Fabrication of TiO2/WO3 Micro-nanofibers Composites and Their Photocatalytic Activity
Source abstract
Abstract
PVP/Ti(OC4H9)4/N5H37W6O24·H2O precursors with different Ti/W molar ratios were successfully syn- thesized by a simple combination method of Sol-Gel and electrospinning techniques. The electrospun precursors was converted into TiO2/WO3 micro-nanofibers via calcination at different temperatures in air. The obtained sam- ples were characterized by X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), scanning electron microscopy (FE-SEM) and ultraviolet-visible diffuse reflectance spectroscopy (UV-Vis) techniques. Photocatalytic activity was evaluated by degradation of methylene blue (MB) under ultraviolet light irradiation. The results showed that WO3-doped TiO2 micro-nanofibers with Ti/W molar ratio of 12:1 and TiO2/WO3 micro- nanofi- bers with Ti/W molar ratio of 4:1 after calcination at 500℃ exhibited better photocatalytic degradation activity than that of pure TiO2 micro-nanofibers.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: TiO2 Photocatalysis and Solar Cells · Advanced Photocatalysis Techniques · Transition Metal Oxide Nanomaterials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.