Synthesis and Characterization of (Y,Bi)AG:Eu3+ Red Phosphor by Coprecipitation Method
Source abstract
Abstract
采用化学共沉淀法合成了Bi3+掺杂的YAG∶Eu3+荧光粉,利用DTA-TGA、XRD分析煅烧过程中前驱体的热效应和YAG晶相的形成过程,并通过XRD、SEM、PL表征不同Bi3+含量的YAG∶Eu3+荧光粉结构、形貌及光致发光性能.结果表明:前驱体在煅烧温度1000℃及以上时,可形成纯相的YAG晶相;Bi3+对Eu3+具有敏化作用,Bi3+的掺入使YAG∶Eu3+荧光粉的光致发光峰强度显著增强,当Bi3+含量为0.0010时, 其发光峰强度达到最大值,其后随着Bi3+含量进一步增加,则因浓度猝灭而导致荧光粉发光峰强度降低;掺入Bi3+对YAG∶Eu3+荧光粉晶胞参数有一定的影响,但不会改变其晶体结构;Bi3+掺杂的YAG∶Eu3+荧光粉均匀、无团聚,呈类球型.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Luminescence Properties of Advanced Materials · Polydiacetylene-based materials and applications · Gas Sensing Nanomaterials and Sensors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (6)
Show source-provided references
1. In Jung-Hyun10.1016/j.supflu.2006.08.006 ↗
2. Li Xia
3. Fadlalla H M H10.1016/j.matchemphys.2008.08.049 ↗
4. Yang R10.1016/j.jeurceramsoc.2008.05.005 ↗
5. Saladino M L10.1016/j.optmat.2008.04.008 ↗
6. Zhou Y H10.1016/S0925-3467(02)00020-4 ↗