固体燃料电池阴极材料La0.6Sr0.4Co0.2Fe0.8O3-δ的微观结构与阻抗特性研究
Source abstract
Abstract
复合钙钛矿氧化物La0.6Sr0.4Co0.2Fe0.8O3-δ是一种适于中温固体氧化物燃料电池的阴极材料.采用柠檬酸螯合法合成了La0.6Sr0.4Co0.2Fe0.8O3-δ粉体,并通过XRD和SEM,研究了前驱体溶液pH值和煅烧温度对其粉体晶相结构的影响;同时,通过烧结体的SEM和交流阻抗分析,详细讨论了前驱体溶液pH值和烧结温度对烧结体显微结构和阻抗特性的影响.结果表明,前驱体溶液pH=4、煅烧温度为900。C的粉体,1400℃下烧结2h获得的烧结体,具有最低的阻抗.