Source abstract
Abstract
An experimental study, augmented by three-dimensional finite element analysis, was performed to assess the effects of various process parameters such as presence of galvanized coating, welding speed and weld geometry (weld start and stop, metal fit-up, and weld orientation) on the fatigue resistance of laser beam welds. It was found that the fatigue resistance of laser beam welds depends upon the welding speed used and weld geometry. With a 2.75 kW CO2 laser and at a welding speed of 38.1 mm s−1, the resultant laser beam welds gave the highest fatigue resistance. For a continuous weld, maintaining good metal fit-up between the metal sheets and orienting the weld perpendicular to the loading direction increased the fatigue resistance of laser beam welds. These increases are attributed to the decrease in stress-intensity factors at the weld bead periphery. Minimal fatigue difference was found between laser beam welded bare and galvanized 0.76 mm thick low carbon steel. Microscopic examinations of laser beam welds indicated that fatigue of a stitch laser beam weld is dominated by crack propagation.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Welding Techniques and Residual Stresses · Fatigue and fracture mechanics · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
1Physics Department, Research and Development Centers
2Body-In-White Center, General Motors Corporation, Warren, Michigan 48090-9055, U.S.A.
References
Reference metadata was not supplied for this record.