journal article·2009-05-01

Partial growth of crack in laser scribing of glass

Koji Yamamoto, Noboru Hasaka, Hideki Morita, Etsuji Ohmura

Journal of Laser Applications· Volume 21· Issue 2
Publisher page

Abstract

The scribing of glass by a CO2 laser is much more effective compared to the conventional mechanical technology in use because the strength of the cut glass is improved since microcracks and particles along the cut edge are lessened. However, the crack depth of laser scribing is limited because the inner compressive stress region under the cooling area prevents median crack growth. This fact was shown by the experimental and thermal stress analyses with a finite element method (FEM) in the authors’ previous study. In this study, the glass was masked partially on the scribing line so as not to generate an inner compressive stress region, and the authors found that the median crack depth of laser scribing was deeper in the experiment. Thermal stress analysis of this phenomenon was conducted by using three-dimensional FEM. As a result, the stress distribution and the phenomenon of which the median crack grew deeper corresponded qualitatively well. It has been supported that the model of laser scribing mechanism proposed in the authors’ previous study is valid.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Laser Material Processing Techniques · Erosion and Abrasive Machining · Advanced Surface Polishing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Graduate School of Engineering, Osaka University, 2-1 Yamadaoka, Suita, Osaka 565–0871, Japan

Mitsuboshi Diamond Industrial Co., Ltd., 1-4-37 Minami-kaneden, Suita, Osaka 564–0044, Japan

References (14)

Show source-provided references
1. Median crack initiation and propagation beneath a disc glass cutter
2. Separation technology for FPD glass
3. 2007 · 513
4. Controlled separation of brittle materials using a laser
5. 1970
6. 2006 · 23
7. Design and validation of a hybrid laser/water-jet machining system for brittle materials10.2351/1.2900554 ↗
8. Crack extension induced by thermal stress associated with uniform heating in a circle
9. Apply on-line crack detection technique to laser cutting with controlled fracture10.1007/s001700170015 ↗
10. Fracture mechanism of laser cutting with controlled fracture10.1115/1.1559163 ↗
11. 2005 · 105
12. Three-dimensional thermal stress analysis on laser scribing of glass10.1016/j.precisioneng.2007.10.004 ↗
13. Thermal stress analysis on laser scribing of glass10.2351/1.2995761 ↗