Effects of three-dimensional vibration on laser cladding of SS316L alloy
Source abstract
Abstract
As a widely used approach for surface modification, laser cladding plays a significant role in surface hardening and repairing of metallic parts. However, the defects existing in laser cladding parts, such as cracks, tensile residual stress, and pores, significantly affect the performance and the application of the cladding parts. In this study, an SS316L layer was fabricated on a 45 steel substrate using a laser cladding process assisted by three-dimensional vibration. The microstructures and the properties of the coating and the bonding interface with various vibration parameters were analyzed and compared. The microstructures of the cladding layer and the matrix were analyzed by an optical microscope and a scanning electron microscope. The results show that the three-dimensional vibration is able to refine the columnar dendrites in the cladding layer. The oscillation accelerates both the liquid flow and the thermal transfer of the molten pool, which not only reduces the temperature gradient but also increases the solidification growth rate. Meanwhile, the porosity and the maximum pore size in the cladding layer were significantly reduced by the vibration. The average microhardness of the cladding layer significantly increased assisted by the three-dimensional vibration. Experimental results demonstrate that the effects of the three-dimensional vibration are more significant than the single vertical vibration. The proposed approach provides a potential way to improve laser additive manufacturing and remanufacturing.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Institute of Laser Advanced Manufacturing, Zhejiang University of Technology 1 , Hangzhou 310023, China
State Key Laboratory of Fluid Power and Mechatronic Systems, Zhejiang University 2 , Hangzhou 310027, China
Funding
Key R&D Program of Zhejiang Province, China · State Key Laboratory of Fluid Power and Mechatronic Systems · National Natural Science Foundation of China
References (30)
Show source-provided references
1. Structure of NiCrAlY coatings deposited on single-crystal alloy turbine blade material by laser cladding10.1016/j.actamat.2009.06.049 ↗
2. Technological and scientific landscape of laser cladding process in 200710.1016/j.surfcoat.2008.06.122 ↗
3. Laser cladding of aerospace materials10.1016/S0924-0136(01)01121-9 ↗
4. Turbine blade tip single crystalline clad deposition with applied remelting passes for well oriented volume extension10.2351/1.4983667 ↗
5. Laser cladding and wear testing of nickel base hardfacing materials: Influence of process parameters10.2351/1.4983160 ↗
6. Experimental investigation of direct diamond laser cladding in combination with high speed camera based process monitoring10.2351/1.4944004 ↗
7. Investigation on the effect of laser remelting for laser cladding nickel based alloy10.2351/1.5096126 ↗
8. High-performance laser cladding with combined energy sources10.2351/1.4817455 ↗
9. Modeling of laser beam and powder flow interaction in laser cladding using ray-tracing10.2351/1.4906394 ↗
10. Microstructure and properties of laser clad coatings studied by orientation imaging microscopy10.1016/j.actamat.2010.09.002 ↗
11. Analysis of crack behavior for Ni-based WC composite coatings by laser cladding and crack-free realization10.1016/j.apsusc.2008.04.003 ↗
12. Fatigue life prediction model for laser clad AISI 4340 specimens with multiple surface cracks10.1016/j.ijfatigue.2016.01.025 ↗
13. Microstructure and porosity evaluation in laser-cladding deposited Ni-based coatings10.1016/j.surfcoat.2016.03.083 ↗
14. Modeling the influence of process parameters and additional heat sources on residual stresses in laser cladding10.1007/s11666-007-9026-7 ↗
15. Effect of laser cladding process parameters on clad quality and in-situ formed microstructure of Fe–TiC composite coatings10.1016/j.surfcoat.2010.08.087 ↗
16. Studies of the effects and mechanism of electromagnetic stirring on the microstructures and hardness of laser cladding WC-Co based alloy coating10.3788/CJL20103710.2672 ↗
17. Control of microstructure and mechanical properties of laser solid formed Inconel 718 superalloy by electromagnetic stirring10.1016/j.optlastec.2017.09.022 ↗
18. Influence of electric-magnetic compound field on the WC particles distribution in laser melt injection10.1016/j.surfcoat.2017.01.116 ↗
19. Microstructural refinement process of pure magnesium by electromagnetic vibrations10.1016/j.msea.2005.09.009 ↗
20. Induction-assisted laser beam welding of a thermomechanically rolled HSLA S500MC steel: A microstructure and residual stress assessment10.1016/j.msea.2013.04.039 ↗
21. Improving microstructure and wear resistance of plasma clad Fe-based alloy coating by a mechanical vibration technique during cladding10.1016/j.msea.2010.09.021 ↗
22. Microstructure evolution and mechanical properties of ultrasonic assisted laser clad yttria stabilized zirconia coating10.1016/j.ceramint.2017.04.103 ↗
23. Microstructure and mechanical properties of AZ91 alloy produced with ultrasonic vibration10.1016/j.msea.2007.09.071 ↗
24. Effects of mechanical vibration on macrostructure and mechanical properties of AC4C aluminum alloy castings10.2320/matertrans.F-M2009822 ↗
25. Influence of vibration frequency on solidification of weldments10.1016/S1359-6462(99)00416-9 ↗
26. Refinement factors of mechanical vibrations on microstructure of Al-7 mass% Si alloys10.2320/matertrans.L-MZ201107 ↗
27. Formation of non-dendritic microstructure of semi-solid aluminum alloy under vibration10.1016/j.scriptamat.2007.11.010 ↗
28. Vibration promotes heat welding of single-walled carbon nanotubes10.1016/j.cplett.2010.12.068 ↗
29. Numerical analysis of the influence of wall vibration on heat transfer with liquid hydrogen boiling flow in a horizontal tube10.1016/j.ijhydene.2017.10.149 ↗
30. ASTM E112-13 · 2016