Abstract

At present, stereolithography 3D printing technology is widely used in ceramic additive manufacturing because of its high printing accuracy. Among them, the stereolithography ceramic slurry of non-oxide ceramics such as silicon carbide, silicon nitride, etc., has problems such as poor dispersion stability and low curing layer thickness because the incident light is difficult to penetrate and produce light curing reaction for printing high-solid-loading slurry. This is all because the refractive index and optical absorbance of the non-oxide ceramic printing material powder are relatively high. Therefore, printing and molding of high-solid-content non-oxide ceramics have become main challenges in stereolithography 3D printing, and the technology has attracted a large number of researchers to study its light-curing mechanism, powder control and other mechanisms. This paper systematically summarizes the
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing and 3D Printing Technologies · Injection Molding Process and Properties · Photopolymerization techniques and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. HALLORAN J W. Ceramic stereolithography: additive manufacturing for ceramics by photopolymerization. Annual Review of Materials Research, 2016, 46(1): 19-40.10.1146/annurev-matsci-070115-031841 ↗
2. DUFAUD O, CORBEL S. Oxygen diffusion in ceramic suspensions for stereolithography. Chemical Engineering Journal, 2003, 92(1): 55-62.10.1016/S1385-8947(02)00115-8 ↗
3. WU H D, CHENG Y L, LIU W, et al. Effect of the particle size and the debinding process on the density of alumina ceramics fabricated by 3D printing based on stereolithography. Ceramics International, 2016, 42(15): 17290-17294.10.1016/j.ceramint.2016.08.024 ↗
4. LI W L, LIU W W, QI F, et al. Determination of micro-mechanical properties of additive manufactured alumina ceramics by nanoindentation and scratching. Ceramics International, 2019, 45(8): 10612-10618.10.1016/j.ceramint.2019.02.128 ↗
5. SCHWENTENWEIN M, HOMA J. Additive manufacturing of dense alumina ceramics. International Journal of Applied Ceramic Technology, 2015, 12(1): 1-7.10.1111/ijac.12319 ↗
6. ZHANG K Q, XIE C, WANG G, et al. High solid loading, low viscosity photosensitive Al2O3 slurry for stereolithography based additive manufacturing. Ceramics International, 2019, 45(1): 203-208.10.1016/j.ceramint.2018.09.152 ↗
7. WU X Q, LIAN Q, LI D C, et al. Effects of soft-start exposure on the curing characteristics and flexural strength in ceramic projection stereolithography process. Journal of the European Ceramic Society, 2019, 39(13): 3788-3796.10.1016/j.jeurceramsoc.2019.05.004 ↗
8. XU X H, ZHOU S X, WU J F, et al. Preparation of highly dispersive solid microspherical α-Al2O3 powder with a hydrophobic surface for stereolithography-based 3d printing technology. Ceramics International, 2020, 46(2): 1895-1906.10.1016/j.ceramint.2019.09.167 ↗
9. LI X B, ZHONG H, ZHANG J X, et al. Fabrication of zirconia all-ceramic crown via DLP-based stereolithography. International Journal of Applied Ceramic Technology, 2020, 17(3): 844-853.10.1111/ijac.13441 ↗
10. FU X S, ZOU B, XING H Y, et al. Effect of printing strategies on forming accuracy and mechanical properties of ZrO2 parts fabricated by SLA technology. Ceramics International, 2019, 45(14): 17630-17637.10.1016/j.ceramint.2019.05.328 ↗
11. HE R X, LIU W, WU Z W, et al. Fabrication of complex-shaped zirconia ceramic parts via a DLP-stereolithography-based 3D printing method. Ceramics International, 2018, 44(3): 3412-3416.10.1016/j.ceramint.2017.11.135 ↗
12. LI X B, ZHONG H, ZHANG J X, et al. Dispersion and properties of zirconia suspensions for stereolithography. International Journal of Applied Ceramic Technology, 2020, 17(1): 239-247.10.1111/ijac.13321 ↗
13. SUN J X, BINNER J, BAI J M. Effect of surface treatment on the dispersion of nano zirconia particles in non-aqueous suspensions for stereolithography. Journal of the European Ceramic Society, 2019, 39(4): 1660-1667.10.1016/j.jeurceramsoc.2018.10.024 ↗
14. WU H D, LIU W, HE R X, et al. Fabrication of dense zirconia- toughened alumina ceramics through a stereolithography-based additive manufacturing. Ceramics International, 2017, 43(1): 968-972.10.1016/j.ceramint.2016.10.027 ↗
15. LIU X Y, ZOU B, XING H Y, et al. The preparation of ZrO2-Al2O3 composite ceramic by SLA-3D printing and sintering processing. Ceramics International, 2020, 46(1): 937-944.10.1016/j.ceramint.2019.09.054 ↗
16. XING H Y, ZOU B, LIU X Y, et al. Effect of particle size distribution on the preparation of ZTA ceramic paste applying for stereolithography 3D printing. Powder Technology, 2020, 359: 314-322.10.1016/j.powtec.2019.09.066 ↗
17. WANG Y Y, WANG Z Y, LIU S H, et al. Additive manufacturing of silica ceramics from aqueous acrylamide based suspension. Ceramics International, 2019, 45(17): 21328-21332.10.1016/j.ceramint.2019.07.118 ↗
18. CHARTIER T, BADEV A, ABOULIATIM Y, et al. Stereolithography process: influence of the rheology of silica suspensions and of the medium on polymerization kinetics-cured depth and width. Journal of the European Ceramic Society, 2012, 32(8): 1625-1634.10.1016/j.jeurceramsoc.2012.01.010 ↗
19. BAE C J, KIM D, HALLORAN J W. Mechanical and kinetic studies on the refractory fused silica of integrally cored ceramic mold fabricated by additive manufacturing. Journal of the European Ceramic Society, 2019, 39(2): 618-623.10.1016/j.jeurceramsoc.2018.09.013 ↗
20. LASGORCEIX M, CHAMPION E, CHARTIER T. Shaping by microstereolithography and sintering of macro-micro-porous silicon substituted hydroxyapatite. Journal of the European Ceramic Society, 2016, 36(4): 1091-1101.10.1016/j.jeurceramsoc.2015.11.020 ↗
21. WANG Z, HUANG C Z, WANG J, et al. Development of a novel aqueous hydroxyapatite suspension for stereolithography applied to bone tissue engineering. Ceramics International, 2019, 45(3): 3902-3909.10.1016/j.ceramint.2018.11.063 ↗
22. PFAFFINGER M, HARTMANN M, SCHWENTENWEIN M, et al. Stabilization of tricalcium phosphate slurries against sedimentation for stereolithographic additive manufacturing and influence on the final mechanical properties. International Journal of Applied Ceramic Technology, 2017, 14(4): 499-506.10.1111/ijac.12664 ↗
23. CHEN Z W, LIU C B, LI J J, et al. Mechanical properties and microstructures of 3D printed bulk cordierite parts. Ceramics International, 2019, 45(15): 19257-19267.10.1016/j.ceramint.2019.06.174 ↗
24. HE R J, ZHOU N P, ZHANG K Q, et al. Progress and challenges towards additive manufacturing of SiC ceramic. Journal of Advanced Ceramics, 2021, 10(4): 637-674.10.1007/s40145-021-0484-z ↗
25. SEFIU A R, DING Y X, SHU F X, et al. Photopolymerization- based additive manufacturing of ceramics: a systematic review. Journal of Advanced Ceramics, 2021, 10(3): 442-471.10.1007/s40145-021-0468-z ↗
26. LIU Y, CHEN Z W. Research progress in photopolymerization- based 3D printing technology of ceramics. Journal of Materials Engineering, 2020(9): 1-12.
27. TANG J, YANG Y, HUANG Z R. Research progress of silicon carbide ceramic slurry based 3D printing. Materials Reports, 35(S01): 8.
28. GRIFFITH M L, HALLORAN J W. Scattering of ultraviolet radiation in turbid suspensions. Journal of Applied Physics, 1997, 81(6): 2538-2546.10.1063/1.364311 ↗
29. DING G J, HE R J, ZHANG K Q, et al. Stereolithography-based additive manufacturing of gray-colored SiC ceramic green body. Journal of the American Ceramic Society, 2019, 102(12): 7198-7209.10.1111/jace.16648 ↗
30. WU K C, SEEFELDT K F, SOLOMON M J, et al. Prediction of ceramic stereolithography resin sensitivity from theory and measurement of diffusive photon transport. Journal of Applied Physics, 2005, 98(2): 10.10.1063/1.1980531 ↗
31. BURGER R, WENDLAND W L. Sedimentation and suspension flows: historical perspective and some recent developments. Journal of Engineering Mathematics, 2001, 41(2/3): 101-116.10.1023/A:1011934726111 ↗
32. CHEN Z W, LI Z Y, LI J J, et al. 3D printing of ceramics: a review. Journal of the European Ceramic Society, 2019, 39(4): 661-687.10.1016/j.jeurceramsoc.2018.11.013 ↗
33. WANG M, XIE C, HE R J, et al. Polymer-derived silicon nitride ceramics by digital light processing based additive manufacturing. Journal of the American Ceramic Society, 2019, 102(9): 5117-5126.10.1111/jace.16389 ↗
34. DE HAZAN Y, PENNER D. SiC and SiOC ceramic articles produced by stereolithography of acrylate modified polycarbosilane systems. Journal of the European Ceramic Society, 2017, 37(16): 5205-5212.10.1016/j.jeurceramsoc.2017.03.021 ↗
35. TANG J, GUO X T, CHANG H T, et al. The preparation of SiC ceramic photosensitive slurry for rapid stereolithography. Journal of the European Ceramic Society, 2021, 41(15): 7516-7524.10.1016/j.jeurceramsoc.2021.08.029 ↗
36. VRANCKENAND K C, POSSEMIERS K, VAN DER VOORT P, et al. Surface modification of silica gels with aminoorganosilanes. Colloids and Surfaces A: Physicochemical and Engineering Aspects, 1995, 98(3): 235-241.10.1016/0927-7757(95)03119-X ↗
37. LIU D, MALGHAN S G. Role of polyacrylate in modifying interfacial properties and stability of silicon nitride particles in aqueous suspensions. Colloids & Surfaces A Physicochemical & Engineering Aspects, 1996, 110(1): 37-45.10.1016/0927-7757(95)03441-2 ↗
38. XIAO C X, NI Q, CHEN HAN, et al. Effect of polyvinylpyrrolidone on rheology of aqueous SiC suspensions dispersed with poly(aspartic acid). Colloids and Surfaces A: Physicochemical and Engineering Aspects, 2012, 399: 108-111.10.1016/j.colsurfa.2012.02.046 ↗
39. LIU G W, ZHANG X Z, YANG J, et al. Recent advances in joining of SiC-based materials (monolithic SiC and SiCf/SiC composites): joining processes, joint strength, and interfacial behavior. Journal of Advanced Ceramics, 2019, 8(1): 19-38.10.1007/s40145-018-0297-x ↗
40. CHEN X W, CHENG G F, ZHANG J M, et al. Residual stress variation in SiCf/SiC composite during heat treatment and its effects on mechanical behavior. Journal of Advanced Ceramics, 2020, 9(5): 567-575.10.1007/s40145-020-0395-4 ↗
41. EOM J H, KIM Y W, RAJU S. Processing and properties of macroporous silicon carbide ceramics: a review. Journal of Asian Ceramic Societies, 2013, 1(3): 220-242.10.1016/j.jascer.2013.07.003 ↗
42. ZHAO R C, BAO J X. Lightweight structure and mirror blank formation of the SiC ceramic mirror with large caliber. Optics & Optoelectronic Technology, 2014, 12(6): 65-69.
43. WU H B, YAN Y J, LIU G L, et al. Effects of grain grading on microstructures and mechanical behaviors of pressureless solid-state-sintered SiC. International Journal of Applied Ceramic Technology, 2015, 12(5): 976-984.10.1111/ijac.12409 ↗
44. LI Y, GAO J Q, YANG J F. Preparation of complicated SiC green bodies via aqueous slip casting. Key Engineering Materials, 2010, 434-435: 88-91.10.4028/www.scientific.net/KEM.434-435.88 ↗
45. BAI X J, DING G J, ZHANG K Q, et al. Stereolithography additive manufacturing and sintering approaches of SiC ceramics. Open Ceramics, 2021, 5: 100046.10.1016/j.oceram.2020.100046 ↗
46. ZHANG H, YANG Y, HU K H, et al. Stereolithography-based additive manufacturing of lightweight and high-strength Cf/SiC ceramics. Additive Manufacturing, 2020, 34: 101199.10.1016/j.addma.2020.101199 ↗
47. DING G J, HE R J, ZHANG K Q, et al. Dispersion and stability of SiC ceramic slurry for stereolithography. Ceramics International, 2020, 46(4): 4720-4729.10.1016/j.ceramint.2019.10.203 ↗
48. DING G J, HE R J, ZHANG K Q, et al. Stereolithography 3D printing of SiC ceramic with potential for lightweight optical mirror. Ceramics International, 2020, 46(11, Part B): 18785-18790.10.1016/j.ceramint.2020.04.196 ↗
49. HU C Q, CHEN Y F, YANG T S, et al. Effect of SiC powder on the properties of SiC slurry for stereolithography. Ceramics International, 2021, 47(9): 12442-12449.10.1016/j.ceramint.2021.01.101 ↗
50. CAO J W, IDREES M, TIAN G Q, et al. Complex SiC-based structures with high specific strength fabricated by vat photopolymerization and one-step pyrolysis. Additive Manufacturing, 2021, 48: 102430.10.1016/j.addma.2021.102430 ↗
51. TIAN X Y, ZHANG W G, LI D C, et al. Reaction-bonded SiC derived from resin precursors by stereolithography. Ceramics International, 2012, 38(1): 589-597.10.1016/j.ceramint.2011.07.047 ↗
52. CHEN R G, LIAN Q, HE X N, et al. A stereolithographic diamond-mixed resin slurry for complex SiC ceramic structures. Journal of the European Ceramic Society, 2021, 41(7): 3991-3999.10.1016/j.jeurceramsoc.2021.02.014 ↗
53. XING H Y, ZOU B, WANG X F, et al. Fabrication and characterization of SiC whiskers toughened Al2O3 paste for stereolithography 3D printing applications. Journal of Alloys and Compounds, 2020, 828(5): 154347.10.1016/j.jallcom.2020.154347 ↗
54. ZORAN K, VLADIMIR D K. Silicon nitride: the engineering material of the future. Journal of Materials Science, 2012, 47(2): 535-552.10.1007/s10853-011-5942-5 ↗
55. HAMPSHIRE S. Silicon nitride ceramics-review of structure, processing and properties. Journal of Achievements of Materials and Manufacturing Engineering, 2007, 24(1): 2685-2689.
56. RILEY F L. Silicon nitride and related materials. Journal of the American Ceramic Society, 2000, 83(2): 245-265.10.1111/j.1151-2916.2000.tb01182.x ↗
57. XING H Y, ZOU B, LIU X Y, et al. Fabrication strategy of complicated Al2O3-Si3N4 functionally graded materials by stereolithography 3D printing. Journal of the European Ceramic Society, 2020, 40(15): 5797-5809.10.1016/j.jeurceramsoc.2020.05.022 ↗
58. CHEN R F, DUAN W Y, WANG G, et al. Preparation of broadband transparent Si3N4-SiO2 ceramics by digital light processing (DLP) 3D printing technology. Journal of the European Ceramic Society, 2021, 41(11): 5495-5504.10.1016/j.jeurceramsoc.2021.04.045 ↗
59. LI X B, ZHANG J X, DUAN Y S, et al. Rheology and curability characterization of photosensitive slurries for 3D printing of Si3N4 ceramics. Applied Sciences, 2020, 10: 6438.10.3390/app10186438 ↗
60. HUANG R J, JIANG Q G, WU H D, et al. Fabrication of complex shaped ceramic parts with surface-oxidized Si3N4 powder via digital light processing based stereolithography method. Ceramics International, 2019, 45(4): 5158-5162.10.1016/j.ceramint.2018.11.116 ↗
61. SHEN X, GAO Y A, XU Z. Research and application of silane coupling agents. Shanghai Journal of Biomedical Engineering, 2006, 27(1): 14-17.
62. LIU Y, ZHAN L N, HE Y, et al. Stereolithographical fabrication of dense Si3N4 ceramics by slurry optimization and pressure sintering. Ceramics International, 2020, 46(2): 2063-2071.10.1016/j.ceramint.2019.09.186 ↗
63. TIAN Z, YANG Y P, WANG Y, et al. Fabrication and properties of a high porosity H-BN-SiO2 ceramics fabricated by stereolithography- based 3D printing. Materials Letters, 2019, 236: 144-147.10.1016/j.matlet.2018.10.058 ↗
64. SHI B H, SHANG Y Y, ZHANG P, et al. Dynamic capillary-driven additive manufacturing of continuous carbon fiber composite. Matter, 2020, 2(6): 1594-1604.10.1016/j.matt.2020.04.010 ↗