Laser cladding technology has attracted substantial attention in cutting-edge areas of metal surface repair and remanufacturing research. Nevertheless, excessive residual stress of cladding is the primary obstacle that hinders its practical application in aerospace, engineering machinery, and other industries. Herein, a comprehensive review of recent advances in the residual stress release in laser cladding is provided in three sections. The first section covers how various laser parameters and material characteristics affect residual stress. The second section discusses the effect and comparison of matching heat treatment methods before and after the laser cladding process on residual stress. The final section focuses on a brand-new concept and technique to release the residual stress during the cladding process via phase transformation. We hope that this review will be a reference for theoretical research and implementation of new laser cladding materials and technologies and present possible scientific solutions and prospects for the ideal reduction in residual stress during the cladding process.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

College of Materials and Metallurgy, Guizhou University 1 , Guiyang 550025, China

Key Laboratory of Advanced Manufacturing Technology of the Ministry of Educating, Guizhou University 2 , Guiyang 550025, China

HanKaiSi Intelligent Technology Co., Ltd. 3 , Guiyang 550016, China

Funding

Guizhou Provincial Basic Research Program (Natural Science)

References (69)

Show source-provided references
1. Cyclic corrosion behavior of Pt/Ru-modified bond coatings exposed to NaCl plus water vapor at 1050 °C10.1016/S1005-0302(10)60036-9 ↗
2. A novel approach to prevent decarburisation through electroless plating10.1080/02670844.2018.1479363 ↗
3. Chlorine-induced high temperature corrosion of inconel 625 sprayed coatings deposited with different thermal spray techniques10.1016/j.surfcoat.2016.12.086 ↗
4. Chemical vapor deposition of TiN on transition metal substrates10.1016/j.surfcoat.2017.11.063 ↗
5. Research on remanufacturing strategy for 45 steel gear using H13 steel powder based on laser cladding technology10.1016/j.jmapro.2019.12.009 ↗
6. Multi-physics modeling and Gaussian process regression analysis of cladding track geometry for direct energy deposition10.1016/j.optlaseng.2019.105950 ↗
7. Microstructural characteristics and formation mechanism of laser cladding of titanium alloys on carbon fiber reinforced thermoplastics10.1016/j.matlet.2017.02.102 ↗
8. Developments in laser-based surface engineering processes: with particular reference to protection against cavitation erosion10.1016/j.surfcoat.2016.02.019 ↗
9. Growth characteristics and mechanism of carbides precipitated in WC–Fe composite coatings by laser induction hybrid rapid cladding10.1016/j.jallcom.2010.06.115 ↗
10. Microstructure and properties of laser cladding FeCrBSi composite powder coatings with higher Cr content10.1016/j.jmatprotec.2013.12.009 ↗
11. Effect of Ti on T15M composite coating fabricated by laser cladding technology10.1016/j.surfcoat.2017.07.008 ↗
12. Laser cladding technique for erosive wear applications: A review10.1088/2053-1591/ab6894 ↗
13. Study on the laser cladding of FeCrNi coating10.1016/j.ijleo.2018.10.062 ↗
14. A physical modeling and predictive simulation of the laser cladding process10.1016/j.addma.2018.05.017 ↗
15. Effect of laser beam incidence angle on cladding morphology in laser cladding process10.1007/s12206-020-0315-0 ↗
16. An assessment of residual stress mitigation strategies for laser clad deposits10.1080/02670836.2016.1192766 ↗
17. Repairing of sintered tools using laser cladding by wire10.1016/j.jmatprotec.2005.02.075 ↗
18. Influence of α/β interface phase on the tensile properties of laser cladding deposited Ti–6Al–4 V titanium alloy10.1016/j.jmst.2016.09.026 ↗
19. A numerical-experimental investigation of heat distribution, stress field and crack susceptibility in Ni60A coatings10.1016/j.optlastec.2019.04.021 ↗
20. Laser powder cladding of Ti-6Al-4 V α/β alloy10.3390/ma10101178 ↗
21. Microstructure characteristics and mechanical properties of a laser cladded Fe-based martensitic stainless steel coating10.1016/j.surfcoat.2020.126795 ↗
22. Residual stress in laser cladded rail10.1016/j.triboint.2019.105844 ↗
23. Numerical evaluation of advanced laser control strategies influence on residual stresses for laser powder bed fusion systems10.1007/s40192-020-00191-3 ↗
24. Numerical simulation of thermal and stress field of single track cladding in wide-beam laser cladding10.1007/s00170-019-04056-8 ↗
25. Numerical simulations of temperature and stress field of Fe-Mn-Si-Cr-Ni shape memory alloy coating synthesized by laser cladding10.1016/j.ijleo.2021.167079 ↗
26. Analysis and optimization of process parameters in Al–SiCp laser cladding10.1016/j.optlaseng.2015.10.014 ↗
27. Titanium/hydroxyapatite (Ti/HA) gradient materials with quasi-continuous ratios fabricated by SLM: Material interface and fracture toughness10.1016/j.matdes.2017.12.037 ↗
28. Application of a new alloy and post processing procedures for laser cladding repairs on hypereutectoid rail components10.3390/ma15155447 ↗
29. Effects of substrate preheating temperatures on the microstructure, properties, and residual stress of 12CrNi2 prepared by laser cladding deposition technique10.3390/ma11122401 ↗
30. Characterization of the microstructures and the shape memory properties of the Fe-Mn-Si-Cr-Ni-C shape memory alloy after severe plastic deformation by differential speed rolling and subsequent annealing10.1016/j.matchar.2017.11.055 ↗
31. Fatigue behavior of a Fe-Mn-Si shape memory alloy used for prestressed strengthening10.1016/j.matdes.2017.07.055 ↗
32. Deposition pattern based thermal stresses in single-layer laser aided direct material deposition process10.1115/1.2401620 ↗
33. Evading stress-property tradeoff in a SMA/PZT laser cladding coating via phase transformations10.1016/j.surfcoat.2022.128313 ↗
34. Systematic evaluation of process parameter maps for laser cladding and directed energy deposition10.1016/j.addma.2018.04.002 ↗
35. Residual stress measurements on AISI 316L samples manufactured by selective laser melting10.1016/j.addma.2017.07.007 ↗
36. Prediction modelling and process optimization for forming multi-layer cladding structures with laser directed energy deposition10.1016/j.optlastec.2020.106607 ↗
37. A numerical investigation for alternative toolpath deposition solutions for surface cladding of stainless steel P420 powder on AISI 1018 steel substrate10.1007/s00170-018-1840-1 ↗
38. Considering cyclic plasticity to predict residual stresses in laser cladding of inconel 718 multi bead samples10.1016/j.jmapro.2019.05.002 ↗
39. Thermal stress cycle simulation in laser cladding process of Ni-based coating on H13 steel10.3390/coatings11020203 ↗
40. Analysis and prediction on geometric characteristics of multi-track overlapping laser cladding10.1007/s00170-018-2107-6 ↗
41. Optimization of processing parameters in fiber laser cladding10.1007/s00170-020-06214-9 ↗
42. Residual stresses in stellite 6 layers cladded on AISI 420 steel plates with a Nd: YAG laser10.2351/1.5039858 ↗
43. Effect of laser cladding process parameters on clad quality and in-situ formed microstructure of Fe-TiC composite coatings10.1016/j.surfcoat.2010.08.087 ↗
44. Laser cladding with scanning optics: Effect of scanning frequency and laser beam power density on cladding process10.2351/1.4868895 ↗
45. Modulation of power density distribution in time and space for high speed laser cladding10.1016/j.jmatprotec.2007.05.052 ↗
46. Effects of laser cladding on crack resistance improvement for aluminum alloy used in aircraft skin10.1016/j.optlastec.2020.106531 ↗
47. Thermo-mechanical analysis in pulsed laser cladding of WC powder on inconel 71810.1007/s00170-017-0117-4 ↗
48. Experimental characterization of laser cladding of CPM 9 V on H13 tool steel for die repair applications10.1016/j.jmapro.2015.06.018 ↗
49. Effects of process variables on interfacial quality of laser cladding on aeroengine blade material GH413310.1016/j.jmatprotec.2008.03.004 ↗
50. Study on microstructure and properties of Fe-based amorphous composite coating by high-speed laser cladding10.1016/j.optlastec.2021.107574 ↗
51. Modeling and optimization for laser cladding via multi-objective quantum-behaved particle swarm optimization algorithm10.1016/j.surfcoat.2019.125129 ↗
52. Effect of cooling rate on residual stress and mechanical properties of laser remelted ceramic coating10.1016/j.jeurceramsoc.2018.04.020 ↗
53. Numerical research on effect of overlap ratio on thermal-stress behaviors of the high-speed laser cladding coating10.1088/1674-1056/abcf9b ↗
54. Effects of laser energy density and path on residual stress of remanufactured key components for shield tunneling machine10.1016/j.matchemphys.2022.126617 ↗
55. Residual stress and fracture strength of brazed joint of ceramic and titanium alloy with the aid of laser deposited functionally graded material layers10.1016/j.jmapro.2018.06.041 ↗
56. Thermo-mechanical model for simulating laser cladding induced residual stresses with single and multiple clad beads10.1016/j.jmatprotec.2015.04.031 ↗
57. Numerical simulation to study the effects of different laser cladding sequences on residual stress and deformation of Ti-6Al-4 V/WC10.1557/s43578-021-00372-6 ↗
58. Impacts of laser cladding residual stress and material properties of functionally graded layers on titanium alloy sheet10.1016/j.addma.2020.101303 ↗
59. Damage tolerance assessment of laser clad repairs of coarse grain Ti-6Al-4 V10.1007/s11340-022-00846-6 ↗
60. The role of microstructure in the stress relaxation and tempering of laser clad Ti-6Al-4 V10.1016/j.msea.2014.02.034 ↗
61. Residual stress in laser cladded heavy-haul rails investigated by neutron diffraction10.1016/j.jmatprotec.2019.116511 ↗
62. Analysis of crack behavior for Ni-based WC composite coatings by laser cladding and crack-free realization10.1016/j.apsusc.2008.04.003 ↗
63. Characteristics of microstructure and stresses and their effects on interfacial fracture behavior for laser-deposited maraging steel10.1016/j.matdes.2017.10.020 ↗
64. Three-dimensional transient finite element analysis for residual stresses in the laser aided direct metal/material deposition process10.2351/1.1961688 ↗
65. Modeling the influence of process parameters and additional heat sources on residual stresses in laser cladding10.1007/s11666-007-9026-7 ↗
66. In-situ synthesis of Fe-Mn-Si-Cr-Ni shape memory alloy functional coating by laser cladding10.3788/COL201412.041403 ↗
67. Direct laser deposition as repair technology for a low transformation temperature alloy: Microstructure, residual stress, and properties10.1016/j.msea.2019.01.072 ↗
68. Effects of stress-induced solid phase transformations on residual stress in laser cladding a Fe-Mn-Si-Cr-Ni alloy coating10.1016/j.matdes.2020.108824 ↗
69. Study on microstructure and properties of a Fe-based SMA/PZT composite coating produced by laser cladding10.1016/j.jallcom.2020.154813 ↗