Power and welding speed influence on bead quality for overlapped joint laser welding
Source abstract
Abstract
Laser welding has gained more and more industry acceptance due to narrow heat affected zone, low distortion levels, possibility of remote processing, and outstanding welding speeds when compared to traditional electric arc processes. Automotive industry requires a significant amount of overlapped joint welding, which usually is applied to the chassis assembling. Thus, as a mean to support laser users to optimize the welding process, this paper presents an approach through an experimental methodology followed by a phenomenological discussion about the quality of overlapped welded joints. Arguments are based on power and welding speed parameters variation and their related outcomes. This approach allows mapping of main defects such as porosity, undercut, and insufficient penetration, as well as identifying eventual preventive actions. A 10 kW IPG Photonics YLS 10000 fiber laser was used to weld 3 mm SAE 1008 steel sheets. The power ranged from 5 to 7 kW while the welding speed ranged from 2 to 5 m/min. High power levels at low welding speeds led to high temperature, resulting in an undercut issue, and low power levels at high welding speed led to insufficient penetration. Porosity was the most common defect. The best results, which did not show any type of discontinuity, were obtained at a laser power of 5 kW and a welding speed of 3 and 4 m/min.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Welding Techniques and Residual Stresses · Advanced machining processes and optimization · Laser Material Processing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Laboratory of Precision Engineering–Laser Division (LMP-Laser), Department of Mechanical Engineering, Federal University of Santa Catarina , Santa Catarina, Brazil
References (16)
Show source-provided references
1. Consideration of manufacturing effects on fatigue design for welded chassis components10.1007/s40194-015-0269-5 ↗
2. A model for estimating penetration depth of laser welding processes10.1088/0022-3727/29/7/018 ↗
3. 2011 · 60510.1007/978-3-642-01237-2 ↗
4. Parameters controlling weld bead profile in conduction laser welding10.1016/j.jmatprotec.2017.06.026 ↗
5. Effect of energy transfer modes on solidification cracking in pulsed laser welding10.1179/1362171815Y.0000000041 ↗
7. Pore formation during laser beam welding of die-cast magnesium alloy AM60B—Mechanism and remedy
8. High-speed simultaneous observation of plasma and keyhole behavior during high power CO2 laser welding: Effect of shielding gas on porosity formation10.2351/1.1324717 ↗
9. Keyhole-induced porosity formation during laser welding10.1016/j.jmatprotec.2017.10.038 ↗
10. Effect of travel speed and beam focus on porosity in alloy 690 laser welds10.1007/s11837-012-0481-3 ↗
11. Porosity formation mechanism and its prevention in laser lap welding for T-joints10.1016/j.jmatprotec.2014.03.011 ↗
12. High-speed laser welding discontinuities10.2351/1.4745217 ↗
13. Diode laser welding of stainless steel 304L10.1016/j.jmatprotec.2016.09.019 ↗
14. Laser keyhole welding of stainless steel thin plate stack for applications in fuel cell manufacturing10.1179/1362171815Y.0000000005 ↗
15. Welding with high power fiber lasers—A preliminary study10.1016/j.matdes.2006.01.009 ↗
16. Global and local mechanical properties of autogenously laser welded Ti-6Al-4V10.1007/s11661-013-2106-z ↗