article·1997-01-01

Preperation and Properties of Sialon Bonded SiC Material

DU Xinghon

Abstract

β-sialon powders (Si(6-z) Al_zO_zN(8-z) with z=3.0) were synthesized by carbothermal reductionand nitriding reaction. A sample of sialon bonded SiC was sintered at 1580~1640℃. Bulk densityof the sintered body was 2.26g/cm~3, three pomt bending strength was 42.0MPa. The bendingstrength was still remained when quenching the sintered body at 1200℃ to cold water (15℃) 10times. Weight loss in flowing air at 1350℃ was less than 0.035%cm~(-2).