以316L不锈钢丝网为基材,利用电泳沉积技术对丝网表面进行改性,考察了添加剂浓度、电压加压方式、热处理温度对铝粉在丝网表面包覆效果的影响,制备出表面规整、高粘结强度的Al2O3/Al载体膜,在30min超声振荡后,载体膜脱落率仅为0.5wt%;结合表面浸涂技术,在丝网上涂覆纳米La0.8Sr0.2MnO3,通过SEM、XRD、BET等手段对催化剂进行表征,发现丝网表面催化剂负载均匀,比表面积达到119.4m^2/g,在30min超声振荡后,脱落率为5.0wt%.催化燃烧性能测试表明,La0.8Sr0.2MnO3在不锈钢丝网上有较好的活性,高空速、高浓度的甲苯在400℃基本能被完全燃烧.