Influence of plume attenuation under high power laser welding of copper using visible wavelengths
Source abstract
Abstract
Joining of copper materials has become a key factor in laser material processing of electric components like electric engines, batteries, or power electronics. A paramount challenge is the design of the laser welding process, which has to fulfil the requirements of high energy efficiency and highest seam quality at the same time. By now, high-power laser beam sources emitting visible laser radiation are available to promote the well-suited noncontact joining method, which is furthermore characterized by local energy input and high automation potential. These laser sources can now face the challenges of welding highly conductive and reflective materials, such as copper, which originate mainly in the low absorption of conventionally used infrared wavelengths at room temperature and the rapid jump of absorptivity at transition from solid to liquid state. An increase in absorption of electromagnetic radiation to more than 40% for copper at room temperature for λ = 515 nm leads to increasing energy input in the material and promotes a more efficient process therefore. However, up to now, mostly the heat conduction welding regime has been examined and the effects of shorter wavelengths on deep penetration welding have not been understood in detail. A strong deviation in weld seam depth between infrared and green laser radiation is observed for identical process parameters depending on the use of additional gas supply [F. Kaufmann, A. Meier, J. Ermer, S. Roth, and M. Schmidt, “Influence of defocusing in deep penetration welding of copper by using visible wavelength,” in Proceedings of the Eleventh International WLT-Conference on Lasers in Manufacturing, Munich, 21–24 June 2021 (M. Reth, Munich, 2021)]. Consequently, radiation attenuation by the metal vapor inside and above the keyhole plays a substantial role in the case of 515 nm laser welding [M. Haubold, A. Ganser, T. Eder, and M. F. Zäh, “Laser welding of copper using a high power disc laser at green wavelength,” Procedia CIRP 74, 446–449 (2018)]. In this work, we investigate in situ measurements of plume attenuation during laser beam welding of copper with 515 and 1030 nm laser beam sources. Both laser sources are equipped with comparable optical setups to achieve identical focal diameters on the material surface. We investigate the plume characteristics in the deep penetration welding mode of copper. A range of industry-relevant process parameters are investigated to create a basis for comparison with theoretical models. It is found that a significant difference in the attenuation of both laser wavelengths occurs in the case of deep penetration welding copper specimen and blowing the vapor plume out of the beam path is recommended therefore for an efficient welding process.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Welding Techniques and Residual Stresses · Laser Material Processing Techniques · Ocular and Laser Science Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Bayerisches Laserzentrum GmbH (blz) 1 , Konrad-Zuse-Str. 2-6, 91052 Erlangen, Germany
Erlangen Graduate School in Advanced Optical Technologies (SAOT) 2 , Paul-Gordan-Str. 6, 91052 Erlangen, Germany
Institute of Photonic Technologies (LPT), Friedrich-Alexander Universität Erlangen-Nürnberg 3 , Konrad-Zuse-Str. 3-5, 91052 Erlangen, Germany
Funding
Bundesministerium für Wirtschaft und Energie
References (25)
Show source-provided references
1. 2003
2. S. Amorosi, “Laser micro-spot welding of copper by real-time process monitoring,” Doctoral thesis (EPFL, 2005), p. 3023.
3. Analysis and possible estimation of keyhole depths evolution, using laser operating parameters and material properties10.2351/1.5040624 ↗
4. The effect of process parameters on the morphology, mechanical strength and electrical resistance of CW laser-welded pure copper hairpins10.1016/j.jmapro.2020.12.018 ↗
5. A. Heider, “Erweitern der prozessgrenzen beim laserstrahlschweißen von kupfer mit einschweißtiefen zwischen 1 mm und 10 mm,” Doctoral thesis [Institut für Strahlwerkzeuge (IFSW) der Universität Stuttgart, Stuttgart, Germany, 2018].
6. Process studies on laser welding of copper with brilliant green and infrared lasers10.1016/j.phpro.2011.03.142 ↗
7. Power modulation to stabilize laser welding of copper10.2351/1.4906127 ↗
8. 2021)
9. Laser welding of copper using a high power disc laser at green wavelength10.1016/j.procir.2018.08.161 ↗
10. Modelling of the processes of evaporation of metal and gas dynamics of metal vapour inside a keyhole in laser welding
11. 2013
12. 2007)
13. P. Shcheglov, “Study of vapour-plasma plume during high power fiber laser beam influence on metals,” Zugl.: Moskau, Univ., Doctoral thesis [Bundesanstalt für Materialforschung und -prüfung (BAM), 2012].
14. Multiple wavelength extinction technique for particle characterization in dense particle clouds10.1002/ppsc.19940110505 ↗
15. Influence of temperature and wavelength on optical behavior of copper alloys10.4028/www.scientific.net/AMM.655.89 ↗
16. M. Beck, “Modellierung des Lasertiefschweißens,” Doctoral thesis (IFSW, Universität Stuttgart, 1996).
17. 2000
18. Plume attenuation of laser radiation during high power fiber laser welding10.1002/lapl.201110010 ↗
19. 1984) · 35
20. Plume attenuation under high power Nd:Yttritium–aluminum–garnet laser welding10.2351/1.1642636 ↗
21. 1995
22. 1958 · 19810.1002/qj.49708436025 ↗
23. Optical properties of some metal oxides in solar absorbers10.1088/0031-8949/25/6A/044 ↗
24. Melt behavior on the keyhole front during high speed laser welding10.1016/j.optlaseng.2013.01.008 ↗
25. 2015