Effect of Graphitization on the Strength of Cast-Iron Tubes of Economizers of Hot Water Boilers
Source abstract
Abstract
Abstract— The article contains the results of examination of cast-iron pipes of water economizers of water-heating boilers, which were in operation in the period of 1986–1991 and which have no external visual defects. We have determined a dependence of wear-out in the form of graphitic corrosion of the surface layer of inner walls of economizer pipes. Researches have been conducted with the use of an JSM-6390LV scanning electron microscope equipped with an attachment for conduct of energy-dispersive analysis, and with the use of a DuraScan 20 microhardness tester. There are images of areas given, where microhardness testing was performed. The areas were exposed to graphitic corrosion. The dimensions of the layer completely transformed as a result of graphitization and the transition zone were determined. The microhardness of the layer completely transformed as a result of graphitization and the transition zone was measured. It was found that the microhardness of these zones is significantly lower than the microhardness of gray cast iron. We have also presented the results of energy-dispersive analysis and specific diagnostic features identifying the graphitization process. In the article we propose a method of assessment of supporting capacity of cast-iron pipes of water economizers based on the rate of their graphitization. A mathematical model takes into account all main properties, features, physical and geometric characteristic of the real structure, which has an analytical model represented by a beam rigidly restrained on both heads, and which is bent by well-distributed dead weight load arising from the pipe’s own weight and the weight of the water flowing through it. The calculated residual wall thickness of 4.53 mm after wear of its internal cylindric surface is comparable with the known empirical data of statical analysis of emergency situations at economizers. The data given in the article could be used by specialists for expert examination of cast-iron pipes of economizers, as well as for justification of their sorting or life extension.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metal Alloys Wear and Properties · Coal Combustion and Slurry Processing · Material Properties and Failure Mechanisms
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. Dosa, I. and Tomuş, B., Efficiency of steam generator ecomomizer at different loads, MultiScience–XXXII. microCAD International Multidisciplinary Scientific Conference, 2018. https://doi.org/10.26649/musci.2018.00310.26649/musci.2018.003 ↗
2. Miswar, Arsyad, H., and Arma, L.H., Construction strength evaluation of boiler economizer tube materials based on hardness value, AIP Conf. Proc., 2023, vol. 2630, p. 040001. https://doi.org/10.1063/5.012597810.1063/5.0125978 ↗
3. Lepov, V.V., Achikasova, V.S., Makharova, S.N., Zakharov, V.E., and Pavlov, N.V., Failure analysis of the material of water boiler pipe operated in the Arctic zone of the Republic of Sakha (Yakutia), Prirodnye Resursy Arktiki i Subarktiki, 2020, vol. 25, no. 3, pp. 143–151. https://doi.org/10.31242/2618-9712-2020-25-3-1410.31242/2618-9712-2020-25-3-14 ↗
4. Olawale, J.O., Odusote, J.K., Rabiu, A.B., and Ochapa, E.O., Evaluation of corrosion behaviour of grey cast iron and low alloy steel in cocoa liquor and well water, J. Miner. Mater. Charact. Eng., 2013, vol. 1, no. 2, pp. 44–48. https://doi.org/10.4236/jmmce.2013.1200910.4236/jmmce.2013.12009 ↗
5. John, E., Boxall, J., Collins, R., Bowman, E., and Susmel, L., Multiaxial fatigue of water pipe grey cast iron, Int. J. Fatigue, 2024, vol. 178, p. 108002. https://doi.org/10.1016/j.ijfatigue.2023.10800210.1016/j.ijfatigue.2023.108002 ↗
6. Hajali, M., McNealy, A., and Efaz, I., Structural analysis of large diameter cast iron pipes under cyclic loading and fatigue failure, Pipelines 2023, 2023, pp. 97–106. https://doi.org/10.1061/9780784485033.01110.1061/9780784485033.011 ↗
7. Agala, A., Khan, M., and Starr, A., Degradation mechanisms associated with metal pipes and the effective impact of LDMs and LLMs in water transport and distribution, Proc. Inst. Mech. Eng., Part C, 2023, vol. 237, no. 8, pp. 1855–1876. https://doi.org/10.1177/0954406222113394810.1177/09544062221133948 ↗
8. Jur, T.A., Middleton, J.I., Yurko, A.A., Windham, R.L., and Grey, J.R., Case studies in graphitic corrosion of cast iron pipe, J. Failure Anal. Prev., 2021, vol. 21, no. 2, pp. 376–386. https://doi.org/10.1007/s11668-020-01097-010.1007/s11668-020-01097-0 ↗
9. Adegbite, S., Fahimi, A., Evans, T.S., Farrow, J., Jesson, D.A., Mulheron, M., and Smith, P.A., Trunk mains failures: The effect of corrosion on residual pipe strength, 4th International Conference on Integrity, Reliability and Failure, Funchal, Portugal, 2013, pp. 6–23.
10. Jara-Arriagada, C. and Stoianov, I., Pressure-induced fatigue failures in cast iron water supply pipes, Eng. Failure Anal., 2024, vol. 155, p. 107731. https://doi.org/10.1016/j.engfailanal.2023.10773110.1016/j.engfailanal.2023.107731 ↗
11. Visochkin, V.A., On legal support for the production and sale of used steel pipes, Ekologicheskii Vestnik Rossii, 2018, no. 6, pp. 48–51.
12. Logan, R., Mulheron, M.J., Jesson, D.A., Smith, P.A., Evans, T.S., Clay-Michael, N., and Whiter, J.T., Graphitic corrosion of a cast iron trunk main: Implications for asset management, WIT Transactions on The Built Environment, WIT Press, 2014, vol. 139, pp. 411–422. https://doi.org/10.2495/uw14035110.2495/uw140351 ↗
13. Yeshanew, D.A., Jiru, M., Lemu, H., and Tolcha, M., Internal corrosion damage mechanisms of the underground ferrous water pipelines, Adv. Sci. Technol.: Res. J., 2022, vol. 16, no. 3, pp. 111–123. https://doi.org/10.12913/22998624/14936910.12913/22998624/149369 ↗
14. Timoshenko, S.P. and Goodier, J.N., Theory of Elasticity, New York: McGraw-Hill, 1970.
15. Birger, I.A. and Mavlyutov, R.R., Soprotivlenie materialov. Uchebnoe posobie (Strength of Materials: A Textbook), Moscow: Nauka, 1986.