Interfacial Mechanical Properties of the Domestic 3rd Generation 2.5D SiCf/SiC Composite
Source abstract
Abstract
国产 3 代 2.5D SiC f /SiC 复合材料的界面力学性能 管皞阳, 张 立, 荆开开, 师维刚, 王 晶, 李玫, 刘永胜 张程煜
Only a short abstract or summary was supplied by the source.
Source: openalex_inverted_index · Quality: short
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis · Advanced Surface Polishing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. 李世波, 徐永东, 张立同. 碳化硅纤维增强陶瓷基复合材料的研究进展. 材料导报, 2001, 15(1): 45.
2. 丁冬海, 周万城, 张标, 等. 连续SiC纤维增韧SiC基体复合材料研究进展. 硅酸盐通报, 2011, 30(2): 356.
3. GRONDAHL C M, TSUCHIYA T. Performance benefit assessment of ceramic components in an MS9001FA gas turbine. Journal of Engineering for Gas Turbines and Power-Transactions of the ASME, 2001, 123(3): 513.10.1115/1.1335476 ↗
4. 张立同, 成来飞. 连续纤维增韧陶瓷基复合材料可持续发展战略探讨. 复合材料学报, 2007(2): 1.
5. SUN J J, LIU W, LV X X, et al. Characterization of BN interface and its effect on the mechanical behavior of SiCf/SiC composites. Vacuum, 2023, 211: 111918.10.1016/j.vacuum.2023.111918 ↗
6. LIU Y, CHAI N, QIN H, et al. Tensile fracture behavior and strength distribution of SiCf/SiC composites with different SiBN interface thicknesses. Ceramics International, 2015, 41(1, Part B): 1609.10.1016/j.ceramint.2014.09.098 ↗
7. 朱思雨, 张巧君, 洪智亮, 等. 平纹编织SiCf/SiC复合材料的中温蠕变断裂时间及损伤机制. 复合材料学报, 2023, 40(1): 464.
8. RUGG K L, TRESSLER R E, LAMON J, et al. Interfacial behavior of microcomposites during creep at elevated temperatures. Journal of the European Ceramic Society, 1999, 19(13): 2297.10.1016/S0955-2219(99)00117-X ↗
9. MARSHALL D B. Analysis of fiber debonding and sliding experiments in brittle matrix composites. Acta Metallurgica et Materialia, 1992, 40(3): 427.10.1016/0956-7151(92)90391-Q ↗
10. MARSHALL D B, OLIVER W C. Measurement of interfacial mechanical-properties in fiber-reinforced ceramic matrix. Journal of the American Ceramic Society, 1987, 70(8): 542.10.1111/j.1151-2916.1987.tb05702.x ↗
11. HSUEH C. Evaluation of interfacial properties of fiber-reinforced ceramic composites using a mechanical properties microprobe. Journal of the American Ceramic Society, 1993, 76(12): 3041.10.1111/j.1151-2916.1993.tb06607.x ↗
12. EVANS A G, DOMERGUE J M, VAGAGGINI E. Methodology for relating the tensile constitutive behavior of ceramic-matrix composites to constituent properties. Journal of the American Ceramic Society, 1994, 77(6): 1425.10.1111/j.1151-2916.1994.tb09739.x ↗
13. WANG Y Q, ZHANG L T, CHENG L F, et al. Characterization of tensile behavior of a two-dimensional woven carbon/silicon carbide composite fabricated by chemical vapor infiltration. Materials Science and Engineering: A, 2008, 497(1/2): 295.10.1016/j.msea.2008.07.050 ↗
14. LIU S H, ZHANG L T, YIN X W, et al. Proportional limit stress and residual thermal stress of 3D SiC/SiC composite. Journal of Materials Science & Technology, 2014, 30(10): 959.10.1016/j.jmst.2014.08.004 ↗
15. JIAO G Q, WANG B. Effects of interface properties on tensile strength of ceramic matrix composites. Journal of Inorganic Materials, 2009, 24(5): 919.10.3724/SP.J.1077.2009.00919 ↗
16. REBILLAT F, LAMON J, NASLAIN R, et al. Interfacial bond strength in SiC/C/SiC composite materials, as studied by single- fiber push-out tests. Journal of the American Ceramic Society, 1998, 81(4): 965.10.1111/j.1151-2916.1998.tb02434.x ↗
17. 于海蛟. 多层界面制备、表征及其对SiCf/SiC复合材料性能的影响. 长沙: 国防科技技术大学博士论文, 2011.
18. SAUDER C, BRUSSON A, LAMON J. Influence of interface characteristics on the mechanical properties of Hi-Nicalon type-S or Tyranno-SA3 fiber-reinforced SiC/SiC minicomposites. International Journal of Applied Ceramic Technology, 2010, 7(3): 291.10.1111/j.1744-7402.2010.02485.x ↗
19. DOMERGUE J M, HEREDIA F E, EVANS A G. Hysteresis loops and the inelastic deformation of 0/90 ceramic matrix composites. Journal of the American Ceramic Society, 1996, 79(1): 161.10.1111/j.1151-2916.1996.tb07894.x ↗
20. Materials, American Society for Testing. ASTM STP1309. West Con Shohocken: ASTM Int’l, 1997.
21. VAGAGGINI E, DOMERGUE J M, EVANS A G. Relationships between hysteresis measurements and the constituent properties of ceramic-matrix composites I: theory. Journal of the American Ceramic Society, 1995, 78(10): 2709.10.1111/j.1151-2916.1995.tb08046.x ↗
22. VILLENEUVE J F, NASLAIN R. Longitudinal/radial thermal expansion and poission ratio of some ceramic fibres as measured by transmission electron microscopy. Composites Science&Technology, 1993, 49(1): 89.10.1016/0266-3538(93)90025-C ↗
23. HUTCHINSON J W, JENSEN H M. Models of fiber debonding and pullout in brittle composites with friction. Mechanics of Materials, 1990, 9(2): 139.10.1016/0167-6636(90)90037-G ↗
24. RODRÍGUEZ M, MOLINA-ALDAREGUÍA J M, GONZÁLEZ C, et al. A methodology to measure the interface shear strength by means of the fiber push-in test. Composites Science and Technology, 2012, 72(15): 1924.10.1016/j.compscitech.2012.08.011 ↗
25. MOLINA-ALDAREGUI´A J M, RODRIGUEZ M, GONZA´LEZ C, et al. An experimental and numerical study of the influence of local effects on the application of the fibre push-in tests. Philosophical Magazine, 2011, 91: 1293.10.1080/14786435.2010.480947 ↗
26. KUNTZ M, GRATHWOHL G. Advanced evaluation of push-in data for the assessment of fiber reinforced ceramic matrix composites. Advanced Engineering Materials, 2001, 3(6): 371.10.1002/1527-2648(200106)3:6<371::AID-ADEM371>3.3.CO;2-P ↗
27. DING J X, MA X K, FAN X M, et al. Failure behavior of interfacial domain in SiC-matrix based composites. Journal of Materials Science & Technology, 2021, 88: 1.10.1016/j.jmst.2021.02.010 ↗
28. CURTIN W A. In-situ fiber strengths in ceramic-matrix composites from fracture mirrors. Journal of the American Ceramic Society, 1994, 77(4): 1075.10.1111/j.1151-2916.1994.tb07272.x ↗
29. THOULESS M D, SBAIZERO O, SIGL L S, et al. Effect of interface mechanical properties on pullout in a SiC-fiber-reinforced lithium aluminum silicate glass-ceramic. Journal of the American Ceramic Society, 1989, 72(4): 517.10.1111/j.1151-2916.1989.tb06171.x ↗
30. AVESTON J, KELLY A. Theory of multiple fracture of fibrous composites. Journal of Materials Science, 1973, 8(3): 352.10.1007/BF00550155 ↗
31. CHRISTENSEN M R, LO K H. Solutions for effective shear proper ties in 3 phase sphere and cylinder. Journal of the Mechanics and Physics of Solids, 1979, 27(4): 315.10.1016/0022-5096(79)90032-2 ↗
32. GUO S, KAGAWA Y. Tensile fracture behavior of continuous SiC fiber-reinforced SiC matrix composites at elevated temperatures and correlation to in situ constituent properties. Journal of the European Ceramic Society, 2002, 22(13): 2349.10.1016/S0955-2219(02)00028-6 ↗
33. REBIlAT F, LAMON J, GUETTE A. The concept of a strong interface applied to SiC/SiC composites with a BN interphase. Acta Materialia, 2000, 48(18/19): 4609.10.1016/S1359-6454(00)00247-0 ↗
34. DICARLO J A, YUN H M, MORSCHER G N, et al. SiC/SiC composites for 1200 °C and above// NAROTTAM P B.Handbook of Ceramic Composites, Boston, MA: Springer, 2005: 77-98.10.1007/0-387-23986-3_4 ↗